High Temperature Alloys Inconel 718 3D Printing Aerospace Engine Fuel Pipe Parts

Table of Contents
Introduction to Inconel 718 Additive Manufacturing for Fuel Pipe Components
Additive Manufacturing Capabilities for Aerospace Fuel Pipes
Process Parameters
Why Inconel 718 for Fuel Pipe Applications
Material and Processing Strategy
Case Study: Inconel 718 3D Printed Fuel Transfer Tube for Aerospace Turbine
Project Background
Manufacturing Workflow
Validation and Inspection
Results and Verification
FAQs

Introduction to Inconel 718 Additive Manufacturing for Fuel Pipe Components

Inconel 718 is a nickel-based superalloy engineered for aerospace-grade strength, corrosion resistance, and long-term performance at high temperatures. With 3D printing, Inconel 718 enables the manufacturing of complex aerospace engine fuel pipes with optimized geometry, reduced weight, and excellent fatigue resistance.

At Neway Aerotech, we specialize in Inconel 718 additive manufacturing using Selective Laser Melting (SLM) to deliver precision aerospace components, including engine fuel pipes and fluid routing systems.

Additive Manufacturing Capabilities for Aerospace Fuel Pipes

Process Parameters

Parameter

Value

Description

Printing Method

Selective Laser Melting (SLM)

Enables fine-resolution and high-density builds

Layer Thickness

30–50 μm

Supports thin-walled pipe features

Wall Thickness

0.8–1.5 mm

Optimal for pressure-bearing aerospace ducts

Surface Roughness (as built)

Ra 8–15 μm

Can be reduced through polishing or internal flow treatment

Post-Processing

HIP, aging, CNC machining

Ensures mechanical integrity and dimensional precision

Why Inconel 718 for Fuel Pipe Applications

Property

Value

Functional Benefit

Operating Temperature

Up to 980°C

Handles thermal loads in turbine environments

Yield Strength @ 700°C

≥ 720 MPa

Maintains form under cyclic stress and internal pressure

Corrosion Resistance

Excellent in oxidizing media

Resists fuel and combustion gas exposure

Fatigue Life

>10⁸ cycles at 650 MPa

Suitable for vibratory turbine mounting locations

Weldability and Ductility

High

Enables design freedom with integrated fittings

Material and Processing Strategy

  • Powder: Gas-atomized Inconel 718, spherical D50 ~35 μm, certified for aerospace use.

  • Build Orientation: Aligned to minimize support in flow regions and avoid internal channel distortion.

  • Post-Treatment:

    • HIP to eliminate internal porosity.

    • Heat treatment per AMS 5663: 980°C solution + 720°C/8h + 620°C/8h aging.

    • CNC machining for connector interfaces, flanges, and thread geometry.

    • Passivation for corrosion durability.

Case Study: Inconel 718 3D Printed Fuel Transfer Tube for Aerospace Turbine

Project Background

A turbine engine integrator required a custom-designed fuel pipe with thin-wall geometry, integrated brackets, and non-linear routing. Traditional fabrication involved multi-piece bending, welding, and joining, which introduced potential failure points and extended lead time.

Manufacturing Workflow

  1. Design: Complex 3D model with 1.2 mm nominal wall and integrated clamps/ports.

  2. Printing: SLM on 400 W system, 40 μm layers, argon atmosphere.

  3. Post Processing:

    • HIP at 1200°C / 100 MPa for 4 hours.

    • Heat-treated and aged.

    • Internal surface smoothed to Ra ≤ 5 μm using abrasive flow machining.

  4. Finishing:

    • Machined AN flanges to ±0.01 mm.

    • Weld-ready sockets ground and chamfered.

    • CMM verified alignment and fitment tolerances.

Validation and Inspection

  • X-ray inspection and ultrasonic testing showed 100% bond integrity.

  • Leak tested to 2× operating pressure (7 bar) with zero failure.

  • Thermal cycle tested 500 cycles between 100°C and 950°C—no dimensional or microstructural degradation observed.

Results and Verification

The printed Inconel 718 fuel pipe eliminated 5 welded joints, reduced weight by 18%, and shortened the supply timeline by over 40%. All mechanical, thermal, and flow test requirements were passed for integration into a certified turbine assembly.

FAQs

  1. What is the minimum wall thickness that can be reliably printed for Inconel fuel pipes?

  2. Can Inconel 718 printed pipes be post-welded or brazed to other metal components?

  3. What surface finishing improves flow and reduces pressure drop in printed fuel lines?

  4. Are HIP and heat treatment necessary for fatigue-critical fuel routing components?

  5. Can pressure, vibration, and thermal cycling tests be performed before shipment?