Русский

Stellite 1

Stellite 1 is a cobalt-based superalloy known for exceptional wear resistance, thermal stability, and high strength, performing reliably at elevated temperatures up to 870°C.

About Stellite 1

Name and Equivalent Names: Stellite 1 is an American cobalt-chromium superalloy with the UNS designation R30001. It meets several standards, including ASTM B426 and ISO 5832-4. While it has no direct equivalents in DIN, BS, or GB/T standards, it is commonly called a cobalt-chromium alloy.

Stellite 1 Basic Introduction

Stellite 1 is a cobalt-based superalloy renowned for its exceptional wear and corrosion resistance under high temperatures and harsh environments. It contains chromium and tungsten, providing a protective oxide layer for superior performance in challenging conditions.

Designed to retain its hardness up to 870°C, Stellite 1 is used in industries such as aerospace, power generation, and oil & gas. Its high thermal stability, strength, and resistance to mechanical fatigue make it suitable for turbine components, valve seats, and wear-resistant coatings.

custom-stellite-1-superalloy-components-equiaxed-crystal-casting-foundry

Alternative Superalloys of Stellite 1

Alternatives to Stellite 1 include other cobalt- and nickel-based alloys with similar wear resistance and thermal stability. Examples include Stellite 6 and 12, known for slightly lower hardness but improved machinability.

Inconel 718 or Hastelloy C276 offers reasonable alternatives for high-wear or corrosive environments, with the added benefit of corrosion resistance in extreme chemical conditions. These alloys may be selected over Stellite 1 when reduced brittleness or increased toughness is required for marine or chemical processing equipment applications.


Stellite 1 Design Intention

Stellite 1 was developed to endure extreme wear, corrosion, and high temperatures, making it a go-to material for severe environments. It is used primarily where components experience high thermal stress and friction, such as valve seats, turbine blades, and coatings for cutting tools.

The alloy’s design focuses on maintaining hardness at elevated temperatures and minimizing degradation under mechanical and thermal fatigue. With good creep rupture life and excellent oxidation resistance, it is particularly useful for aerospace, energy, and oil industries.


Stellite 1 Chemical Composition

Stellite 1 contains a high cobalt concentration, providing a solid matrix with superior wear resistance. Chromium (29-32%) enhances corrosion resistance, while tungsten (12-15%) contributes to hardness. A small amount of carbon (2.4-3.0%) increases strength, but excessive nickel (max 3%) is limited to prevent embrittlement.

Element

Composition (%)

Cobalt (Co)

Balance

Chromium (Cr)

29.0-32.0

Tungsten (W)

12.0-15.0

Carbon (C)

2.4-3.0

Nickel (Ni)

Max 3.0

Silicon (Si)

Max 1.0

Iron (Fe)

Max 3.0


Stellite 1 Physical Properties

Stellite 1 offers high density, excellent thermal conductivity, and superior performance under high-temperature conditions. It has a melting point of 1315°C, allowing it to perform well under heat-intensive applications.

Property

Value

Density (g/cm³)

8.87

Melting Point (°C)

1315

Thermal Conductivity (W/(m·K))

14.5

Elastic Modulus (GPa)

205


Metallographic Structure of Stellite 1 Superalloy

Stellite 1 exhibits a dense, face-centered cubic (FCC) cobalt matrix reinforced by carbides dispersed throughout the structure. The carbides, primarily chromium and tungsten-based, provide superior hardness and wear resistance.

Due to its high carbon content, Stellite 1 has a microstructure that resists deformation, even under extreme conditions. However, this structure can make the alloy brittle, requiring specialized machining and finishing processes such as grinding to achieve desired shapes and dimensions.


Stellite 1 Mechanical Properties

Stellite 1 has excellent tensile and yield strength, even at high temperatures. It maintains mechanical stability up to 870°C and resists fatigue and creep under prolonged thermal stress.

Property

Value

Tensile Strength (MPa)

900

Yield Strength (MPa)

500

Creep Strength

Stable at 870°C

Hardness (HRC)

55-60

Elongation (%)

2-5%

Modulus of Elasticity (GPa)

210


Key Features of Stellite 1 Superalloy

  1. Exceptional Wear Resistance Stellite 1 is designed for high-friction environments, such as valve components and cutting tools. Its hardness ensures a long service life under abrasive conditions, even at elevated temperatures.

  2. High Thermal Stability This alloy maintains structural integrity and mechanical properties at temperatures up to 870°C. Its ability to resist thermal fatigue makes it suitable for high-temperature environments like turbines and engines.

  3. Corrosion and Oxidation Resistance The chromium content in Stellite 1 forms a protective oxide layer, shielding it from oxidation and corrosion in harsh chemical or marine environments and extending the component lifespan.

