Hastelloy S

Hastelloy S is a high-performance alloy known for exceptional thermal resistance, cyclic fatigue strength, and durability in harsh, high-temperature environments.

About Hastelloy S

Hastelloy S, designated by UNS N06635, is a superalloy designed to excel under extreme conditions. It is recognized for its thermal stability, high strength, and corrosion resistance, particularly in cyclic environments. This alloy is used where performance under severe thermal stress is essential.

Hastelloy S Basic Introduction

Hastelloy S is a nickel-based superalloy with chromium content ranging between 15.0-17.0%, designed for high-temperature operations. It offers high fatigue strength, even in environments subject to cyclic thermal variations. Known for its stability at elevated temperatures, it finds applications in aerospace, energy production, and chemical industries where materials are exposed to extreme heat.

Due to its long-term durability in challenging conditions, Hastelloy S provides a reliable solution for components subjected to thermal and mechanical stress. The alloy maintains strength and structural integrity over long periods, even at elevated temperatures.

custom-hastelloy-s-superalloy-components-manufacturing-company

Alternative Superalloys of Hastelloy S

Alternatives to Hastelloy S include Inconel 625, which offers thermal and mechanical stability. Inconel 718 is another option, especially where creep resistance is needed. Hastelloy C-276 may be considered for applications requiring superior corrosion resistance alongside high-temperature performance.

These alternatives provide similar properties but may differ in weldability, fatigue resistance, or corrosion behavior, making them suitable for different industrial applications.


Hastelloy S Design Intention

Hastelloy S was developed to meet the needs of industries requiring materials that withstand high thermal stress and cyclic conditions. The alloy is primarily used in environments involving extreme temperatures, providing reliable fatigue strength. Its design ensures resistance to mechanical deformation over extended periods at elevated temperatures.

In addition to thermal stability, the alloy's chemical composition contributes to enhanced oxidation resistance. The alloy is suitable for aerospace and power generation applications, where exposure to thermal fatigue and chemical attack is expected.


Hastelloy S Chemical Composition

The carefully balanced composition of Hastelloy S ensures high thermal fatigue resistance. Chromium provides oxidation resistance, while nickel ensures stability at elevated temperatures.

Element

Composition (%)

Nickel (Ni)

Balance

Chromium (Cr)

15.0-17.0

Iron (Fe)

3.0 max

Carbon (C)

0.015 max

Other Elements

Trace amounts


Hastelloy S Physical Properties

Hastelloy S offers excellent mechanical and thermal stability. Its density and thermal conductivity ensure it performs well in high-temperature environments.

Property

Value

Density (g/cm³)

8.86

Melting Point (°C)

1390

Thermal Conductivity (W/(m·K))

10.2

Modulus of Elasticity (GPa)

202


Metallographic Structure of Hastelloy S Superalloy

Hastelloy S exhibits a stable face-centered cubic (FCC) crystal structure, which provides excellent strength and ductility at high temperatures. The alloy’s microstructure remains stable over long periods of thermal exposure, preventing phase transformations that could degrade mechanical performance.

The distribution of chromium ensures enhanced oxidation resistance throughout the matrix, while the nickel-rich structure stabilizes the alloy during cyclic thermal operations. The alloy maintains high resistance to stress corrosion cracking, a crucial factor in applications involving cyclic temperature changes.


Hastelloy S Mechanical Properties

The mechanical properties of Hastelloy S ensure it remains reliable under thermal stress and mechanical load.

Property

Value

Tensile Strength (MPa)

750-800

Yield Strength (MPa)

300-400

Hardness (HRC)

20-35

Elongation (%)

~50

Elastic Modulus (GPa)

210


Key Features of Hastelloy S Superalloy

  1. Thermal Stability Hastelloy S excels in high-temperature environments, maintaining mechanical integrity at temperatures up to 800°C. This makes it ideal for applications in the aerospace and energy sectors.

  2. Resistance to Thermal Fatigue The alloy offers excellent fatigue resistance under cyclic thermal conditions, ensuring long service life in challenging environments.

  3. Corrosion Resistance With its balanced chromium content, Hastelloy S resists oxidation and chemical corrosion, ensuring durability in oxidizing and reducing environments.

