Français

Rene 95

Rene 95 is a nickel-chromium superalloy designed for high-temperature applications, offering excellent creep resistance, thermal stability, and fatigue strength.

About Rene 95 Superalloy

Name and Equivalent Names

Rene 95, identified by UNS N07095, is a nickel-based superalloy. It conforms to AMS 5844 standards and is primarily used in aerospace, energy, and gas turbine industries. Known for its excellent high-temperature strength, Rene 95 is recognized for applications requiring long-term stability and resistance to mechanical stress.

Rene 95 Basic Introduction

Rene 95 is a high-performance nickel-chromium alloy developed in extreme environments where mechanical strength and thermal stability are essential. Its composition, including hafnium, tantalum, and boron, enhances its creep resistance and fatigue life.

This alloy performs exceptionally well at temperatures above 900°C, maintaining stability under mechanical stress and thermal cycles. It is widely used in aerospace engines, turbines, and other high-performance components that require long service life and excellent thermal fatigue resistance.

rene-95-superalloy-casting-and-forging-parts-cnc-machining-service-manufacturer

Alternative Superalloys of Rene 95

Alternatives to Rene 95 include Inconel 718, Hastelloy X, and Rene 80. Inconel 718 offers enhanced corrosion resistance, especially in marine environments. Hastelloy X is known for its excellent weldability and performance at elevated temperatures, making it suitable for aerospace components. Rene 80 provides exceptional fatigue resistance and thermal stability, making it a reliable alternative for gas turbines. Each alloy offers specific advantages based on environmental and mechanical requirements.


Rene 95 Design Intention

Rene 95 was designed to meet the needs of high-stress applications where thermal stability and creep resistance are critical. It is intended for aerospace components, gas turbines, and other industrial systems that operate at elevated temperatures. The alloy’s inclusion of elements like tantalum and hafnium enhances its high-temperature performance, ensuring durability under extreme thermal cycles and mechanical loads.


Rene 95 Chemical Composition

Rene 95 contains nickel as its base, with chromium to improve oxidation resistance and hafnium and tantalum to enhance high-temperature stability. Boron strengthens the grain boundaries, improving fatigue resistance and preventing mechanical failures under stress.

Element

Content (wt%)

Nickel (Ni)

Balance

Chromium (Cr)

12.0 – 14.0

Cobalt (Co)

8.0

Molybdenum (Mo)

3.5

Aluminum (Al)

2.5 – 3.5

Titanium (Ti)

2.5 – 3.0

Tungsten (W)

3.5

Hafnium (Hf)

1.6

Tantalum (Ta)

4.0

Boron (B)

Max 0.02


Rene 95 Physical Properties

Rene 95 has a high density and excellent thermal conductivity, supporting its use in heat-intensive applications. Its high modulus of elasticity ensures it maintains structural stability under mechanical stress.

Property

Value

Density (g/cm³)

8.95

Melting Point (°C)

1360

Thermal Conductivity (W/m·K)

10.8

Modulus of Elasticity (GPa)

218


Metallographic Structure of Rene 95 Superalloy

Rene 95 features an γ-phase nickel matrix with γ' (gamma prime) precipitates, enhancing its creep resistance and mechanical strength. Adding hafnium and tantalum improves grain boundary strength, limiting dislocation movement under stress.

This alloy also benefits from boron, further strengthening grain boundaries and ensuring fatigue resistance under cyclic thermal loads. The metallographic structure of Rene 95 makes it ideal for high-performance applications that demand long service life under extreme conditions.


Rene 95 Mechanical Properties

Rene 95 offers exceptional mechanical strength, thermal fatigue resistance, and a long creep life. These properties make it ideal for applications subjected to high mechanical stress and extreme temperatures.

Property

Value

Tensile Strength (MPa)

1100 – 1250

Yield Strength (MPa)

900 – 1000

Creep Strength

Strong >900°C

Hardness (HRC)

~40

Elongation (%)

~10

Elastic Modulus (GPa)

~215


Key Features of Rene 95 Superalloy

1. High-Temperature Strength

Rene 95 maintains excellent tensile and yield strength at temperatures above 900°C, making it ideal for aerospace engines and gas turbines.

