SRR 99

SRR 99 is a first-generation single-crystal superalloy known for its high tensile strength, creep resistance, and excellent thermal fatigue performance at 1000°C.

About SRR 99 Superalloy

Name and Equivalent Name

SRR 99 is a first-generation nickel-based single-crystal superalloy. Though not assigned a UNS number, it corresponds to AMS 5866 standards. SRR 99 is similar to first-generation alloys like CMSX-2 and PWA 1480, all developed for high-temperature applications.

SRR 99 Basic Introduction

SRR 99 is a nickel-based single-crystal alloy designed to withstand high temperatures and mechanical stress. It eliminates grain boundaries and minimizes creep deformation under stress, making it ideal for jet engine turbine blades and vanes.

This alloy combines high creep resistance with excellent thermal fatigue performance, ensuring long service life under extreme conditions. SRR 99 is widely used in the aerospace and energy sectors, where maintaining mechanical integrity at elevated temperatures is critical.

srr-99-single-crystal-superalloy-investment-casting-blades-manufacturer

Alternative Superalloys of SRR 99

SRR 99 can be compared with first-generation single-crystal superalloys such as CMSX-2, PWA 1480, and René N4. These alloys offer similar high-temperature strength, fatigue resistance, and creep performance. However, second-generation alloys, including CMSX-4 and René N5, provide improved creep resistance at higher costs. SRR 99 is preferred when balancing mechanical performance with ease of manufacturing is essential.


SRR 99 Design Intention

SRR 99 was developed to meet the stringent demands of jet engines and gas turbines. Its single-crystal structure eliminates grain boundary sliding, enhancing fatigue life and reducing creep deformation at temperatures exceeding 1000°C. The high tungsten and rhenium content further enhance creep resistance, while chromium improves oxidation resistance. SRR 99’s design ensures long operational life under cyclic thermal stress.


SRR 99 Chemical Composition

The elements in SRR 99 contribute to its high-temperature performance. Chromium provides oxidation resistance, tungsten strengthens the matrix, and rhenium enhances creep resistance.

Element

Weight %

Nickel (Ni)

Balance

Chromium (Cr)

8%

Cobalt (Co)

5%

Molybdenum (Mo)

2%

Tungsten (W)

10%

Aluminum (Al)

5.5%

Tantalum (Ta)

3%

Carbon (C)

0.08%


SRR 99 Physical Properties

SRR 99 is known for its stability at high temperatures and ability to resist mechanical and thermal fatigue.

Property

Value

Density

8.74 g/cm³

Melting Point

1360°C

Thermal Conductivity

11 W/(m·K)

Modulus of Elasticity

215 GPa

Tensile Strength

1070 MPa


Metallographic Structure of SRR 99 Superalloy

SRR 99 has a single-crystal microstructure with no grain boundaries, reducing the risk of creep deformation under prolonged stress. The matrix comprises gamma (γ) phases, while gamma-prime (γ') precipitates, primarily consisting of nickel, aluminum, and tantalum, enhance mechanical strength.

The alloy's microstructure ensures stability under cyclic thermal loading. The uniform dispersion of γ' precipitates throughout the matrix provides superior fatigue resistance, making SRR 99 a reliable material for jet engines and gas turbines.


SRR 99 Mechanical Properties

SRR 99 offers excellent tensile strength and high-temperature fatigue resistance, ensuring reliable performance in demanding applications.

Property

Value

Tensile Strength

~1050 MPa

Yield Strength

~900 MPa

Creep Strength

High at 1000°C

Fatigue Strength

~500 MPa

Creep Rupture Life

~15,000 hours at 950°C

Hardness (HRC)

~38-42

Elongation

~12%


Key Features of SRR 99 Superalloy

  1. High Creep Resistance SRR 99 exhibits excellent creep resistance at 1000°C, making it ideal for turbine blades that endure sustained mechanical stress under extreme heat.

