Stellite 31

High-performance Stellite 31 alloy offers excellent wear resistance, high fracture toughness, and superior thermal fatigue resistance for extreme environments.

About Stellite 31

Stellite 31 is a high-performance cobalt-chromium alloy known for its wear resistance, durability, and fracture toughness. Classified under UNS R30031, it meets ASTM B426 and AMS 5379 standards. This alloy is designed for applications exposed to severe abrasion, mechanical cycling, and thermal stress.

With a balance of cobalt and chromium, along with trace elements such as carbon, manganese, and silicon, Stellite 31 provides outstanding resistance in extreme environments. It is often used in critical industrial components where mechanical strength and corrosion resistance are essential.

Stellite 31 Basic Introduction

Stellite 31 is widely recognized for its superior wear and abrasion resistance. Its ability to withstand high temperatures and mechanical cycling makes it an ideal material for high-stress environments.

This alloy is commonly applied in aerospace, energy, and manufacturing industries. Its high hardness and good elongation properties ensure strength and flexibility under extreme mechanical conditions, making it suitable for long-term use in demanding applications.

custom-stellite-31-superalloy-components-equiaxed-crystal-casting-foundry

Alternative Superalloys of Stellite 31

Alternatives to Stellite 31 include other cobalt-based alloys, such as Stellite 6 and Stellite 21, which offer excellent corrosion resistance and wear properties. Inconel 718 or Haynes 25 can be considered for specific applications requiring higher creep strength.

Nickel-based superalloys like Hastelloy C-276 provide similar corrosion resistance for chemical processing environments. In cases where lightweight materials are essential, Titanium Grade 5 (Ti-6Al-4V) might be used with lower abrasion resistance than Stellite 31.


Stellite 31 Design Intention

Stellite 31 was designed to perform in environments where extreme wear, abrasion, and thermal fatigue are primary concerns. Its composition ensures it can withstand harsh conditions while retaining mechanical integrity, even at elevated temperatures.

The alloy is intended for valve seats, cutting tools, and pump wear rings. These parts need hardness and toughness to endure abrasive and mechanical stress without degradation. Its fracture resistance ensures reliability in critical applications that involve high-stress cycling.


Stellite 31 Chemical Composition

The chemical elements in Stellite 31 enhance its wear and thermal resistance. Cobalt forms the base, providing durability and flexibility, while chromium protects corrosion. The small amounts of manganese and silicon improve strength and toughness.

Element

Content (wt.%)

Cobalt (Co)

Balance

Chromium (Cr)

27.0–30.0

Carbon (C)

0.4–0.6

Nickel (Ni)

≤ 3.0

Silicon (Si)

≤ 1.0

Manganese (Mn)

≤ 1.0


Stellite 31 Physical Properties

Stellite 31’s physical properties ensure high mechanical and thermal performance. It retains structural integrity under extreme conditions, such as high temperatures and mechanical cycling.

Property

Value

Density (g/cm³)

8.44

Melting Point (°C)

1340

Thermal Conductivity (W/(m·K))

12.2

Modulus of Elasticity (GPa)

206


Metallographic Structure of Stellite 31 Superalloy

Stellite 31 features a matrix structure that combines a solid cobalt solution with chromium carbides dispersed throughout. The carbide phases enhance the alloy’s wear resistance, while the cobalt matrix offers ductility and toughness.

The alloy’s microstructure is specifically tailored for applications requiring high resistance to abrasive wear. Its carbide particles are uniformly distributed, preventing localized wear and ensuring even degradation across the material’s surface.


Stellite 31 Mechanical Properties

Stellite 31 demonstrates excellent mechanical properties, balancing hardness with fracture toughness. It can endure mechanical and thermal cycling, making it ideal for extreme operating environments.

Property

Value

Tensile Strength (MPa)

720

Yield Strength (MPa)

~600

Hardness (HRC)

55–60

Elongation (%)

3–5


Key Features of Stellite 31 Superalloy

  1. Superior Wear Resistance Stellite 31’s ability to withstand abrasive conditions makes it a top choice for components exposed to extreme wear. Its hard carbide structure prevents material loss even under continuous friction.

  2. High Fracture Toughness The alloy’s strong fracture resistance ensures mechanical stability, reducing the risk of sudden failure during high-stress operations. It maintains performance even under cyclic mechanical loads.

