English

Inconel 625

Inconel 625 is a high-performance superalloy offering excellent corrosion resistance, high tensile strength, and thermal stability, ideal for aerospace, marine, and chemical industries.

About Inconel 625 Superalloy

Material Name and Equivalent Names: Inconel 625 is known by names such as Haynes 625, Nicrofer 6020, Nickelvac 625, Altemp 625, and Chronin 625. It complies with UNS N06625 and aligns with ASTM B443, B446, B704, B705, and B366. International equivalents include DIN/EN 2.4856, BS 3076: NA21, and GB/T 15059: GH625.

Inconel 625 Basic Introduction

Inconel 625 is a nickel-based superalloy known for its outstanding corrosion resistance, high tensile strength, and excellent thermal stability. It performs exceptionally well in extreme environments with high temperatures, pressure, and aggressive chemicals.

This alloy is widely used across aerospace, marine, chemical processing, and power generation industries. Its ability to resist oxidation and corrosion under harsh conditions and high mechanical strength at temperatures up to 982°C makes it a top choice for heat exchangers, exhaust systems, reactor components, and marine equipment.

custom-inconel-625-superalloy-vacuum-investment-castings

Alternative Superalloys of Inconel 625

Alternative materials to Inconel 625 include Inconel 718, Hastelloy C-276, and Incoloy 825. Inconel 718 offers superior mechanical strength but is optimized for cryogenic and slightly lower temperatures. Hastelloy C-276 provides better resistance to pitting and crevice corrosion but lacks the high-temperature strength of Inconel 625. Incoloy 825 is suitable for environments requiring excellent resistance to sulfuric and phosphoric acids but offers lower mechanical strength than Inconel 625.

Each alternative is suited to specific environments, but Inconel 625 is an optimal choice for applications requiring strength and corrosion resistance at elevated temperatures.


Inconel 625 Design Intention

Inconel 625 was designed to provide exceptional strength, corrosion resistance, and thermal stability across a broad temperature range. The alloy’s high nickel content ensures outstanding corrosion resistance, especially in marine and chemical environments. Adding molybdenum and niobium enhances strength and solid-solution hardening without the need for precipitation hardening treatments.

Its high resistance to oxidation and stress-corrosion cracking makes it ideal for demanding applications such as turbine blades, marine exhaust systems, and chemical reactors, where long-term reliability is essential.


Inconel 625 Chemical Composition

Inconel 625’s composition balances elements to enhance corrosion resistance, strength, and thermal stability. Nickel offers excellent oxidation resistance, while chromium ensures stability in oxidizing environments. Molybdenum and niobium further boost strength and resistance to pitting corrosion.

Element

Composition (%)

Nickel (Ni)

58

Chromium (Cr)

20.0 – 23.0

Molybdenum (Mo)

8.0 – 10.0

Iron (Fe)

5

Niobium (Nb)

3.15 – 4.15

Aluminum (Al)

0.4


Inconel 625 Physical Properties

Inconel 625 offers a high melting point and density, with excellent thermal conductivity and stiffness, making it ideal for high-performance applications in extreme environments.

Property

Value

Density (g/cm³)

8.44

Melting Point (°C)

1290

Thermal Conductivity (W/(m·K))

9.8

Modulus of Elasticity (GPa)

206


Metallographic Structure of Inconel 625 Superalloy

Inconel 625 has an austenitic, face-centered cubic (FCC) structure, providing excellent ductility and mechanical strength. This microstructure resists grain boundary precipitation, which helps maintain the alloy’s corrosion resistance and mechanical stability at high temperatures.

The alloy's microstructure remains stable even after prolonged exposure to extreme conditions. Adding niobium enhances solid-solution hardening, while molybdenum contributes to pitting resistance, making Inconel 625 suitable for high-stress environments like marine and chemical processing industries.


Inconel 625 Mechanical Properties

Inconel 625 offers exceptional mechanical properties, enabling it to perform well under high temperatures and extreme stress.

Property

Value

Tensile Strength (MPa)

930 – 1035

Yield Strength (MPa)

517 – 690

Creep Strength

Strong at 982°C

Fatigue Strength (MPa)

380 – 450

Hardness (HRC)

Rockwell C35 – 45

Elongation (%)

30 – 50

Creep Rupture Life

~12,000 hrs at 982°C


Key Features of Inconel 625 Superalloy

1. Outstanding Corrosion Resistance: Inconel 625 is highly corrosion-resistant in various environments, including seawater, chemical acids, and industrial chemicals. This makes it ideal for marine, chemical, and power generation industries.

