Nimonic 901

Nimonic 901 is a nickel-chromium-iron alloy offering excellent strength, creep resistance, and fatigue stability, ideal for high-temperature aerospace and industrial applications.

About Nimonic 901 Superalloy

Name and Equivalent Name

Nimonic 901, also known as Nickel-Chromium-Iron Alloy 901, is identified by UNS N09901. It meets several global standards, including ASTM B637, DIN/EN 2.4662, and AMS 5660. Its chemical composition and properties make it ideal for components subjected to extreme temperatures and cyclic stress.

Nimonic 901 Basic Introduction

Nimonic 901 is a precipitation-hardenable superalloy that provides excellent strength, fatigue resistance, and stability under high temperatures up to 650°C. Its composition includes nickel, chromium, iron, and titanium, which allow it to withstand thermal cycling and mechanical stress without compromising its performance.

This alloy is extensively used in aerospace, power generation, and industrial sectors, where reliability under continuous load and temperature variations is crucial. Nimonic 901’s ability to resist oxidation and maintain creep strength makes it suitable for turbines, compressors, and heat exchangers.

nimonic-901-superalloy-castings-cnc-machining-factory

Alternative Superalloys of Nimonic 901

Inconel 718 is a similar nickel-based alloy offering comparable creep resistance but with better corrosion resistance. Rene 41 and Waspaloy provide higher temperature capabilities but may be more expensive for certain applications. Hastelloy X is another viable alternative when resistance to oxidation and corrosion is prioritized.

Nimonic 80A and Incoloy 800 are practical alternatives for lower-temperature applications, offering excellent fatigue resistance. The selection depends on operational conditions such as temperature, load, and environmental factors.


Nimonic 901 Design Intention

Nimonic 901 is designed to maintain mechanical strength and fatigue resistance in high-temperature environments. Its iron content provides added cost-effectiveness compared to pure nickel alloys while retaining excellent oxidation resistance. The alloy's molybdenum improves creep resistance, and adding aluminum aids in precipitation hardening.

Nimonic 901 is suitable for applications like turbine discs, shafts, and fasteners, requiring high thermal stability and reliable fatigue performance. This alloy ensures consistent operation under cyclic loads and extended high-temperature exposure, making it ideal for aerospace and industrial uses.


Nimonic 901 Chemical Composition

The chemical composition of Nimonic 901 provides a balance of strength, fatigue resistance, and thermal stability, ensuring performance in demanding environments.

Element

Composition (%)

Nickel (Ni)

40.0 – 45.0

Chromium (Cr)

11.0 – 14.0

Iron (Fe)

Balance

Titanium (Ti)

2.2 – 3.0

Molybdenum (Mo)

5.0 – 6.0

Cobalt (Co)

1.0 max

Aluminum (Al)

0.35 – 0.75


Nimonic 901 Physical Properties

Nimonic 901 offers high thermal conductivity and dimensional stability in high-stress environments.

Property

Value

Density

8.28 g/cm³

Melting Point

1340°C

Thermal Conductivity

13.1 W/(m·K)

Modulus of Elasticity

210 GPa


Metallographic Structure of Nimonic 901 Superalloy

Nimonic 901 features a face-centered cubic (FCC) crystal structure similar to nickel-based superalloys. The presence of aluminum and titanium facilitates precipitation hardening by forming gamma prime (γ') phases, significantly enhancing strength and stability.

This alloy maintains microstructural stability under high thermal and mechanical loads, preventing grain boundary sliding, which contributes to improved creep resistance. The stable structure ensures reliable performance in turbine discs, fasteners, and shafts subjected to cyclic loading.


Nimonic 901 Mechanical Properties

Nimonic 901's mechanical properties ensure long-lasting performance under cyclic stress and high temperatures.

Property

Value

Tensile Strength

930 – 1100 MPa

Yield Strength

690 – 760 MPa

Hardness

Rockwell C35 – 40

Elongation

15 – 20%

Elastic Modulus

~210 GPa

Creep Strength

Good at 650°C

Fatigue Strength

~400 MPa

Creep Rupture Life

Long-lasting at 650°C


Key Features of Nimonic 901 Superalloy

  1. High Creep and Fatigue Resistance Nimonic 901 maintains excellent creep and fatigue resistance at temperatures up to 650°C, making it suitable for turbine and compressor components subjected to continuous stress.

