Français

Stellite 6

Stellite 6 is a cobalt-chromium alloy offering excellent wear resistance, corrosion resistance, and thermal stability, ideal for applications in extreme environments.

About Stellite 6

Name and Equivalent Name: Stellite 6 is a cobalt-chromium superalloy with the UNS designation R30006. It conforms to ASTM F75, B426, B659, and ISO 5832-4 standards, with equivalents such as DIN/EN 2.4771 and GB/T 15025: CoCrW6. It is also known under AMS 5894 and approved for use under ASME SB-75 and NACE MR0175 standards.

Stellite 6 Basic Introduction

Stellite 6 is a high-performance cobalt-based alloy renowned for its excellent resistance to wear, abrasion, and corrosion. Its high strength and hardness are maintained at elevated temperatures, making it suitable for extreme environments. This alloy is particularly effective in applications involving sliding wear, chemical exposure, and thermal cycling.

Stellite 6 performs well at temperatures up to 870°C, retaining strength and fatigue resistance. It is used in various industries, including aerospace, energy, oil & gas, and chemical processing, where components are exposed to high temperatures and harsh conditions. It finds applications in valve seats, turbine components, cutting tools, and coatings for wear-resistant surfaces.

custom-stellite-6-superalloy-components-equiaxed-crystal-casting-foundry

Alternative Superalloys of Stellite 6

Stellite 6 has several alternatives depending on the application. Stellite 21 offers improved corrosion resistance but with slightly lower hardness, making it suitable for chemical environments. Stellite 12 provides higher hardness and is used where extreme wear resistance is required.

Inconel 718 or Hastelloy C276 may be alternatives for high-temperature aerospace components. These alloys offer enhanced oxidation resistance and lower brittleness. Nimonic 90 or Rene 41 could be viable substitutes for applications involving higher mechanical stress.


Stellite 6 Design Intention

The design of Stellite 6 aims to balance wear resistance and corrosion protection while maintaining mechanical stability at high temperatures. It is intended for components that experience sliding wear, chemical exposure, and thermal fatigue. The alloy is designed to perform under harsh mechanical conditions, withstanding thermal cycling and abrasion over prolonged periods.

Its primary applications include valve seats, cutting tools, and turbine components. Stellite 6 ensures a long service life, reducing maintenance in critical applications where material failure is not an option. Its high performance in corrosive and high-temperature environments makes it a versatile choice across multiple industries.


Stellite 6 Chemical Composition

The key components in Stellite 6 offer a balance of wear resistance and corrosion protection. Chromium provides oxidation resistance, while tungsten improves hardness. Carbon contributes to strength but can increase brittleness if not appropriately managed.

Element

Composition (%)

Cobalt (Co)

Balance

Chromium (Cr)

27.0-32.0

Tungsten (W)

4.0-6.0

Carbon (C)

1.0-1.4

Nickel (Ni)

Max 3.0

Silicon (Si)

Max 1.0

Iron (Fe)

Max 3.0


Stellite 6 Physical Properties

Stellite 6 offers high density and thermal conductivity, contributing to its durability in demanding environments. Its thermal stability ensures excellent performance at elevated temperatures, with minimal wear and degradation.

Property

Value

Density (g/cm³)

8.79

Melting Point (°C)

1330

Thermal Conductivity (W/(m·K))

12.7

Elastic Modulus (GPa)

206


Metallographic Structure of Stellite 6 Superalloy

The metallographic structure of Stellite 6 features a cobalt-based matrix with finely dispersed carbides. Chromium and tungsten carbides reinforce the matrix, ensuring excellent wear resistance under sliding and abrasive conditions. The distribution of these carbides also enhances corrosion resistance by forming a protective oxide layer.

This alloy’s microstructure provides stability under thermal cycling, making it ideal for components exposed to high temperatures. Although the carbon content enhances strength, it can limit ductility, requiring careful machining and processing. Overall, the structure ensures long-term durability in extreme environments.


Stellite 6 Mechanical Properties

Stellite 6 exhibits excellent tensile and yield strength with high resistance to thermal fatigue. Its mechanical properties remain stable at elevated temperatures, making it suitable for applications under prolonged thermal stress.

Property

Value

Tensile Strength (MPa)

700-950

Yield Strength (MPa)

450-600

Creep Strength

Strong at 870°C

Hardness (HRC)

45-50

Elongation (%)

5-10%

Modulus of Elasticity (GPa)

205


Key Features of Stellite 6 Superalloy

  1. Outstanding Wear Resistance Stellite 6 provides exceptional resistance to sliding wear and abrasion. This makes it ideal for valve seats, cutting tools, and components exposed to mechanical friction, extending the lifespan of critical equipment.

  2. Thermal Stability at High Temperatures Stellite 6 maintains mechanical stability at temperatures up to 870°C. Its resistance to thermal fatigue ensures reliable performance in turbines, engines, and heat exchangers under extreme conditions.