2. Exceptional High-Temperature Strength: The alloy retains mechanical integrity at temperatures up to 982°C, making it suitable for exhaust systems, gas turbines, and heat exchangers exposed to extreme heat.

3. Excellent Fatigue and Creep Resistance: Inconel 625 offers strong resistance to fatigue and creep, ensuring reliability in high-stress environments over extended periods. It is often used in aerospace and power generation for long-term service applications.

4. Superior Oxidation Resistance: The alloy’s high chromium and nickel content provides excellent resistance to oxidation, even in harsh oxidizing environments. This makes it ideal for high-temperature applications where thermal stability is crucial.

5. Versatile Applications Across Industries: Inconel 625 serves multiple industries, including aerospace, marine, chemical processing, and power generation. Its mechanical and chemical properties combination ensures reliable performance in diverse, challenging environments.

Inconel 625 Superalloy’s Machinability

Inconel 625 is ideal for Vacuum Investment Casting due to its ability to maintain excellent mechanical properties at high temperatures and its oxidation resistance, ensuring high precision for complex parts.

Single Crystal Casting is unsuitable for Inconel 625 since the alloy lacks the microstructural properties required for single-crystal formation, typically used for turbine blades.

Inconel 625 performs well with Equiaxed Crystal Casting. The process provides a uniform grain structure, which enhances the alloy’s fatigue resistance in high-temperature environments.

Superalloy Directional Casting is less commonly used for Inconel 625 because the alloy performs best with equiaxed grains, though it can still offer adequate creep resistance if needed.

Inconel 625 is generally used in Powder Metallurgy Turbine Disc applications due to its excellent oxidation and corrosion resistance, which are critical for turbine environments

The alloy is suitable for Superalloy Precision Forging, where forging enhances strength and durability, making it suitable for aerospace and marine applications.

Superalloy 3D Printing is challenging for Inconel 625 due to its high nickel content, which complicates the printing process but is still used for specific specialized applications.

Inconel 625 is an excellent choice for CNC Machining due to its workability and ability to retain precision under tight tolerances, though advanced tooling is required.

The alloy supports Superalloy Welding and offers excellent weldability without requiring post-weld heat treatment, maintaining joint strength and corrosion resistance.

Hot Isostatic Pressing (HIP) can enhance Inconel 625 by improving density and eliminating internal voids, making it suitable for critical applications requiring high reliability.


Inconel 625 Superalloy Applications

In Aerospace and Aviation, Inconel 625 is used for turbine blades, exhaust systems, and heat exchangers due to its high strength and oxidation resistance at elevated temperatures.

In Power Generation, the alloy uses gas turbines, nuclear reactors, and heat exchangers, where thermal fatigue resistance ensures long-term reliability.

For Oil and Gas, Inconel 625 is essential in downhole equipment, risers, and offshore platforms due to its corrosion resistance in harsh environments.

In the Energy sector, the alloy is utilized in geothermal and nuclear plants, ensuring stability under high temperatures and chemical exposure.

For Marine applications, Inconel 625’s corrosion resistance makes it suitable for exhaust systems, seawater pumps, and heat exchangers in marine environments.

In mining, the alloy is applied to equipment such as slurry pumps and valves, where resistance to wear and corrosion ensures reliability under abrasive conditions.

In the Automotive industry, Inconel 625 is used for high-performance exhaust manifolds and turbocharger components due to its ability to withstand extreme temperatures.

For Chemical Processing, the alloy is used in reactors, piping systems, and heat exchangers, offering excellent resistance to acids and alkalis.

In the Pharmaceutical and Food industries, the alloy’s resistance to corrosion and contamination makes it ideal for sterile equipment such as valves and heat exchangers.

In Military and Defense, Inconel 625 is used in missile systems and jet engines, ensuring reliable performance in extreme conditions.

In the Nuclear sector, the alloy plays a crucial role in reactors and heat exchangers, where high-temperature stability and corrosion resistance are vital.


When to Choose Inconel 625 Superalloy

Inconel 625 is the ideal choice for applications that require exceptional corrosion resistance, high mechanical strength, and thermal stability. It suits industries like Aerospace and Aviation, Marine, and Chemical Processing, where components must withstand extreme environments.

For custom superalloy parts, Inconel 625 offers the versatility and reliability needed for demanding conditions. Whether in gas turbines, exhaust systems, or chemical reactors, this alloy ensures long-lasting performance, reducing maintenance and downtime. Its unique strength and corrosion resistance combination makes it a valuable asset across multiple industries, ensuring operational efficiency and extended service life.