2. Exceptional Creep Resistance

This alloy offers superior creep resistance, ensuring stable performance under continuous mechanical stress at high temperatures.

3. Strong Thermal Fatigue Resistance

Rene 95 performs reliably in applications that experience cyclic thermal loads, such as turbine blades and combustion chambers.

4. Enhanced Grain Boundary Strength

The alloy’s composition, including boron and hafnium, strengthens the grain boundaries, preventing mechanical failures and extending component life.

5. Long Service Life

Rene 95 provides excellent long-term durability, with a creep rupture life exceeding 10,000 hours at high temperatures, ensuring reliability in critical systems.

Rene 95 Superalloy’s Machinability

Rene 95 is suitable for Vacuum Investment Casting because of its ability to form high-strength components with excellent surface quality under controlled environments.

It is not typically applied in Single Crystal Casting due to its polycrystalline structure, which makes it more appropriate for applications requiring grain strengthening.

Rene 95 can be used in Equiaxed Crystal casting to produce components with uniform grains, providing strength and creep resistance under extreme conditions.

While Superalloy Directional Casting can be used for Rene 95, its primary applications focus on equiaxed forms, where it performs better with uniform grain structures.

Rene 95 is preferred for powder metallurgy turbine disc production due to its exceptional creep strength and thermal fatigue resistance, which are crucial to turbine components.

The alloy is highly suitable for Superalloy Precision Forging, delivering vital components that retain integrity under mechanical stress and high temperatures.

Superalloy 3D Printing is not ideal for Rene 95 because its complex composition makes maintaining uniformity through additive manufacturing difficult.

Rene 95 is compatible with CNC Machining, allowing the fabrication of intricate components with high precision and maintaining excellent mechanical properties.

Welding Rene 95 is challenging, but with specialized techniques, Superalloy Welding can be performed to create durable joints with proper preheating and post-weld heat treatment.

Hot Isostatic Pressing (HIP) is essential for Rene 95 to eliminate porosity and enhance its mechanical properties, ensuring uniform strength across the material.


Rene 95 Superalloy Applications

In Aerospace and Aviation, Rene 95 is used for turbine blades, discs, and combustion components, providing high strength and thermal stability.

In Power Generation, Rene 95 ensures reliable gas turbine performance, offering thermal fatigue resistance and long service life.

In the Oil and Gas industry, the alloy is used in valves and downhole tools, providing mechanical reliability in high-pressure and corrosive environments.

Rene 95 supports Energy production by enhancing the efficiency and durability of turbine components under high-temperature conditions.

In Marine applications, Rene 95’s corrosion resistance is ideal for exhaust systems and propulsion units exposed to seawater.

For Mining operations, Rene 95 is used in pump components and wear-resistant parts, ensuring durability in abrasive and high-pressure environments.

The automotive sector benefits from Rene 95’s thermal fatigue resistance, which is applied to turbochargers and high-performance exhaust systems.

In Chemical Processing, Rene 95 ensures stability and oxidation resistance in reactors and heat exchangers exposed to extreme environments.

For the Pharmaceutical and Food industries, Rene 95 provides safe, durable components for valves and seals, maintaining performance under challenging conditions.

In Military and Defense, Rene 95 is used in jet engines and missile components, offering reliability under extreme thermal and mechanical stress.

The Nuclear industry uses Rene 95 for reactor components, where high strength, radiation resistance, and thermal fatigue are critical for safety.


When to Choose Rene 95 Superalloy

Rene 95 should be selected for applications demanding high mechanical strength, thermal fatigue resistance, and durability in extreme environments. It is ideal for custom superalloy parts used in aerospace engines, gas turbines, and energy production, where components face continuous mechanical stress and high temperatures.

Rene 95 is also suitable for industries such as chemical processing, oil and gas, and military defense, where the alloy’s oxidation resistance and mechanical stability are essential. When long-term performance and reliability are required, especially at temperatures above 900°C, Rene 95 ensures consistent performance and extended service life.

Explorer les blogs associés