  3. Excellent Corrosion Resistance With a high chromium content, Stellite 6 forms a protective oxide layer, offering superior resistance to oxidation and corrosion in chemical and marine environments.

  4. Resistance to Thermal Fatigue This alloy is designed to perform well under repeated thermal cycling. Its stable microstructure ensures durability in power generation turbines and aerospace applications, where temperature fluctuations are frequent.

  5. Limited Machinability but Good Weldability Stellite 6’s hardness can make machining difficult, often requiring grinding for precision. However, the alloy offers excellent weldability for hard-facing applications, enhancing wear resistance and reducing maintenance needs.

Stellite 6 Superalloy’s Machinability and Processing

  • Vacuum Investment Casting: Stellite 6 is suitable for vacuum investment casting due to its ability to maintain mechanical properties and corrosion resistance. This process ensures precise, oxidation-free components ideal for aerospace and chemical industries.

  • Single Crystal Casting: Stellite 6 is not applicable for single crystal casting since the alloy’s carbide microstructure disrupts the uniform grain structure required for creep resistance and strength in single-crystal components.

  • Equiaxed Crystal Casting: Stellite 6 performs well in equiaxed crystal casting, offering uniform mechanical properties and high wear resistance throughout the structure, making it ideal for valve seats and pump components.

  • Superalloy Directional Casting: Due to its carbide-rich microstructure, Stellite 6 is not ideal for directional casting, which requires specific grain orientation for enhanced high-temperature strength in aerospace applications.

  • Powder Metallurgy Turbine Disc: Stellite 6 is not commonly used in powder metallurgy for turbine discs due to its limited ductility, which makes it less suitable for rotating parts subjected to mechanical stress.

  • Superalloy Precision Forging: While Stellite 6’s brittleness limits its use in precision forging, it is used in overlays and wear-resistant coatings applied through precision hard-facing methods.

  • Superalloy 3D Printing: Stellite 6 presents challenges for 3D printing due to its hardness and carbide formation, which complicate the additive manufacturing process and require specialized heat treatments to reduce brittleness.

  • CNC Machining: Stellite 6 suits CNC machining but requires specialized tools and techniques. Its high hardness makes grinding necessary for precision, especially in components like valves and turbine blades.

  • Superalloy Welding: Stellite 6 is highly suitable for welding and is often used for hard-facing applications. The alloy’s wear and corrosion resistance make it ideal for extending the service life of critical components.

  • Hot Isostatic Pressing (HIP): HIP improves the mechanical properties of Stellite 6 by eliminating porosity, enhancing fatigue resistance, and ensuring a longer service life for components used in harsh environments.


Stellite 6 Superalloy Applications

  • Aerospace and Aviation: Stellite 6 is used for valve seats, turbine blades, and bearings in aerospace engines due to its excellent wear resistance and thermal stability at high temperatures.

  • Power Generation: In power plants, Stellite 6 is applied to steam turbines, control valves, and wear surfaces, providing durability and resistance to erosion in high-pressure environments.

  • Oil and Gas: Stellite 6 is used in valves, drilling tools, and refinery equipment, ensuring wear and corrosion resistance under abrasive conditions in oil and gas operations.

  • Energy: Stellite 6 is employed in thermal energy systems and gas turbines, providing reliable performance under repeated thermal cycling and mechanical wear.

  • Marine: Stellite 6 is used in propeller shafts, pumps, and other marine components that require protection against corrosion and wear from saltwater exposure.

  • Mining: In mining, Stellite 6 is applied to drill bits, crushers, and slurry pumps, providing excellent abrasion resistance in abrasive and high-stress conditions.

  • Automotive: The alloy is used in exhaust valves and other engine components, where wear resistance and thermal fatigue protection are essential for performance.

  • Chemical Processing: Stellite 6 is used in chemical reactors, pumps, and valves, providing long-term corrosion resistance in aggressive chemical environments.

  • Pharmaceutical and Food: The alloy ensures non-contaminating surfaces in food and pharmaceutical processing equipment, offering wear resistance and extended service life.

  • Military and Defense: Stellite 6 is employed in missile components, armor-piercing rounds, and other defense applications, offering high wear resistance under extreme conditions.

  • Nuclear: Stellite 6 is used for valve seats and seals in nuclear reactors, providing reliable performance under thermal and radiation exposure.


When to Choose Stellite 6 Superalloy

Custom superalloy parts made from Stellite 6 are ideal when high wear resistance, corrosion protection, and thermal stability are required. It performs exceptionally well in harsh environments where components face friction, mechanical wear, and chemical exposure. Stellite 6’s ability to maintain mechanical properties up to 870°C makes it a top choice for aerospace, power generation, and oil & gas applications.

This alloy is especially suitable for components such as valve seats, turbine blades, and bearings, which are subject to thermal cycling and abrasion. While its machinability can be challenging, Stellite 6 offers excellent weldability, making it ideal for hard-facing and overlay applications. For industries seeking reliable, long-lasting materials under extreme conditions, Stellite 6 is an optimal solution.

Explorer les blogs associés