  4. Good Creep Strength and Fatigue Resistance With high creep strength at elevated temperatures, Stellite 1 resists deformation under long-term mechanical stress. Its fatigue resistance also ensures durability under cyclic loading.

  5. Challenges in Machinability Stellite 1’s hardness, while beneficial for performance, make it difficult to machine. Precision grinding and advanced machining techniques are required for shaping, making it better suited for wear-resistant coatings and hard-facing applications.

Stellite 1 Superalloy’s Machinability and Processing

Stellite 1 is challenging to machine due to its extreme hardness and wear resistance, typically requiring grinding instead of conventional machining. It can be effectively employed in applications such as CNC Machining for final finishing processes, but tooling wear must be managed.

  • Vacuum Investment Casting: Stellite 1 is suitable for this process due to its ability to withstand high temperatures and retain hardness, which makes it a good candidate for producing intricate, high-performance parts.

  • Single Crystal Casting: Stellite 1 is generally unsuitable for single-crystal casting because it forms carbide precipitates and lacks the single-crystal microstructure needed to enhance creep resistance in aerospace turbine blades.

  • Equiaxed Crystal Casting: Stellite 1 is applicable in this process, especially for components requiring uniform properties throughout the material, such as wear-resistant parts.

  • Superalloy Directional Casting: Stellite 1 is less suitable for this casting method due to its inability to form directional grains effectively, which prioritizes high-temperature strength along specific grain directions.

  • Powder Metallurgy Turbine Disc: Stellite 1 is rarely used in powder metallurgy for turbine discs due to its high carbon content and limited creep strength, which restricts its suitability for rotating high-stress components.

  • Superalloy Precision Forging: Stellite 1’s brittleness makes it less suitable for precision forging, as it lacks the necessary ductility for deformation during forging processes.

  • Superalloy 3D Printing: Although 3D printing technologies are advancing, Stellite 1’s properties make it challenging to use effectively in additive manufacturing due to issues with brittleness and cracking during solidification.

  • Superalloy Welding: Stellite 1 is frequently used for hardfacing through welding. It provides wear-resistant overlays on valve seats, cutting tools, and other components subject to high abrasion.

  • Hot Isostatic Pressing (HIP): HIP is suitable for improving the density and mechanical properties of Stellite 1, especially for critical aerospace components, by eliminating internal porosity and enhancing fatigue resistance.


Stellite 1 Superalloy Applications

  • Aerospace and Aviation: Stellite 1 is used for hard-facing aircraft engine components, including valves and combustion chambers, ensuring high wear resistance under extreme temperatures.

  • Power Generation: In power plants, Stellite 1 is applied to steam turbine blades and valves, resisting erosion and corrosion, especially in high-pressure environments.

  • Oil and Gas: Stellite 1 performs well in drilling tools, valve seats, and refinery equipment, where wear resistance is critical under extreme pressure and corrosive conditions.

  • Energy: The alloy is used in thermal power plants and energy systems for components requiring durability under high stress and thermal fatigue.

  • Marine: Stellite 1 is ideal for marine applications where resistance to saltwater corrosion and mechanical wear is essential, such as propeller shafts and pump components.

  • Mining: In mining, Stellite 1 is used in drill bits, crushers, and slurry pumps, providing long-lasting wear resistance in abrasive environments.

  • Automotive: Although less common, Stellite 1 is sometimes employed in high-performance automotive engines for exhaust valves, ensuring high-temperature durability.

  • Chemical Processing: The alloy is used in chemical reactors, valves, and pumps where corrosion resistance is essential in aggressive chemical environments.

  • Pharmaceutical and Food: Stellite 1 finds limited use in pharmaceutical and food applications, mainly for valve seats and processing equipment requiring wear resistance and non-contaminating properties.

  • Military and Defense: The alloy is used for armor-piercing rounds, missile components, and other critical defense equipment, offering wear resistance and strength.

  • Nuclear: In nuclear power plants, Stellite 1 is applied to valves and seals that require high radiation resistance and stability under thermal cycling conditions.


When to Choose Stellite 1 Superalloy

Custom superalloy parts like Stellite 1 are recommended when components require extreme wear resistance, high thermal stability, and corrosion resistance. It excels in abrasive environments with critical hardness, such as aerospace turbines, oil drilling tools, and chemical reactor valves. However, its machinability challenges and brittleness make it better suited for specific applications where grinding or welding is viable. Stellite 1 also offers excellent performance in applications involving prolonged exposure to high temperatures and thermal fatigue, making it ideal for energy, power generation, and marine sectors.