Ti-6Al-7Nb titanium alloy offers excellent corrosion resistance, biocompatibility, and fatigue strength, ideal for medical implants and aerospace components.

About Ti-6Al-7Nb Superalloy

Ti-6Al-7Nb, also known as Titanium Grade 7Nb, is a high-performance titanium alloy. With UNS designation R56700, it meets ASTM F1295 and DIN/EN 3.7176 standards. Known for its biocompatibility and fatigue resistance, it is widely applied in the medical field and aerospace applications.

This alloy was developed as an alternative to Ti-6Al-4V, particularly for biomedical applications. Substituting vanadium with niobium eliminates concerns regarding its potential toxicity, making it suitable for long-term implantation. It offers excellent corrosion resistance, especially in saline environments.

Ti-6Al-7Nb Basic Introduction

Ti-6Al-7Nb was designed primarily for biomedical applications due to its excellent biocompatibility. Its properties include high fatigue resistance, corrosion resistance, and good mechanical strength, which make it ideal for orthopedic and dental implants.

In addition to medical uses, Ti-6Al-7Nb is useful in aerospace due to its mechanical stability and ability to withstand moderate temperatures. The combination of strength and lightweight properties ensures that it can be used effectively in environments with critical performance and durability.

ti-6al-7nb-titanium-parts-casting-and-cnc-machining-service

Alternative Superalloys of Ti-6Al-7Nb

Alternative materials for Ti-6Al-7Nb include Ti-6Al-4V (TC4), known for its similar strength but low biocompatibility. Another option is Ti-6Al-4V ELI, used for medical implants but may not have the same corrosion resistance in saline environments as Ti-6Al-7Nb.

Cobalt-chromium alloys are another alternative for medical implants but tend to be heavier. Stainless steel alloys, though cheaper, do not offer the same biocompatibility or corrosion resistance. NiTi alloys are also considered in some applications where shape-memory properties are needed.


Ti-6Al-7Nb Design Intention

The design intention of Ti-6Al-7Nb is focused on improving the performance and safety of implants and aerospace components. The substitution of niobium for vanadium enhances biocompatibility while maintaining excellent mechanical properties. It ensures long-term stability under stress and fatigue loads.

The alloy’s corrosion resistance is especially beneficial in saline environments, making it a preferred choice for implants that contact bodily fluids. Its use extends beyond biomedical applications to aerospace, where weight savings and mechanical integrity are essential.


Ti-6Al-7Nb Chemical Composition

Including niobium (6.5-7.5%) in Ti-6Al-7Nb enhances its biocompatibility, while aluminum (5.5-6.75%) provides strength without increasing density. Together, these elements create a lightweight, strong, and corrosion-resistant material.

Element

Composition (wt%)

Aluminum (Al)

5.5 – 6.75

Niobium (Nb)

6.5 – 7.5

Iron (Fe)

Max 0.20

Titanium (Ti)

Balance


Ti-6Al-7Nb Physical Properties

Ti-6Al-7Nb has a 4.48 g/cm³ density, making it lightweight with good thermal conductivity and elasticity. It offers high melting points and moderate strength.

Property

Value

Density (g/cm³)

4.48

Melting Point (°C)

1650

Tensile Strength (MPa)

860

Thermal Conductivity (W/m·K)

7.4

Modulus of Elasticity (GPa)

113


Metallographic Structure of Ti-6Al-7Nb Superalloy

Ti-6Al-7Nb features a biphasic microstructure composed of alpha and beta phases. The alpha phase ensures corrosion resistance and stability, while the beta phase contributes to the alloy's ductility and strength. This combination provides excellent fatigue resistance and mechanical stability.

The niobium content promotes the stabilization of the beta phase, ensuring mechanical strength at elevated temperatures. This balance between phases makes Ti-6Al-7Nb highly effective for applications requiring cyclic loading and long-term structural reliability.


Ti-6Al-7Nb Mechanical Properties

Ti-6Al-7Nb offers excellent mechanical strength and fatigue properties, with a tensile strength of 900 MPa and yield strength of 800 MPa. It performs well in moderate temperatures up to 350°C.

Property

Value

Tensile Strength (MPa)

900

Yield Strength (MPa)

800

Elongation (%)

15 – 20

Hardness (HRC)

25 – 30

Modulus of Elasticity (GPa)

110 – 115


Key Features of Ti-6Al-7Nb Superalloy

  1. Biocompatibility Ti-6Al-7Nb is specifically designed for medical implants, ensuring long-term safety in contact with biological tissues. Its composition avoids the potential toxicity of vanadium.

