English

Ti-5Al-5V-5Mo-3Cr (Ti5553)

Ti-5Al-5V-5Mo-3Cr (Ti5553) titanium alloy offers excellent strength, fatigue resistance, and creep resistance at elevated temperatures. Ideal for aerospace and high-performance applications.

About Ti-5Al-5V-5Mo-3Cr (Ti5553) Superalloy

Name and Equivalent Name

Ti-5Al-5V-5Mo-3Cr, known as Titanium Ti5553 Alloy, conforms to UNS R58650, ASTM B348, GB/T 3621: TB6, and AMS 4940 standards. It is widely used in aerospace and industrial applications for its high mechanical strength and fatigue resistance.

Ti-5Al-5V-5Mo-3Cr (Ti5553) Basic Introduction

Ti-5Al-5V-5Mo-3Cr (Ti5553) is a high-performance beta-phase titanium alloy known for its exceptional mechanical properties, high tensile strength, fatigue resistance, and excellent creep resistance at elevated temperatures. It maintains stability and mechanical integrity at temperatures up to 450°C, making it a preferred material for aerospace and high-stress industrial components.

This alloy is used in critical applications such as landing gears, engine components, and fasteners. Ti5553’s unique combination of strength, durability, and lightweight properties ensures long-term reliability under cyclic loading, making it suitable for aerospace structures and advanced engineering designs.

ti-5al-5v-5mo-3cr-ti5553-titanium-parts-casting-and-cnc-machining-service

Alternative Superalloys of Ti-5Al-5V-5Mo-3Cr (Ti5553)

Alternatives to Ti-5Al-5V-5Mo-3Cr (Ti5553) include Ti-6Al-4V (Grade 5), which offers slightly lower strength but improved machinability. Ti-3Al-8V-6Cr-4Mo-4Zr (Beta C) provides excellent corrosion resistance and fatigue performance but with slightly lower tensile strength.

Inconel 718 or Ti-10V-2Fe-3Al are often used for highly high-temperature environments due to their superior heat resistance. However, depending on the application, these alternatives can be heavier or more challenging to process than Ti5553.


Ti-5Al-5V-5Mo-3Cr (Ti5553) Design Intention

Ti5553 was designed to meet the need for a high-strength titanium alloy capable of withstanding cyclic loads and creep at elevated temperatures. The alloy’s formulation ensures it maintains stability and fatigue resistance during long-term use in demanding aerospace and industrial applications.

The design focus of Ti5553 is to balance mechanical performance with weight savings, making it ideal for structural components exposed to high stress. It is especially suitable for aircraft landing gears, where strength and fatigue resistance are paramount.


Ti-5Al-5V-5Mo-3Cr (Ti5553) Chemical Composition

The chemical composition of Ti5553 is carefully formulated to provide high tensile strength, fatigue resistance, and excellent performance under thermal stress.

Element

Content (wt%)

Aluminum (Al)

4.0 – 6.0

Vanadium (V)

4.5 – 5.5

Chromium (Cr)

2.5 – 4.5

Molybdenum (Mo)

4.0 – 5.5

Iron (Fe)

≤ 0.25


Ti-5Al-5V-5Mo-3Cr (Ti5553) Physical Properties

Ti5553 combines lightweight properties with high mechanical strength, making it suitable for aerospace and industrial applications.

Property

Value

Density

4.66 g/cm³

Melting Point

1620°C

Thermal Conductivity

7.2 W/(m·K)

Elastic Modulus

115 GPa


Metallographic Structure of Ti-5Al-5V-5Mo-3Cr (Ti5553) Superalloy

Ti-5Al-5V-5Mo-3Cr (Ti5553) is primarily a beta-phase titanium alloy, providing excellent strength, flexibility, and fatigue resistance. The beta-phase structure enhances its machinability, making it suitable for complex geometries and advanced aerospace components.

Heat treatment can improve the alloy’s mechanical properties by refining the grain structure and enhancing tensile strength and creep resistance. This microstructure ensures consistent performance under cyclic loading, which is crucial for aircraft and high-performance applications.


Ti-5Al-5V-5Mo-3Cr (Ti5553) Mechanical Properties

The alloy’s high mechanical performance ensures reliability in demanding environments, maintaining stability at elevated temperatures and under stress.

Property

Value

Tensile Strength

1200 – 1300 MPa

Yield Strength

1100 – 1200 MPa

Hardness

35 – 40 HRC

Elongation

~10%


Key Features of Ti-5Al-5V-5Mo-3Cr (Ti5553) Superalloy

  1. High Creep Resistance Ti5553 maintains mechanical integrity at temperatures up to 450°C, providing excellent creep resistance for long-term use in aerospace components.

