Inconel 738LC

Inconel 738LC, a high-performance superalloy, offers exceptional thermal resistance, creep strength, and fatigue resistance at elevated temperatures.

About Inconel 738LC Superalloy

Inconel 738LC, or Alloy 738LC, complies with ASTM B637 and DIN/EN 2.4652 standards. In China, it is classified under GB/T 14992: GH738LC. This superalloy contains a significant proportion of nickel, complemented by chromium, aluminum, titanium, and tungsten, to ensure superior high-temperature performance.

The alloy is primarily utilized in aerospace and power generation sectors, where high thermal fatigue resistance and mechanical integrity are essential. Its stable properties under extreme temperatures make it ideal for turbine blades and combustion chambers, ensuring reliability in critical operations.

Inconel 738LC Basic Introduction

Inconel 738LC is renowned for its outstanding strength and resistance to oxidation at elevated temperatures. It is specifically designed for applications demanding prolonged exposure to high heat, such as gas turbines and jet engines.

The alloy's composition includes gamma-prime strengthening precipitates, enabling it to maintain mechanical performance during thermal cycling. This characteristic makes it ideal for environments with fluctuating thermal conditions, providing increased component lifespan and reduced maintenance.

custom-inconel-738lc-superalloy-vacuum-investment-castings

Alternative Superalloys of Inconel 738LC

Alternatives to Inconel 738LC include Inconel 718, Rene 80, and Mar-M247. Inconel 718 offers superior weldability, making it suitable for complex structures. Rene 80 and Mar-M247 are often employed in applications requiring directional solidification to enhance mechanical properties.

These alternatives are chosen based on specific application requirements, such as manufacturing constraints or enhanced resistance to stress rupture. The selection between these alloys depends on the desired trade-off between manufacturability, cost, and mechanical performance.

Inconel 738LC Design Intention

Inconel 738LC is designed to provide exceptional creep and fatigue resistance at high temperatures. Its composition ensures durability under extreme mechanical stress, maintaining structural integrity over extended periods.

This alloy is optimized for turbine applications, where components must withstand continuous exposure to high temperatures and mechanical loads. Its thermal fatigue resistance makes it an excellent material for jet engines and stationary power turbines, reducing maintenance requirements and extending service life.

Inconel 738LC Chemical Composition

Inconel 738LC's chemical composition is designed for high-temperature applications. Aluminum and titanium contribute to gamma-prime phase formation, enhancing strength. Cobalt and tungsten improve fatigue resistance and durability.

Element

Composition (%)

Nickel (Ni)

60.0–65.0

Chromium (Cr)

15.5–16.5

Aluminum (Al)

3.4–3.8

Titanium (Ti)

3.4–3.8

Cobalt (Co)

Balance

Tungsten (W)

1.5

Inconel 738LC Physical Properties

Inconel 738LC has a high melting point and excellent thermal conductivity, providing stability in high-temperature applications.

Property

Value

Density

8.12 g/cm³

Melting Point

1300°C

Thermal Conductivity

10.7 W/(m·K)

Modulus of Elasticity

210 GPa

Metallographic Structure of Inconel 738LC Superalloy

Inconel 738LC features a gamma matrix reinforced by gamma-prime precipitates, which provide excellent creep resistance. The alloy’s microstructure includes carbides along grain boundaries, enhancing resistance to grain boundary sliding.

This unique metallurgical structure enables the alloy to maintain mechanical integrity during long-term exposure to high temperatures and mechanical loads, ensuring reliable performance in turbine and aerospace applications.

Inconel 738LC Mechanical Properties

Inconel 738LC maintains superior mechanical strength and fatigue resistance at elevated temperatures, making it ideal for critical applications.

Property

Value

Tensile Strength

1100 MPa

Yield Strength

900 MPa

Hardness

Rockwell C40-45

Elongation

10-12%

Fatigue Strength

450 MPa

Key Features of Inconel 738LC Superalloy

  1. High-Temperature Strength Inconel 738LC retains mechanical strength at temperatures up to 982°C, ensuring reliable performance in challenging environments.

