العربية

Ti-6Al-6V-2Sn

Explore the exceptional properties of Ti-6Al-6V-2Sn, a titanium superalloy known for high strength, excellent thermal fatigue resistance, and durability in cyclic environments.

About Ti-6Al-6V-2Sn Superalloy

Ti-6Al-6V-2Sn, also known as Titanium Grade 6Al-6V-2Sn, is a high-performance titanium alloy with enhanced strength and fatigue resistance. Its combination of aluminum, vanadium, and tin provides a unique balance of mechanical properties, making it practical for thermal applications up to 500°C. Ti-6Al-6V-2Sn’s compatibility with cyclic loads makes it ideal for aerospace, energy, and chemical industries.

Ti-6Al-6V-2Sn Basic Introduction

Ti-6Al-6V-2Sn is a highly versatile titanium alloy for high-strength applications, offering superior thermal and fatigue performance. With good durability under cyclic loading, this alloy is frequently used in aerospace components such as engine parts and structural frames. Its ability to withstand high temperatures and maintain mechanical integrity makes it suitable for energy and automotive industries.

In addition to its excellent performance in thermal fatigue environments, Ti-6Al-6V-2Sn offers good corrosion resistance, especially in chemically aggressive environments, enhancing its lifespan and usability across various sectors.

ti-6al-6v-2sn-titanium-parts-casting-and-cnc-machining-service

Alternative Superalloys of Ti-6Al-6V-2Sn

Alternative materials to Ti-6Al-6V-2Sn include Ti-6Al-4V, which offers similar strength but with lower thermal resistance, and Ti-10V-2Fe-3Al, which excels in fatigue resistance for cyclic stress applications. Ti-5Al-5V-5Mo-3Cr offers better performance in environments requiring high creep strength. Each alternative alloy has specific properties tailored to meet particular operational demands, such as temperature limits or mechanical stress endurance.


Ti-6Al-6V-2Sn Design Intention

The design of Ti-6Al-6V-2Sn focuses on providing excellent strength at elevated temperatures with good fatigue resistance for cyclic applications. Aluminum contributes to weight reduction and stability, vanadium enhances strength, and tin improves corrosion resistance. These features ensure that the alloy performs reliably in aerospace and power generation industries, where thermal stability and durability are essential.


Ti-6Al-6V-2Sn Chemical Composition

The alloying elements play a critical role in Ti-6Al-6V-2Sn’s performance. Aluminum ensures stability and lightweight properties, while vanadium provides additional strength. Tin contributes to corrosion resistance, making the alloy ideal for chemically harsh environments.

Element

Composition (%)

Aluminum (Al)

5.5 - 6.75

Vanadium (V)

5.5 - 7.5

Tin (Sn)

1.5 - 2.5

Chromium (Cr)

Max 0.25

Iron (Fe)

Max 0.20


Ti-6Al-6V-2Sn Physical Properties

Ti-6Al-6V-2Sn exhibits outstanding thermal conductivity and maintains good mechanical strength at elevated temperatures. These properties make it suitable for aerospace and industrial applications.

Property

Value

Density (g/cm³)

4.64

Melting Point (°C)

1665

Thermal Conductivity (W/(m·K))

7

Modulus of Elasticity (GPa)

115


Metallographic Structure of Ti-6Al-6V-2Sn Superalloy

Ti-6Al-6V-2Sn has a typical alpha-beta microstructure, with alpha-phase particles distributed within a beta-phase matrix. This dual-phase structure enhances both strength and thermal fatigue resistance. The alloy retains its microstructure at temperatures up to 500°C, allowing it to maintain mechanical stability during prolonged exposure to thermal stress.

Ti-6Al-6V-2Sn’s metallographic structure in cyclic loading conditions ensures durability and high fatigue strength. This stability in structure is essential for components used in aircraft engines and power turbines.