  2. Superior Fatigue Resistance The alloy is designed to perform under cyclic loading, making it ideal for landing gears, engine parts, and other aerospace applications.

  3. Lightweight with High Strength, Ti5553 offers a high strength-to-weight ratio, contributing to improved fuel efficiency and performance in the aerospace and automotive industries.

  4. Thermal Stability The alloy exhibits excellent mechanical properties and stability at elevated temperatures, ensuring reliable performance under thermal stress.

  5. Good Machinability Ti5553’s beta-phase structure enhances its machinability, allowing for precise and efficient fabrication of complex parts required in high-performance applications.

Ti-5Al-5V-5Mo-3Cr (Ti5553) Superalloy’s Machinability

Vacuum Investment Casting: Ti-5Al-5V-5Mo-3Cr (Ti5553) is not typically used for Vacuum Investment Casting due to its high beta-phase content, which limits its castability and increases complexity in achieving precise shapes.

Single Crystal Casting: Single Crystal Casting is unsuitable for Ti5553, as this alloy is not designed for single-crystal microstructures but for high-strength beta-phase applications.

Equiaxed Crystal Casting: Equiaxed Crystal casting can be used with Ti5553, ensuring uniform grain structure, which enhances fatigue resistance and mechanical reliability.

Superalloy Directional Casting: Superalloy Directional Casting is not ideal for Ti5553, as the alloy's strength is better optimized in equiaxed structures rather than directionally solidified forms.

Powder Metallurgy Turbine Disc: Ti5553 is generally applied to Powder Metallurgy Turbine Disc production as an excellent strength-to-weight ratio with moderate high-temperature capability.

Superalloy Precision Forging: Superalloy Precision Forging is a highly effective process for Ti5553, enhancing its strength and fatigue performance, making it ideal for aerospace components.

Superalloy 3D Printing: Superalloy 3D Printing is feasible for Ti5553, though it requires advanced printing technologies to manage residual stress and maintain mechanical properties.

CNC Machining: CNC Machining works well with Ti5553, allowing for precision in fabricating complex aerospace and automotive components.

Superalloy Welding: Superalloy Welding is suitable for Ti5553, but careful control of heat input is required to prevent cracking and maintain structural integrity.

Hot Isostatic Pressing (HIP): Hot Isostatic Pressing (HIP) significantly improves Ti5553’s fatigue performance by eliminating internal defects and optimizing the microstructure.


Ti-5Al-5V-5Mo-3Cr (Ti5553) Superalloy Applications

Aerospace and Aviation: In Aerospace and Aviation, Ti5553 is used for landing gear, fasteners, and structural components, offering high strength and fatigue resistance.

Power Generation: Power Generation applications benefit from Ti5553’s mechanical stability under thermal stress, making it suitable for turbine components and high-pressure systems.

Oil and Gas: In the Oil and Gas industries, Ti5553 is used for valves, pipelines, and offshore structures, providing corrosion resistance and durability.

Energy: In Energy systems, Ti5553 supports components in renewable energy installations like wind turbines, ensuring reliability under cyclic loads.

Marine: The Marine sector employs Ti5553 in propeller shafts and seawater-exposed parts due to its corrosion resistance and fatigue performance.

Mining: Mining applications include wear-resistant drill bits and pump housings, where the alloy’s mechanical strength ensures durability.

Automotive: Automotive industries use Ti5553 for lightweight, high-strength components such as suspension systems and engine parts.

Chemical Processing: In Chemical Processing, Ti5553 is used for reactors and heat exchangers, providing resistance to aggressive chemicals.

Pharmaceutical and Food: The Pharmaceutical and Food sectors benefit from Ti5553’s hygienic properties, using it for valves, mixers, and processing equipment.

Military and Defense: In Military and Defense, Ti5553 is employed in lightweight armor and aerospace components for enhanced durability.

Nuclear: The Nuclear sector uses Ti5553 in radiation-resistant components and reactor parts, ensuring mechanical stability under extreme conditions.


When to Choose Ti-5Al-5V-5Mo-3Cr (Ti5553) Superalloy

Custom superalloy parts made from Ti5553 are ideal for aerospace, marine, and automotive industries where high strength and fatigue resistance are critical. This alloy is most effective in components that experience cyclic loading and require long-term reliability. Ti5553’s thermal stability and resistance to creep make it suitable for high-temperature environments, such as engines and turbines. Its lightweight properties also contribute to fuel efficiency in aerospace and automotive applications. Additionally, Ti5553 provides corrosion resistance, making it an excellent choice for marine and chemical environments. Precision forging and CNC machining allow for the efficient fabrication of complex parts, ensuring optimal performance in demanding conditions.