Rene N5

Rene N5 is a high-performance nickel-chromium superalloy offering exceptional creep resistance, thermal fatigue strength, and long service life for aerospace engines and turbines.

About Rene N5 Superalloy

Name and Equivalent Names

Rene N5 is a nickel-chromium-based superalloy with no direct ASTM or ISO equivalents but is recognized under AMS 5970 standards. Thanks to its creep resistance and fatigue strength, it offers exceptional performance at high temperatures, especially in aerospace engines. The alloy is also listed under NACE MR0175, ensuring corrosion resistance for oil and gas applications.

Rene N5 Basic Introduction

Rene N5 is a single-crystal superalloy designed for high-temperature applications, particularly in aerospace engines and industrial gas turbines. It provides excellent mechanical properties at temperatures above 1000°C, with outstanding resistance to cyclic fatigue.

This alloy’s unique chemical composition, including rhenium (Re) and hafnium (Hf), enhances its thermal stability and fatigue resistance, making it ideal for turbine blades and other high-stress engine components. Rene N5 ensures long service life, even under continuous operation in extreme environments, minimizing maintenance costs and downtime.

rene-n5-superalloy-casting-and-forging-parts-cnc-machining-service-manufacturer

Alternative Superalloys of Rene N5

Alternative materials for Rene N5 include CMSX-4, Inconel 738, and Mar-M-247. CMSX-4 provides similar single-crystal performance but with slightly different mechanical properties. Inconel 738 offers excellent oxidation resistance but may not match Rene N5’s fatigue strength. Mar-M-247 is ideal for equiaxed casting and has good creep resistance, though it is not optimized for single-crystal applications like Rene N5.


Rene N5 Design Intention

Rene N5 was developed to meet the rigorous demands of aerospace engines and industrial turbines, focusing on high thermal resistance, mechanical strength, and fatigue durability. The alloy’s single-crystal structure eliminates grain boundaries, which reduces the risk of creep and fatigue failure at elevated temperatures.

Adding rhenium and hafnium enhances the alloy’s ability to withstand cyclic loading and thermal fatigue, making it suitable for turbine blades that operate under extreme stress. Rene N5 is designed to provide a long service life, reducing the need for frequent replacements in critical systems.


Rene N5 Chemical Composition

The chemical composition of Rene N5 ensures excellent high-temperature strength, thermal resistance, and creep durability. Rhenium and hafnium improve fatigue resistance and structural integrity.

Element

Content (wt%)

Nickel (Ni)

Balance

Chromium (Cr)

7.0

Cobalt (Co)

7.5

Aluminum (Al)

5.8

Titanium (Ti)

6.2

Tungsten (W)

6.0

Rhenium (Re)

3.0

Hafnium (Hf)

0.15


Rene N5 Physical Properties

Rene N5’s physical properties ensure stability and durability in high-stress, high-temperature environments. Its high density and thermal conductivity make it ideal for aerospace engines and gas turbines.

Property

Value

Density (g/cm³)

8.73

Melting Point (°C)

1345

Thermal Conductivity (W/m·K)

10.9

Modulus of Elasticity (GPa)

214


Metallographic Structure of Rene N5 Superalloy

Rene N5 has a single-crystal structure, eliminating grain boundaries and significantly enhancing creep and fatigue resistance at elevated temperatures. The γ-phase matrix and γ' (gamma prime) precipitates prevent dislocation movement, providing high mechanical stability under stress.

The presence of rhenium and hafnium further strengthens the alloy, improving its resistance to thermal fatigue and deformation. This unique metallographic structure ensures reliable performance in turbine blades, where mechanical strength and stability are critical under continuous high-temperature operation.


Rene N5 Mechanical Properties

Rene N5 offers exceptional mechanical properties, making it suitable for high-stress, high-temperature environments. Its fatigue resistance and long service life are key benefits.

Property

Value

Tensile Strength (MPa)

~1280

Yield Strength (MPa)

~1100

Creep Strength

Outstanding at >1000°C

Hardness (HRC)

~45

Elongation (%)

8 – 10

Elastic Modulus (GPa)

~220


Key Features of Rene N5 Superalloy

1. Exceptional Creep Resistance

Rene N5 provides superior creep resistance at temperatures above 1000°C, ensuring stable mechanical performance under continuous operation. This makes it ideal for turbine blades in aerospace engines.