  2. Oxidation Resistance Its high chromium and aluminum content provide superior resistance to oxidation, preventing material degradation in high-temperature gases.

  3. Creep Resistance The alloy's gamma-prime strengthening ensures it maintains structural integrity under prolonged mechanical stress at high temperatures.

  4. Fatigue Resistance Inconel 738LC excels in cyclic environments, making it ideal for applications requiring resistance to thermal fatigue.

  5. Corrosion Resistance This superalloy offers excellent corrosion resistance in aggressive environments, ensuring long service life with minimal maintenance.

Inconel 738LC Superalloy’s Machinability

Inconel 738LC can be effectively used in Vacuum Investment Casting due to its stability at high temperatures and oxidation resistance. This technique ensures the precision required for aerospace components by minimizing defects during production.

However, Inconel 738LC is not suited for Single Crystal Casting. Its composition is optimized for equiaxed grain structures, making it unsuitable for achieving the unidirectional properties needed in single-crystal turbine blades.

Inconel 738LC performs well in Equiaxed Crystal Casting, maintaining excellent fatigue resistance and thermal stability. This casting method aligns with the alloy’s properties, ensuring high-performance parts for high-temperature applications.

It is also applicable in Superalloy Directional Casting. The controlled grain structure in directional casting enhances the alloy’s creep resistance, making it ideal for turbine components exposed to mechanical stress.

The alloy is recommended for Powder Metallurgy Turbine Disc applications. Its has high yield strength and tensile strength

Inconel 738LC is not ideal for Superalloy Precision Forging. The alloy's mechanical properties are optimized for casting, not deformation-based processes like forging.

Superalloy 3D Printing is unsuitable for Inconel 738LC due to its composition and microstructure, which are challenging to maintain during additive manufacturing.

The alloy performs well in CNC Machining due to its excellent mechanical properties and thermal stability. However, specialized cutting tools are required due to their hardness.

Inconel 738LC is not ideal for Superalloy Welding. Its high alloying content makes welding challenging, with risks of cracking. Pre- and post-weld treatments are necessary to avoid issues.

Hot Isostatic Pressing (HIP) is beneficial for Inconel 738LC. HIP enhances mechanical properties and reduces internal voids, ensuring reliable performance in high-stress environments.

Inconel 738LC Superalloy Applications

In the Aerospace and Aviation industry, Inconel 738LC is used for turbine blades and combustion chambers due to its exceptional thermal fatigue resistance.

In the power generation industry, this alloy is employed in gas turbines to improve operational efficiency and to withstand continuous high temperatures.

In the Oil and Gas sector, Inconel 738LC is used in heat exchangers and valves, providing corrosion resistance in harsh environments.

The Energy industry relies on Inconel 738LC for components that endure long-term exposure to extreme heat, ensuring system reliability.

In the marine sector, this alloy is applied to exhaust systems and turbine parts, resisting corrosion in marine environments.

In the Mining industry, Inconel 738LC is utilized in equipment exposed to high temperatures and wear, ensuring durability.

The Automotive industry uses Inconel 738LC for high-performance engines, particularly turbochargers.

In the Chemical Processing industry, the alloy’s corrosion resistance is essential for reactors and heat exchangers.

In the Pharmaceutical and Food industry, Inconel 738LC ensures contamination-free operations in high-temperature sterilization equipment.

In the Military and Defense sector, the alloy is used for jet engines and missile components, providing high mechanical performance.

In the Nuclear industry, Inconel 738LC ensures reactor safety by maintaining integrity under radiation and high heat.

When to Choose Inconel 738LC Superalloy

Inconel 738LC is ideal for applications requiring high thermal fatigue resistance and excellent mechanical properties at elevated temperatures. It excels in environments where components are exposed to sustained heat and mechanical stress, such as turbine blades in aerospace and power generation. This alloy offers significant advantages if long-term durability and reduced maintenance are priorities.

For manufacturers needing custom superalloy parts, Inconel 738LC’s resistance to creep, fatigue, and oxidation makes it an excellent choice. Its compatibility with advanced casting techniques ensures optimal performance and reliability, particularly in critical industries like energy and aviation.