  2. Thermal Stability and Oxidation Resistance The alloy offers good oxidation and thermal degradation resistance, ensuring long-term durability in high-temperature environments like aerospace engines and power generation turbines.

  3. Cost-Effectiveness With its iron content, Nimonic 901 provides a more economical solution than pure nickel-based superalloys without compromising performance.

  4. Microstructural Stability Precipitation hardening through gamma prime phases ensures reliable mechanical properties under thermal cycling, extending the lifespan of critical components.

  5. Versatility in Industrial Applications Nimonic 901 finds applications across multiple industries, including aerospace, oil and gas, and chemical processing, where reliability under stress and heat is paramount.

Nimonic 901 Superalloy’s Machinability

Nimonic 901 is suitable for Vacuum Investment Casting due to its ability to maintain dimensional precision and mechanical strength, making it ideal for producing complex components used in aerospace and power generation industries.

It is not recommended for Single Crystal Casting since its microstructure does not support the formation of single-crystal structures, which are required for advanced jet engine components.

The alloy performs well in Equiaxed Crystal Casting, providing isotropic mechanical properties that enhance fatigue resistance, making it suitable for turbine components operating under cyclic loads.

Nimonic 901 can be applied in Superalloy Directional Casting, enhancing strength by aligning grain boundaries, which is ideal for turbine blades and vanes exposed to high stress.

It is not recommended for Powder Metallurgy Turbine Disc manufacturing since its properties are optimized for casting rather than powder-based processes.

The alloy performs efficiently in Superalloy Precision Forging, providing reliable fatigue strength and stability, particularly in high-temperature applications like turbine shafts and discs.

Nimonic 901 is not typically used in Superalloy 3D Printing due to its complex precipitation-hardened microstructure, which can be challenging to manage during additive manufacturing processes.

The alloy is suitable for CNC Machining, providing excellent machinability and stability, especially when precise dimensions are required for high-performance components.

Superalloy Welding requires specialized techniques for Nimonic 901 to prevent cracking, as its precipitation-hardened structure can make it prone to stress during welding.

Nimonic 901 responds well to Hot Isostatic Pressing (HIP), enhancing material density and eliminating porosity, significantly improving its fatigue life and mechanical integrity.


Nimonic 901 Superalloy Applications

In Aerospace and Aviation, Nimonic 901 is used in turbine discs, compressor blades, and shafts, offering excellent fatigue strength under cyclic loading and high-temperature conditions.

For power generation, the alloy is applied to turbines and heat exchangers, providing the thermal stability and creep resistance required for continuous operation under extreme temperatures.

In the Oil and Gas sector, Nimonic 901 is used in downhole tools and valves, ensuring resistance to stress and corrosion in harsh environments.

Within the Energy industry, Nimonic 901’s creep and fatigue resistance make it suitable for industrial gas turbines and power plant components operating under thermal stress.

The alloy is also ideal for marine applications, such as exhaust systems and propulsion components, which resist high temperatures and seawater corrosion.

In Mining, Nimonic 901 is applied to pump components and drilling equipment, offering wear resistance and reliability in abrasive environments.

The Automotive industry uses Nimonic 901 in turbochargers and exhaust systems, benefiting from its ability to handle high temperatures and mechanical stress.

For Chemical Processing, Nimonic 901 ensures reliable performance in heat exchangers and reactors, where thermal stability and corrosion resistance are essential.

In the Pharmaceutical and Food industries, the alloy is used in specialized valves and process equipment, offering excellent corrosion resistance and heat tolerance.

Military and Defense applications include missile systems and jet engines, where Nimonic 901 provides the strength and stability needed for high-performance operations.

In Nuclear reactors, the alloy is applied to heat exchangers and fasteners, offering superior mechanical stability and corrosion resistance under radiation exposure.


When to Choose Nimonic 901 Superalloy

Nimonic 901 is the optimal choice for custom superalloy parts when high-temperature strength, fatigue resistance, and thermal stability are required. It is particularly suited for use in gas turbines, compressors, and industrial equipment where reliability under cyclic stress is critical.

The alloy is ideal for applications exposed to continuous heat and mechanical stress, such as aerospace engines and power generation turbines. Its ability to maintain mechanical integrity under thermal cycling ensures a long service life, reducing downtime and maintenance costs.

Explore our solutions for custom superalloy parts to find the best fit for your specific industrial needs and ensure optimal performance in challenging environments.