2. High Thermal Fatigue Resistance

The alloy performs exceptionally well under cyclic loading, reducing the risk of fatigue failure. This ensures the reliability of components exposed to extreme temperature fluctuations.

3. Enhanced Structural Integrity

The single-crystal structure eliminates grain boundaries, minimizing the potential for deformation and enhancing the alloy’s resistance to stress and fatigue.

4. Long Service Life

Rene N5 is designed to provide extended service life, reducing maintenance costs and ensuring uninterrupted performance in aerospace and industrial gas turbines.

5. Optimized for High-Temperature Applications

With a melting point of 1345°C and exceptional thermal conductivity, Rene N5 is optimized for use in environments requiring continuous exposure to extreme heat.

Rene N5 Superalloy’s Machinability

Due to its single-crystal nature, Rene N5 is not typically used for Vacuum Investment Casting, which requires specialized casting methods for optimal performance.

Rene N5 is ideally suited for Single Crystal Casting because this method eliminates grain boundaries, maximizing fatigue resistance and thermal stability at high temperatures.

Equiaxed Crystal casting is not recommended for Rene N5 since it undermines the alloy’s designed advantages of single-crystal structure and creep resistance.

Superalloy Directional Casting is a viable option, although single-crystal casting is preferred to ensure optimal fatigue resistance and strength.

Due to its good processability through PM techniques, Rene N5 is generally used in powder metallurgy turbine disc applications, especially with Rene 88 and Rene 95.

The alloy is unsuitable for Superalloy Precision Forging due to its brittle nature at forging temperatures. However, it excels in cast components.

Rene N5 is not widely applied in Superalloy 3D Printing due to difficulties in achieving uniform single-crystal properties using additive manufacturing techniques.

CNC Machining is effective for Rene N5, enabling the creation of high-precision turbine components with excellent dimensional accuracy.

Superalloy Welding on Rene N5 requires specialized techniques due to its high resistance to deformation and potential cracking at grain boundaries.

Rene N5 benefits from Hot Isostatic Pressing (HIP), which enhances the alloy’s density and eliminates internal voids, improving mechanical performance under thermal stress.


Rene N5 Superalloy Applications

In Aerospace and Aviation, Rene N5 is widely used in turbine blades and vanes, offering superior fatigue resistance and high-temperature stability.

In the Power Generation industry, the alloy ensures efficient performance in gas turbines, reducing downtime through extended service life.

In Oil and Gas, Rene N5 provides excellent creep and corrosion resistance, making it suitable for components exposed to harsh conditions.

The energy sector benefits from Rene N5’s reliability, used in turbines for continuous power generation with minimal maintenance.

For marine applications, Rene N5 ensures high durability in engines and propulsion systems subjected to extreme environments.

In Mining, the alloy offers outstanding wear resistance, extending the life of heavy-duty equipment such as drills and pumps.

The Automotive industry utilizes Rene N5 in high-performance engines and turbochargers, where thermal resistance is essential.

In Chemical Processing, the alloy ensures reliability in reactors and heat exchangers, where high-temperature corrosion is a concern.

For Pharmaceutical and Food applications, Rene N5 offers corrosion-resistant components used in production systems.

In Military and Defense, Rene N5 is crucial for jet engine components, ensuring long-term reliability in critical operations.

For Nuclear applications, the alloy offers excellent thermal and mechanical properties, making it ideal for use in reactors and turbine systems.


When to Choose Rene N5 Superalloy

Rene N5 should be selected when extreme thermal and mechanical stability is required, particularly in aerospace engines and gas turbines. Its single-crystal structure ensures resistance to creep and thermal fatigue, making it suitable for custom superalloy parts that operate in temperatures exceeding 1000°C.

The alloy offers excellent reliability under cyclic loading, making it ideal for components that experience frequent temperature changes. It performs well in aerospace, power generation, oil and gas, and military defense, where efficiency, durability, and minimal maintenance are essential. Rene N5 ensures optimal performance and extended service life, reducing operational costs and enhancing system reliability.