Rene 104

Rene 104 is a high-performance nickel-chromium superalloy offering excellent creep resistance, fatigue strength, and thermal stability for turbine applications.

About Rene 104 Superalloy

Name and Equivalent Names

Rene 104 is a nickel-based superalloy designed to meet AMS 5835 standards. Although no specific ASTM or ISO equivalents exist, it is widely known for its superior performance in high-temperature turbine components. The alloy’s unique composition, which includes rhenium and hafnium, enhances its strength and creep resistance under extreme conditions.

Rene 104 Basic Introduction

Rene 104 is a nickel-chromium superalloy developed to withstand high-temperature stress and mechanical fatigue. It is specially designed for applications in aerospace and power generation turbines, where components are subjected to extreme thermal cycles. This alloy provides excellent creep resistance, maintaining strength and stability at temperatures up to 1000°C.

The alloy's metallurgical properties allow it to resist deformation under stress, making it an excellent choice for long-term use in turbine blades and discs. With superior fatigue strength and thermal conductivity, Rene 104 ensures efficiency and reliability in harsh environments, significantly extending the service life of critical components.

rene-104-superalloy-casting-and-forging-parts-cnc-machining-service-manufacturer

Alternative Superalloys of Rene 104

Inconel 718, Rene 95, and Hastelloy X are potential alternatives to Rene 104. Inconel 718 offers superior corrosion resistance and weldability, making it ideal for aerospace components. Rene 95 provides similar creep resistance but may not perform as well as Rene 104 under continuous high temperatures. Hastelloy X is known for its oxidation resistance and high-temperature stability, making it suitable for jet engines and gas turbines. The choice between these alloys depends on specific operational requirements.


Rene 104 Design Intention

Rene 104 was designed to meet the need for high-strength, creep-resistant materials capable of performing under prolonged high-temperature conditions. Its composition, including rhenium and hafnium, enhances the alloy’s thermal stability and fatigue resistance. This makes it ideal for turbine blades, where maintaining mechanical integrity under extreme stress is critical.

The alloy was explicitly developed for aerospace and power generation industries, where components are exposed to high thermal loads. With a design focus on creep rupture life and fatigue strength, Rene 104 ensures reliable performance, reducing the risk of mechanical failure over long operating periods.


Rene 104 Chemical Composition

The chemical composition of Rene 104 ensures high strength and stability under extreme conditions. Nickel forms the base, with chromium and cobalt providing oxidation resistance. Adding rhenium, hafnium, and boron improves the alloy’s high-temperature performance and grain boundary strength.

Element

Content (wt%)

Nickel (Ni)

Balance

Chromium (Cr)

11.0 – 13.0

Cobalt (Co)

11.0 – 13.0

Molybdenum (Mo)

3.0

Aluminum (Al)

4.5

Titanium (Ti)

4.5

Tungsten (W)

2.0

Hafnium (Hf)

0.2

Rhenium (Re)

3.0

Boron (B)

Max 0.03


Rene 104 Physical Properties

Rene 104 offers excellent density, thermal conductivity, and elastic modulus, making it ideal for components subjected to thermal stress. Its melting point and strength make it highly suitable for extreme environments.

Property

Value

Density (g/cm³)

8.7

Melting Point (°C)

1380

Thermal Conductivity (W/m·K)

10.5

Modulus of Elasticity (GPa)

212


Metallographic Structure of Rene 104 Superalloy

Rene 104 has a γ-phase nickel matrix with γ' (gamma prime) precipitates that enhance high-temperature strength. The γ' phase strengthens the alloy by preventing dislocation movement, ensuring stability during mechanical stress and thermal cycling.

The alloy benefits from adding rhenium and hafnium, which improve grain boundary strength and resistance to creep. This metallographic structure makes Rene 104 highly suitable for aerospace and power generation turbines, where components must endure extreme heat and mechanical loads without deformation or failure.


Rene 104 Mechanical Properties

Rene 104 demonstrates outstanding mechanical strength and creep resistance at elevated temperatures. It maintains structural integrity and fatigue resistance under extreme conditions, making it ideal for long-term turbine use.