Ti-6Al-6V-2Sn Mechanical Properties

Mechanical Property

Value

Tensile Strength (MPa)

1000

Yield Strength (MPa)

850

Hardness (HRC)

35 - 40

Elongation (%)

12 - 18

Elastic Modulus (GPa)

110 - 115


Key Features of Ti-6Al-6V-2Sn Superalloy

  1. High Thermal Fatigue Resistance Ti-6Al-6V-2Sn maintains its mechanical properties at elevated temperatures, making it suitable for applications up to 500°C.

  2. Superior Fatigue Strength The alloy exhibits excellent performance under cyclic loading, ensuring reliability in aerospace and automotive applications.

  3. Corrosion Resistance With its enhanced tin content, Ti-6Al-6V-2Sn offers good corrosion resistance, especially in chemically harsh environments.

  4. Durability in Cyclic Environments Ti-6Al-6V-2Sn is designed for long-term use, performing consistently under repeated stress and thermal cycling.

  5. Lightweight with High Strength The alloy provides a high strength-to-weight ratio, which is critical for aerospace and industrial components, reducing overall system weight without compromising performance.

Ti-6Al-6V-2Sn Superalloy’s Machinability

Vacuum Investment Casting: Ti-6Al-6V-2Sn is not the preferred choice for Vacuum Investment Casting due to challenges in maintaining stability in molten states.

Single Crystal Casting: The alloy is unsuitable for Single Crystal Casting as it lacks the specific composition required for forming single-crystal structures.

Equiaxed Crystal Casting: Ti-6Al-6V-2Sn performs adequately in Equiaxed Crystal Casting processes, ensuring balanced mechanical properties.

Directional Casting: Superalloy Directional Casting is viable for improved structural integrity with this alloy.

Powder Metallurgy Turbine Disc: Ti-6Al-6V-2Sn is not commonly used for Powder Metallurgy Turbine Disc production due to alternative materials offering superior performance.

Precision Forging: This alloy is ideal for Superalloy Precision Forging due to its high strength and fatigue resistance.

Superalloy 3D Printing: Ti-6Al-6V-2Sn is not typically used for Superalloy 3D Printing due to limitations in additive manufacturing compatibility.

CNC Machining: The alloy performs well in CNC Machining processes, offering precision and excellent machinability.

Superalloy Welding: Ti-6Al-6V-2Sn allows Superalloy Welding, ensuring robust and corrosion-resistant joints.

Hot Isostatic Pressing (HIP): The alloy can benefit from Hot Isostatic Pressing (HIP) to improve structural uniformity and reduce porosity.


Ti-6Al-6V-2Sn Superalloy Applications

Aerospace and Aviation: Used for turbine engines and airframes to enhance thermal fatigue resistance. See more at Aerospace and Aviation.

Power Generation: Effective in turbines and heat exchangers. Visit Power Generation.

Oil and Gas: Reliable for pipelines and high-pressure systems. Explore Oil and Gas.

Energy: This alloy is used in renewable energy systems for its durability. Learn more at Energy.

Marine: Ti-6Al-6V-2Sn offers corrosion resistance for marine components. See Marine.

Mining: Used in high-wear components. Learn more at Mining.

Automotive: Applied in engines for lightweight durability. See Automotive.

Chemical Processing: Resistant to chemical corrosion, making it ideal for reactors. Visit Chemical Processing.

Pharmaceutical and Food: Used in equipment that demands high corrosion resistance. See Pharmaceutical and Food.

Military and Defense: Provides strength and lightweight benefits in defense applications. See Military and Defense.

Nuclear: Ti-6Al-6V-2Sn is used in nuclear reactors for its stability. Learn more at Nuclear.


When to Choose Ti-6Al-6V-2Sn Superalloy

Ti-6Al-6V-2Sn should be chosen for applications where high thermal fatigue resistance and strength-to-weight ratios are critical. It is ideal for aerospace components, such as turbine blades and structural airframes, where high durability under cyclic loads is essential.

The alloy provides long-lasting corrosion resistance for marine and energy systems and performs well under thermal stress. In the automotive sector, it reduces component weight without compromising strength. For custom superalloy parts, visit Custom Superalloy Parts.

This alloy’s versatility makes it the go-to choice for sectors demanding high performance in challenging environments.

استكشف المدونات ذات الصلة