CMSX-10 is a high-performance single crystal superalloy designed for extreme environments, offering exceptional creep resistance, fatigue strength, and thermal stability above 1100°C.

About CMSX-10

Name and Equivalent Name: CMSX-10 is a single-crystal superalloy widely used in industries that require high mechanical strength and stability under extreme heat. It follows the AMS 5957 standard and complies with ISO 9001 and NACE MR0175. Known for its remarkable performance in gas turbines and jet engines, CMSX-10 outperforms many conventional superalloys, making it a key material in advanced applications.

CMSX-10 Basic Introduction

CMSX-10 is a nickel-based single-crystal superalloy developed to meet the rigorous demands of high-temperature operations. It delivers superior mechanical strength, fatigue resistance, and creep stability, ensuring reliable performance in gas turbines and jet engines.

With a melting point of 1350°C and outstanding creep rupture life exceeding 30,000 hours at 1100°C, CMSX-10 ensures minimal deformation even under cyclic thermal loads. The alloy is ideal for turbine blades, exhaust systems, and rotating components, making it essential for the aerospace and energy sectors.

cmsx-10-superalloy-single-crystal-casting-blades-manufacturer

Alternative Superalloys of CMSX-10

CMSX-10 is often compared to CMSX-4 and CMSX-8, designed for similar high-temperature applications. CMSX-4 offers improved oxidation resistance, making it suitable for environments with high exposure to combustion gases. CMSX-8 provides enhanced fatigue resistance and thermal stability, performing well in demanding power systems.

Other alternatives include Rene N5 and IN738. Rene N5 offers comparable mechanical properties with slight improvements in corrosion resistance. IN738 is a polycrystalline alloy used where single-crystal performance is not required, balancing cost and performance effectively.


CMSX-10 Design Intention

CMSX-10 is designed to withstand extreme thermal and mechanical stress without deformation. Its single-crystal structure eliminates grain boundaries, reducing the risk of creep and fatigue failures. Including rhenium improves its creep resistance, while tungsten and tantalum enhance high-temperature strength.

The alloy is optimized for gas turbines and aerospace engines, where consistent mechanical performance under cyclic thermal loads is essential. Its high fatigue resistance ensures reliability over extended service periods, reducing maintenance and downtime in critical operations.


CMSX-10 Chemical Composition

CMSX-10 contains critical elements that provide outstanding creep resistance, oxidation protection, and mechanical stability at elevated temperatures. Nickel is the matrix, while rhenium and tungsten enhance long-term stability and fatigue strength.

Element

Composition (%)

Nickel (Ni)

Balance

Chromium (Cr)

2

Cobalt (Co)

3

Tungsten (W)

5.5

Molybdenum (Mo)

0.4

Aluminum (Al)

5.7

Tantalum (Ta)

8

Rhenium (Re)

6

Hafnium (Hf)

0.1


CMSX-10 Physical Properties

CMSX-10 offers excellent mechanical and thermal properties. Its high melting point ensures performance under extreme conditions, while its modulus of elasticity and thermal conductivity enhance structural stability and heat management.

Property

Value

Density (g/cm³)

8.76

Melting Point (°C)

1350

Thermal Conductivity (W/(m·K))

10.9

Modulus of Elasticity (GPa)

220


Metallographic Structure of CMSX-10 Superalloy

CMSX-10 features a single crystal microstructure with no grain boundaries, minimizing creep deformation and enhancing fatigue resistance. This structure ensures long-term performance under continuous stress and high temperatures.

The alloy’s gamma-prime (γ') sediments, formed by elements like aluminum and tantalum, are distributed throughout the matrix, resisting dislocation movement and strengthening the material. The absence of grain boundaries ensures the alloy performs reliably in cyclic environments, making it ideal for rotating parts in gas turbines and aerospace engines.


CMSX-10 Mechanical Properties

CMSX-10 offers superior tensile and yield strength, exceptional fatigue resistance and creep stability. These properties make it ideal for demanding aerospace and power generation applications.

Property

Value

Tensile Strength (MPa)

1280

Yield Strength (MPa)

1150

Creep Strength

Excellent at 1100-1150°C

Fatigue Strength (MPa)

700

Hardness (HRC)

45 – 50

Elongation (%)

8 – 10

Creep Rupture Life

> 30,000 hours at 1100°C

Modulus of Elasticity (GPa)

~230


Key Features of CMSX-10 Superalloy

  1. Exceptional Creep Resistance CMSX-10 provides excellent creep resistance at temperatures above 1100°C, ensuring minimal deformation under long-term mechanical stress.