  2. Thermal Fatigue Performance SRR 99 performs reliably under thermal cycling conditions, ensuring long service life in jet engines and gas turbines by minimizing fatigue cracking.

  3. Oxidation Resistance The alloy's 8% chromium content enhances oxidation resistance, preventing surface degradation in high-temperature environments.

  4. Mechanical Strength SRR 99 provides high tensile strength (1070 MPa) and yield strength (900 MPa), ensuring durability under mechanical stress in aerospace applications.

  5. Extended Creep Rupture Life With a creep rupture life of 15,000 hours at 950°C, SRR 99 offers reliable performance in critical high-temperature applications requiring prolonged service.

SRR 99 Superalloy’s Machinability

SRR 99 is compatible with Vacuum Investment Casting due to its excellent flow characteristics and ability to produce high-precision parts, such as turbine blades.

It is ideal for Single Crystal Casting, as its single-crystal structure eliminates grain boundaries, improving fatigue resistance and creep performance.

SRR 99 is unsuitable for Equiaxed Crystal casting because it relies on the superior mechanical properties of a single-crystal structure, which equiaxed casting cannot provide.

While SRR 99 can be considered for Superalloy Directional Casting, it performs better in fully single-crystal applications for higher fatigue resistance.

SRR 99 is unsuitable for Powder Metallurgy Turbine Discs as the powder metallurgy process cannot maintain the single-crystal microstructure required for optimal performance.

The alloy is not recommended for Superalloy Precision Forging due to the challenges in shaping single-crystal materials without introducing defects.

Superalloy 3D Printing is impractical for SRR 99, as additive manufacturing processes struggle to achieve single-crystal structures.

SRR 99 can undergo CNC Machining, though its hardness requires specialized cutting tools to achieve precise tolerances without excessive wear.

Superalloy Welding of SRR 99 is generally avoided since welding introduces defects that may compromise the integrity of its single-crystal structure.

Hot Isostatic Pressing (HIP) can eliminate internal porosity and enhance the mechanical properties of SRR 99 components.


SRR 99 Superalloy Applications

In Aerospace and Aviation, SRR 99 is used in jet engine turbine blades and vanes, where high creep resistance and fatigue life are essential.

For Power Generation, SRR 99 is applied in gas turbines, ensuring long service life and stable operation under high thermal loads.

In the Oil and Gas industry, SRR 99 is utilized in components exposed to extreme temperatures, such as high-performance turbine sections.

In the Energy sector, SRR 99 contributes to turbines used in both conventional and renewable power plants, delivering reliable performance under cyclic stress.

The Marine industry benefits from SRR 99's resistance to thermal and mechanical fatigue in propulsion systems and turbines.

In Mining, SRR 99 is used in specialized tools and components for high-temperature operations, such as pumps and wear-resistant parts.

The Automotive industry leverages SRR 99 in high-performance engines, particularly motorsports, where heat resistance is essential.

For Chemical Processing, SRR 99 ensures reliable operation in reactors and heat exchangers exposed to corrosive and high-temperature conditions.

In Pharmaceutical and Food applications, SRR 99 is used for sterilization equipment requiring heat and corrosion resistance.

Military and Defense applications include jet engine components and advanced propulsion systems, leveraging SRR 99's high-temperature performance.

In the Nuclear industry, SRR 99 is applied in reactors and turbines, offering stability and reliability under extreme operating conditions.


When to Choose SRR 99 Superalloy

Choose SRR 99 when your application requires exceptional creep resistance, fatigue performance, and oxidation resistance at elevated temperatures. It is the ideal material for custom superalloy parts in jet engines, gas turbines, and high-temperature manufacturing. Use SRR 99 when long service life and stability under thermal cycling are critical. Aerospace and power generation industries benefit most from this alloy, where mechanical strength and thermal fatigue resistance are vital. If you need components that perform reliably under extreme conditions, SRR 99 provides the durability and performance needed for critical applications.