  3. Thermal and Mechanical Cycling Resistance Stellite 31 retains mechanical integrity under repeated temperature fluctuations, ensuring reliability in dynamic environments. This makes it suitable for turbines and industrial equipment.

  4. Corrosion Resistance With its high chromium content, Stellite 31 offers excellent protection against corrosion, particularly in environments exposed to moisture or chemicals.

  5. Long-Term Durability Designed for harsh environments, the alloy ensures extended service life without degradation, making it ideal for critical aerospace and energy components.

Stellite 31 Superalloy’s Machinability

Vacuum Investment Casting Stellite 31 is generally not used in Vacuum Investment Casting due to its high carbide content and limited flow characteristics during casting, making it unsuitable for precision casting of complex shapes.

Single Crystal Casting Stellite 31 cannot be applied in Single Crystal Casting due to its multiphase microstructure, which inhibits the formation of single crystals necessary for high-temperature turbine blades.

Equiaxed Crystal Casting Stellite 31 is not ideal for Equiaxed Crystal Casting because its properties are tailored for extreme wear resistance rather than the uniformity required in equiaxed crystal applications.

Directional Casting Stellite 31 is incompatible with Superalloy Directional Casting since its primary function is to resist wear rather than enhance creep resistance, a key characteristic of directionally solidified alloys.

Powder Metallurgy Turbine Disc Due to its carbide-rich structure, Stellite 31 is unsuitable for Powder Metallurgy Turbine Disc, which requires highly ductile and creep-resistant materials for turbine performance.

Precision Forging: The hardness of Stellite 31 makes it unsuitable for Superalloy Precision Forging, as it presents challenges during deformation and limits the production of high-precision parts.

Superalloy 3D Printing Stellite 31 is not used in Superalloy 3D Printing due to its wear-resistant carbides, which complicate powder-based printing processes and reduce printability.

CNC Machining Superalloy CNC Machining is possible with Stellite 31, though challenging. Its hardness requires specialized tooling and techniques to achieve precise tolerances.

Superalloy Welding Stellite 31 performs well in Superalloy Welding applications, maintaining integrity in joints exposed to high abrasion and heat. It is commonly used for overlay welding and hard-facing.

Hot Isostatic Pressing (HIP) Although HIP is effective for many superalloys, Stellite 31’s microstructure limits its applicability in Hot Isostatic Pressing (HIP) due to the limited ability to reduce porosity.


Stellite 31 Superalloy Applications

Aerospace and Aviation Stellite 31 is used in Aerospace and Aviation for critical components requiring wear resistance, such as bushings and valve seats in jet engines.

Power Generation In Power Generation, Stellite 31 is applied in steam turbines for its durability and resistance to wear, ensuring long-lasting performance under extreme conditions.

Oil and Gas The Oil and Gas industry utilizes Stellite 31 for valve seats, pump components, and wear rings, benefiting from its corrosion resistance in harsh environments.

Energy In the Energy sector, Stellite 31 enhances the durability of equipment subject to abrasion, such as compressors and drilling tools.

Marine Marine applications leverage Stellite 31’s corrosion resistance for propeller shafts, rudders, and pump wear rings, ensuring performance in saltwater environments.

Mining The Mining industry relies on Stellite 31 for drilling equipment and wear plates, which can withstand abrasive mining environments.

Automotive In Automotive industries, Stellite 31 is used for valve seats and other high-stress engine components that benefit from wear and heat resistance.

Chemical Processing Chemical Processing plants use Stellite 31 in equipment subjected to aggressive chemicals, such as heat exchangers and pump components.

Pharmaceutical and Food industries use Stellite 31 for cutting and processing tools where cleanliness and durability are paramount.

Military and Defense In Military and Defense, Stellite 31 is used for armor components and high-stress parts requiring wear and corrosion resistance.

Nuclear Nuclear reactors employ Stellite 31 for critical components that demand longevity under high radiation and extreme heat.


When to Choose Stellite 31 Superalloy

Stellite 31 is ideal for environments requiring wear resistance, thermal stability, and corrosion resistance. It is especially suited for components exposed to extreme temperatures and mechanical cycling, such as valve seats, turbine blades, and wear rings. This alloy ensures superior performance and long service life in applications where other materials may degrade over time.

Custom superalloy parts made with Stellite 31 are preferred when durability and reliability are non-negotiable. It is most effective in aerospace, power generation, and chemical processing, where high-performance materials are critical. Choose Stellite 31 when operational longevity, wear resistance, and thermal cycling are vital requirements.