Property

Value

Tensile Strength (MPa)

1250 – 1300

Yield Strength (MPa)

~1100

Creep Strength

Excellent at 1000°C

Hardness (HRC)

38 – 42

Elongation (%)

8 – 12

Elastic Modulus (GPa)

~220


Key Features of Rene 104 Superalloy

1. Exceptional Creep Resistance

Rene 104 provides excellent creep resistance, ensuring reliable performance at temperatures up to 1000°C. This makes it ideal for turbine components exposed to continuous mechanical stress and heat.

2. Strong Fatigue Resistance

The alloy offers superior fatigue resistance, enabling components to withstand cyclic thermal and mechanical loads without cracking or deforming, ensuring long service life.

3. High-Temperature Stability

With a melting point of 1380°C, Rene 104 remains stable under extreme heat, making it a preferred material for aerospace and energy applications.

4. Enhanced Grain Boundary Strength

Adding rhenium and hafnium improves grain boundary strength, preventing creep deformation and mechanical failure over extended periods of use.

5. Long Service Life

Rene 104 delivers exceptional durability, with a long creep rupture life that ensures consistent performance in critical systems like gas turbines and jet engines.

Rene 104 Superalloy’s Machinability

Rene 104 can be used in Vacuum Investment Casting due to its excellent thermal stability and ability to form precise, high-performance components for aerospace and energy industries.

The alloy is not typically employed in Single Crystal Casting as it is optimized for applications requiring polycrystalline structures, which enhance creep and fatigue resistance.

Rene 104 performs exceptionally well in Equiaxed Crystal casting, producing uniform grain structures contributing to its thermal and mechanical stability.

Superalloy Directional Casting can also be used with Rene 104, though its properties are often more effective in equiaxed forms, enhancing uniform performance.

The alloy is not ideal for powder metallurgy turbine disc manufacturing due to the challenges of maintaining consistent properties in powdered forms.

Rene 104 is compatible with Superalloy Precision Forging, allowing the production of components with high mechanical strength and stability under stress.

Superalloy 3D Printing is not preferred for Rene 104 because it is challenging to maintain uniform properties during additive manufacturing.

Rene 104 can be processed efficiently using CNC Machining, ensuring the precision and quality needed for critical aerospace and turbine components.

Welding Rene 104 requires specialized procedures, but with proper techniques, Superalloy Welding can create durable joints, maintaining their structural integrity.

Hot Isostatic Pressing (HIP) improves Rene 104’s mechanical properties by eliminating internal porosity, ensuring consistent strength and long service life.


Rene 104 Superalloy Applications

In Aerospace and Aviation, Rene 104 is used for turbine blades, discs, and structural components, ensuring high performance in extreme thermal conditions.

In Power Generation, the alloy is utilized in gas turbines, providing excellent thermal fatigue resistance and reliability under continuous operation.

Rene 104 supports the Oil and Gas industry by offering durability and corrosion resistance for valves, downhole tools, and high-pressure components.

The Energy sector benefits from Rene 104’s thermal stability, which ensures efficiency and long service life for turbine and heat exchange components.

In Marine applications, Rene 104’s corrosion resistance is ideal for exhaust systems and propulsion components exposed to seawater environments.

For Mining operations, Rene 104 provides wear resistance and durability for pumps, drill bits, and other heavy-duty components.

In the automotive industry, Rene 104 is applied to high-performance exhaust systems and turbochargers, ensuring thermal resistance and durability.

In Chemical Processing, Rene 104 provides oxidation resistance for reactors and heat exchangers exposed to extreme temperatures and corrosive chemicals.

The alloy supports the Pharmaceutical and Food industries by offering corrosion-resistant components like valves and seals used in harsh environments.

In Military and Defense, Rene 104 is employed in missile and jet engine components, ensuring reliability under extreme thermal and mechanical stress.

The Nuclear industry uses Rene 104 for reactor parts, where thermal fatigue and radiation resistance is essential for operational safety.


When to Choose Rene 104 Superalloy

Rene 104 should be selected for applications demanding long-term reliability, high-temperature performance, and resistance to fatigue and creep. It is particularly suitable for custom superalloy parts in gas turbines, jet engines, and energy systems, where components are exposed to continuous mechanical stress and thermal cycling.

This alloy is ideal for aerospace, oil and gas, and military defense, where components must withstand extreme environmental conditions. Its corrosion resistance also makes it a valuable material for marine and chemical processing applications. When performance and durability are critical, especially at temperatures above 1000°C, Rene 104 ensures operational efficiency and extended service life.