Français

Hastelloy W

Hastelloy W offers exceptional strength, fatigue, and corrosion resistance for high-temperature environments, which is ideal for aerospace and energy applications.

About Hastelloy W

Hastelloy W is also called Alloy W, designated by the UNS N10004. It meets ASTM standards B622 and B619 and is recognized under NACE MR0175 for corrosion resistance. This alloy is known for its excellent fatigue and thermal stress resistance, making it suitable for high-temperature operations.

Due to its nickel-based composition with additions of molybdenum and tungsten, Hastelloy W performs effectively at temperatures up to 900°C, providing reliable service in extreme environments. This alloy is often employed in specialized industrial applications where other materials fail under harsh thermal or mechanical stresses.

Hastelloy W Basic Introduction

Hastelloy W is a versatile superalloy primarily composed of nickel, molybdenum, and tungsten. Its unique chemical structure allows it to withstand severe fatigue and creep, common in high-stress environments such as aerospace and chemical processing.

This alloy is designed to maintain mechanical integrity and thermal fatigue resistance, even during prolonged exposure to elevated temperatures. Industries value it for applications where stability and reliability are paramount, including turbine components, chemical reactors, and heat exchangers.

custom-hastelloy-w-superalloy-components-manufacturing-company

Alternative Superalloys of Hastelloy W

Alternative alloys that offer similar performance include Hastelloy C-276 and Inconel 718. These alternatives are known for their high-temperature resistance and corrosion resistance. Hastelloy C-276, in particular, offers excellent resistance to chemical attack, making it ideal for harsh chemical processing environments.

Inconel 718, while also corrosion-resistant, provides superior mechanical strength and is often employed in turbine engines. Alloy W is preferable when a balance between fatigue strength, thermal stability, and creep resistance is critical.


Hastelloy W Design Intention

Hastelloy W was designed to excel in high-temperature environments with recurring thermal fatigue cycles. Its primary objective is to maintain strength and resistance under cyclic stress conditions. The alloy’s design also minimizes structural degradation during long-term exposure to high temperatures and mechanical loads.

Industries that deal with aggressive environments, such as chemical processing and aerospace, rely on Hastelloy W for its exceptional mechanical properties. Its molybdenum and tungsten content enhance its ability to resist both chemical corrosion and high-temperature fatigue, ensuring performance longevity.


Hastelloy W Chemical Composition

The chemical composition of Hastelloy W is formulated to ensure resistance to fatigue, creep, and thermal stress. Molybdenum and tungsten improve its high-temperature strength, while nickel is the base to ensure corrosion resistance.

Element

Composition (wt%)

Nickel (Ni)

Balance

Chromium (Cr)

4.0-6.0

Molybdenum (Mo)

22.0-25.0

Iron (Fe)

2.0-4.0

Tungsten (W)

3.5-5.0

Carbon (C)

0.05 max

Silicon (Si)

0.08 max


Hastelloy W Physical Properties

Hastelloy W exhibits excellent thermal conductivity and mechanical strength, making it ideal for high-temperature applications.

Property

Value

Density (g/cm³)

9.17

Melting Point (°C)

1370

Thermal Conductivity (W/(m·K))

8.7

Modulus of Elasticity (GPa)

206


Metallographic Structure of Hastelloy W Superalloy

Hastelloy W possesses a homogenous microstructure that withstands thermal cycling and creep conditions. The primary phase is a solid-solution nickel matrix, which imparts ductility and corrosion resistance. Secondary phases include carbides that provide additional strength at elevated temperatures.

The microstructure resists grain coarsening even during extended periods at high temperatures, maintaining mechanical stability. This structure enables the alloy to perform reliably under fluctuating thermal loads, preventing fatigue failure over long service periods.


Hastelloy W Mechanical Properties

Hastelloy W maintains mechanical integrity under harsh conditions, showing excellent fatigue resistance and high creep strength.

Mechanical Property

Value

Tensile Strength (MPa)

760

Yield Strength (MPa)

300-350

Hardness (HRC)

20-35

Elongation (%)

~50%

Elastic Modulus (GPa)

210


Key Features of Hastelloy W Superalloy

  1. High-Temperature Resistance Hastelloy W performs exceptionally well in temperatures up to 900°C, making it suitable for turbines, reactors, and heat exchangers.