  2. High Fatigue Strength The alloy is designed to withstand cyclic thermal loads, making it suitable for rotating components in aerospace engines and gas turbines.

  3. Long Creep Rupture Life With a creep rupture life exceeding 30,000 hours at 1100°C, CMSX-10 ensures long-term reliability, reducing maintenance in critical applications.

  4. Outstanding Thermal Stability CMSX-10 maintains mechanical strength under continuous exposure to extreme temperatures, ensuring stable performance in demanding environments.

  5. Oxidation and Corrosion Resistance The alloy’s chromium and aluminum content provide excellent oxidation resistance, making it ideal for high-temperature combustion environments.

CMSX-10 Superalloy’s Machinability

CMSX-10 can be used in Vacuum Investment Casting because it can form complex components with high precision and superior surface finish, ensuring excellent mechanical integrity.

Single Crystal Casting is the optimal method for CMSX-10, leveraging its grain-free structure to achieve exceptional creep resistance and fatigue strength at high temperatures.

CMSX-10 is unsuitable for Equiaxed Crystal casting because introducing grains would compromise the alloy’s mechanical performance, making it less effective for high-temperature applications.

Superalloy Directional Casting is unnecessary for CMSX-10 as the alloy already maximizes performance through single crystal casting, eliminating grain boundaries.

CMSX-10 is compatible with Powder Metallurgy Turbine Disc production since it is used for high-performance turbine parts with critical temperature gradients and thermal cycling.

Using CMSX-10 in Superalloy Precision Forging is impractical due to its hardness and inability to be forged without compromising its integrity.

Superalloy 3D Printing is not ideal for CMSX-10 because additive manufacturing methods introduce microstructural defects, reducing fatigue and creep resistance.

CNC Machining is suitable for CMSX-10, though it requires specialized tools and machining strategies to handle its hardness and maintain precision.

Superalloy Welding can be performed on CMSX-10 for localized repairs, but it requires careful heat control to avoid cracking.

Hot Isostatic Pressing (HIP) is essential for CMSX-10 to eliminate internal porosity and enhance mechanical properties, ensuring long-term durability.


CMSX-10 Superalloy Applications

In Aerospace and Aviation, CMSX-10 is used in turbine blades and jet engines, offering exceptional fatigue resistance and reliability under extreme thermal stress.

For Power Generation, CMSX-10 ensures efficient gas turbine operation by withstanding continuous exposure to high temperatures and mechanical loads.

In the Oil and Gas sectors, CMSX-10 supports critical components such as turbines and valves, providing stability in extreme environments.

CMSX-10 plays a crucial role in Energy systems, including high-performance gas turbines, where durability and thermal stability are essential for long-term operation.

In Marine industries, CMSX-10 is used in exhaust systems and propulsion components, offering resistance to high temperatures and corrosive environments.

Mining operations benefit from CMSX-10’s superior strength and wear resistance, ensuring the longevity of essential equipment such as impellers and nozzles.

In Automotive applications, CMSX-10 enhances turbocharger efficiency by maintaining performance under extreme thermal cycling conditions.

Chemical Processing industries use CMSX-10 in high-temperature reactors and valves, providing corrosion resistance and operational stability.

In the Pharmaceutical and Food industries, CMSX-10 is employed in heat-treatment equipment to ensure high durability and performance under thermal cycling.

Military and Defense sectors rely on CMSX-10 for jet engines and missile components, where high mechanical strength and fatigue resistance are critical.

In Nuclear applications, CMSX-10 ensures stability and performance in reactor components, withstanding radiation exposure and high temperatures.


When to Choose CMSX-10 Superalloy

Choose custom superalloy parts made from CMSX-10 for applications that require superior fatigue strength, creep resistance, and thermal stability at extreme temperatures. This alloy is ideal for gas turbines, jet engines, and power generation systems, where performance under continuous thermal cycling and high mechanical stress is critical.

CMSX-10 is also highly suitable for aerospace, oil and gas, and energy applications, offering long-term reliability with reduced maintenance needs. Its ability to perform under cyclic fatigue conditions ensures operational efficiency, making it a top choice for critical components exposed to extreme environments. Use CMSX-10, which has a long service life, high mechanical integrity, and resistance to thermal fatigue, which are essential for success.