  4. Mechanical Strength The alloy retains high tensile and yield strength even at elevated temperatures, making it a reliable choice for structural components under thermal stress.

  5. Long-Term Durability Hastelloy S offers extended service life, performing well in harsh environments involving thermal and chemical stress over long periods.

Hastelloy S Superalloy’s Machinability

Vacuum Investment Casting: Hastelloy S is suitable for use in Vacuum Investment Casting due to its ability to maintain chemical stability and structural integrity in complex castings. However, its limited ductility may necessitate additional heat treatments.

Single Crystal Casting: Hastelloy S is not typically used in Single Crystal Casting as it lacks the microstructural properties required for single-crystal formation.

Equiaxed Crystal Casting: The alloy can be utilized in Equiaxed Crystal Casting due to its balanced mechanical properties and ease of solidification, making it suitable for applications requiring standard crystal structures.

Directional Casting: Hastelloy S is less suited for Superalloy Directional Casting due to its lower creep resistance than other directional cast superalloys.

Powder Metallurgy Turbine Disc: Despite high thermal resistance, Hastelloy S is not ideal for Powder Metallurgy Turbine Disc production due to its chemical limitations in powder consolidation.

Precision Forging: Hastelloy S can be used in Superalloy Precision Forging, offering high thermal resistance. However, close control of forging parameters is needed to prevent cracking.

Superalloy 3D Printing: Due to its thermal stability, Hastelloy S performs well in Superalloy 3D Printing for high-temperature parts, provided proper printing parameters are applied.

CNC Machining: Hastelloy S is well-suited for CNC Machining due to its stability and strength. Specialized cutting tools and cooling methods are recommended for effective machining.

Superalloy Welding: Hastelloy S performs well in Superalloy Welding with a careful selection of welding methods to avoid cracking, particularly under cyclic thermal loads.

Hot Isostatic Pressing (HIP): The alloy can undergo Hot Isostatic Pressing (HIP) to improve mechanical properties and eliminate internal porosity, making it more reliable for demanding applications.


Hastelloy S Superalloy Applications

Aerospace and Aviation: Hastelloy S is ideal for Aerospace and Aviation applications due to its ability to withstand high temperatures and thermal fatigue, especially in engines and turbines.

Power Generation: The alloy performs well in Power Generation applications like gas turbines, providing reliable service under cyclic thermal stress.

Oil and Gas: Hastelloy S is commonly used in Oil and Gas operations where materials are exposed to harsh chemicals and high temperatures, ensuring structural durability.

Energy: In Energy applications, it offers excellent resistance to stress and fatigue, making it suitable for high-temperature heat exchangers.

Marine: Due to its excellent corrosion resistance, Marine industries use Hastelloy S for components exposed to harsh seawater environments.

Mining: The alloy’s durability makes it ideal for Mining equipment, ensuring reliable performance under thermal and mechanical stress.

Automotive: In Automotive applications, Hastelloy S is used for exhaust components where high-temperature stability is critical.

Chemical Processing: The alloy performs well in Chemical Processing, handling aggressive chemicals and maintaining stability at elevated temperatures.

Pharmaceutical and Food: In the Pharmaceutical and Food industries, Hastelloy S offers reliability under thermal cycling conditions in production equipment.

Military and Defense: Military and defense sectors utilize alloy for equipment subjected to harsh environmental conditions and extreme temperatures.

Nuclear: Hastelloy S finds applications in Nuclear reactors due to its resistance to high-temperature environments and radiation damage.


When to Choose Hastelloy S Superalloy

Hastelloy S is a premium choice for high-temperature environments where materials must resist thermal fatigue and maintain mechanical stability. Its applications range from aerospace turbines and power generation to chemical processing plants. Custom superalloy parts crafted from Hastelloy S provide excellent performance under cyclic stresses, making it indispensable in industries where long-term reliability is critical.

This alloy is ideal for heat exchangers, gas turbines, and exhaust systems, where its stability under cyclic thermal loads ensures long service life. Additionally, industries requiring high-performance materials under aggressive chemical and environmental conditions benefit from the durability of Hastelloy S.