  2. Thermal Fatigue Resistance The alloy's structure ensures minimal degradation during thermal cycling, making it ideal for applications exposed to fluctuating temperatures.

  3. Creep Resistance Hastelloy W provides excellent creep resistance, allowing it to maintain structural integrity over prolonged periods under mechanical stress.

  4. Corrosion Resistance The nickel-based composition ensures corrosion resistance, especially in chemically aggressive environments.

  5. Fatigue Strength It offers high fatigue strength, allowing it to endure cyclic stress conditions without mechanical failure, making it perfect for aerospace and industrial applications.

Hastelloy W Superalloy’s Machinability

  • Vacuum Investment Casting Hastelloy W can be effectively used in Vacuum Investment Casting due to its excellent thermal stability, enabling high-precision castings for complex shapes and high-temperature applications.

  • Single Crystal Casting Hastelloy W is unsuitable for Single Crystal Casting as it lacks the directional solidification properties necessary for single-crystal applications, such as turbine blades.

  • Equiaxed Crystal Casting Equiaxed Crystal Casting is compatible with Hastelloy W, providing uniform grain structures ideal for industrial components requiring mechanical stability.

  • Hastelloy W is generally not used in Superalloy Directional Casting as it is optimized for equiaxed grain structures rather than directional solidification.

  • Powder Metallurgy Turbine Disc Hastelloy W can be applied in Powder Metallurgy Turbine Disc manufacturing, offering excellent high-temperature strength and thermal fatigue resistance.

  • Precision Forging Superalloy Precision Forging with Hastelloy W is possible, producing high-strength components with enhanced fatigue resistance for demanding environments.

  • Superalloy 3D Printing Superalloy 3D Printing is feasible with Hastelloy W, allowing complex geometries and reducing material waste while retaining mechanical integrity.

  • CNC Machining Hastelloy W is suitable for CNC Machining due to its excellent machinability, producing precise parts for high-stress industrial applications.

  • Superalloy Welding Superalloy Welding is compatible with Hastelloy W, providing strong welds with minimal cracking, suitable for structural components exposed to thermal fatigue.

  • Hot Isostatic Pressing (HIP) Hot Isostatic Pressing (HIP) can enhance the mechanical properties of Hastelloy W, improving its performance by eliminating internal porosities.


Hastelloy W Superalloy Applications

  • Aerospace and Aviation Aerospace and Aviation applications include components in jet engines and gas turbines where high-temperature fatigue resistance is essential.

  • In Power Generation, Hastelloy W is used for heat exchangers and turbine components exposed to thermal stress.

  • Oil and Gas: Due to its corrosion resistance and strength, oil and Gas industries use Hastelloy W in chemical reactors and pipelines.

  • Energy In the energy sector, it is applied to heat exchangers and boilers, where stability under fluctuating temperatures is required.

  • Marine Marine applications include components exposed to seawater corrosion and thermal fatigue, such as pumps and valves.

  • Mining Mining industries use Hastelloy W for wear-resistant tools and equipment that are subjected to harsh environments and mechanical stress.

  • Automotive In Automotive applications, Hastelloy W, is used for exhaust components and turbocharger systems exposed to high temperatures.

  • Chemical Processing Chemical Processing plants rely on Hastelloy W for reactors and pipelines due to its corrosion resistance to aggressive chemicals.

  • Pharmaceutical and Food, Pharmaceutical and Food industries, use Hastelloy W for equipment requiring cleanliness and chemical corrosion resistance.

  • Military and Defense Military and defense sectors utilize Hastelloy W in high-performance systems that need reliability under extreme stress.

  • Nuclear Nuclear industries use Hastelloy W in reactors and containment systems due to its resistance to high temperatures and radiation.


When to Choose Hastelloy W Superalloy

Hastelloy W is ideal for environments requiring superior fatigue resistance, high-temperature stability, and corrosion resistance. It excels in demanding aerospace, chemical processing, and power generation sectors. If you need custom superalloy parts, visit Custom Superalloy Parts for tailored solutions. This alloy offers long service life and mechanical reliability in high-stress, high-temperature applications, making it a trusted material across various industries.