  2. Corrosion Resistance The alloy exhibits excellent corrosion resistance, particularly in saline environments, making it ideal for implants and marine applications.

  3. Fatigue Resistance Ti-6Al-7Nb provides high fatigue strength, enabling it to withstand cyclic loads over extended periods, which is crucial for both implants and aerospace components.

  4. Thermal Stability The alloy maintains mechanical performance up to 350°C, making it suitable for moderate-temperature environments.

  5. Lightweight Strength With a density of 4.48 g/cm³, Ti-6Al-7Nb combines lightweight properties with mechanical strength, making it ideal for aerospace applications.

Ti-6Al-7Nb Superalloy’s Machinability

Vacuum Investment Casting Ti-6Al-7Nb is not typically used in Vacuum Investment Casting because its properties are better suited for CNC machining and biomedical applications rather than complex casting processes.

Single Crystal Casting This alloy is unsuitable for Single Crystal Casting as it lacks the required properties for high-temperature turbine blades and similar components.

Equiaxed Crystal Casting Although Equiaxed Crystal Casting is suitable for strength-demanding parts, Ti-6Al-7Nb is better applied in biomedical and aerospace fields due to its biocompatibility and fatigue resistance.

Directional Casting Ti-6Al-7Nb is not recommended for Directional Casting since other alloys provide better performance for high-temperature and structural applications.

Powder Metallurgy Turbine Disc The alloy does not meet the specific requirements for powder metallurgy turbine disc applications, which need exceptional creep resistance at high temperatures.

Precision Forging Ti-6Al-7Nb performs well in Superalloy Precision Forging, especially in medical implants and lightweight aerospace parts.

Superalloy 3D Printing The alloy is ideal for Superalloy 3D Printing, allowing for precise, lightweight parts in the aerospace and biomedical sectors.

CNC Machining Superalloy CNC Machining is a preferred method for shaping Ti-6Al-7Nb into medical and aerospace components, thanks to its excellent machinability.

Superalloy Welding While not commonly welded, superalloy welding can be performed using advanced techniques to meet aerospace requirements.

Hot Isostatic Pressing (HIP) Hot Isostatic Pressing (HIP) effectively enhances the mechanical properties of Ti-6Al-7Nb, improving its fatigue life and structural integrity.


Ti-6Al-7Nb Superalloy Applications

Aerospace and Aviation Ti-6Al-7Nb is widely used in Aerospace and Aviation due to its lightweight, fatigue, and corrosion resistance in structural components.

Power Generation The alloy finds applications in Power Generation, particularly in auxiliary parts that require lightweight and durable materials.

Oil and Gas Ti-6Al-7Nb suits oil and Gas components exposed to corrosive environments, ensuring durability and reliability.

Energy In the Energy sector, the alloy is used in lightweight components subjected to stress and cyclic loads.

Marine Ti-6Al-7Nb performs well in Marine environments, offering corrosion resistance and strength for parts exposed to seawater.

Mining In Mining, the alloy’s wear resistance and durability make it ideal for drilling components and equipment use.

Automotive Ti-6Al-7Nb is increasingly used in Automotive applications for high-performance, lightweight parts.

Chemical Processing The alloy is effective in Chemical Processing equipment where corrosion resistance is essential for longevity.

Pharmaceutical and Food In the Pharmaceutical and Food industries, Ti-6Al-7Nb’s biocompatibility and corrosion resistance make it ideal for processing equipment.

Military and Defense Ti-6Al-7Nb is valuable in Military and Defense applications for lightweight armor and aerospace components.

Nuclear The alloy is well-suited for nuclear applications and has high durability and corrosion resistance.


When to Choose Ti-6Al-7Nb Superalloy

Ti-6Al-7Nb is the go-to material for biocompatibility, fatigue, and corrosion resistance. It excels in medical implants, offering long-term reliability and safety. In aerospace, it provides lightweight strength and fatigue resistance critical for structural components. Ti-6Al-7Nb ensures excellent performance under stress and in corrosive environments for chemical, energy, and marine applications.

Custom superalloy parts made from Ti-6Al-7Nb for custom applications deliver the precision and reliability needed for challenging sectors. Whether in medical devices or aerospace systems, this alloy perfectly balances strength and weight, making it an ideal solution.