Stellite 20

Stellite 20 is a cobalt-chromium alloy known for high-temperature performance, corrosion resistance, fracture toughness, and long-term reliability in demanding environments.

About Stellite 20

Name and Equivalent Name: Stellite 20, designated as UNS R30020, belongs to the cobalt-chromium alloy family. It conforms to ASTM B426 and B659 and is categorized under AMS 5798 standards. This material, called Cobalt-Chromium Alloy 20, offers a balance of wear resistance and thermal stability, making it ideal for various industrial applications.

Stellite 20 Basic Introduction

Stellite 20 is a high-performance cobalt-chromium superalloy designed for superior performance in high-temperature applications. With moderate carbon content, it provides excellent wear resistance, enhanced by the presence of molybdenum, which improves corrosion resistance in aggressive environments.

This alloy is used in aerospace, energy, and chemical processing industries, where long-term reliability under extreme conditions is essential. Stellite 20 is known for its outstanding fracture toughness, thermal fatigue resistance, and extended service life, making it a preferred material for valve seats, pump components, and cutting tools.

custom-stellite-20-superalloy-components-equiaxed-crystal-casting-foundry

Alternative Superalloys of Stellite 20

While Stellite 20 offers a balance of wear resistance, toughness, and corrosion protection, other alloys can be alternatives for specific applications. Stellite 6 provides better wear resistance but is less effective in high-stress environments. Stellite 12 offers enhanced hardness, making it better for abrasive applications but less suited for fracture-critical applications.

Hastelloy C22 or Inconel 625 might better suit high-temperature environments with significant oxidation resistance requirements. Similarly, Rene 41 and Nimonic 90 are ideal alternatives for aerospace components requiring advanced thermal fatigue resistance.


Stellite 20 Design Intention

Stellite 20 was designed to meet the demands of high-stress and high-temperature environments. Its primary intention is to provide durability under thermal cycling and corrosion exposure. The alloy’s molybdenum content enhances corrosion resistance, while its moderate carbon content ensures good fracture toughness without compromising wear resistance.

This alloy is intended for critical components such as valve seats, cutting tools, and mechanical seals, where performance and reliability are paramount. The design ensures minimal maintenance, extending the lifespan of equipment operating in harsh environments, such as turbines and chemical reactors.


Stellite 20 Chemical Composition

Stellite 20’s composition includes cobalt for toughness and chromium for corrosion resistance. Molybdenum adds further corrosion protection, while carbon provides strength, making it suitable for wear-prone applications.

Element

Composition (%)

Cobalt (Co)

Balance

Chromium (Cr)

25.0-30.0

Molybdenum (Mo)

5.0-6.0

Carbon (C)

Max 0.25

Nickel (Ni)

Max 2.0

Silicon (Si)

Max 1.0

Manganese (Mn)

Max 1.0


Stellite 20 Physical Properties

Stellite 20 combines density, thermal stability, and moderate thermal conductivity, ensuring reliability in high-temperature environments.

Property

Value

Density (g/cm³)

8.76

Melting Point (°C)

1380

Thermal Conductivity (W/(m·K))

11.5

Elastic Modulus (GPa)

200


Metallographic Structure of Stellite 20 Superalloy

Stellite 20 consists of a cobalt matrix with dispersed molybdenum and chromium carbides. These carbides give the alloy superior wear resistance, ensuring durability in abrasive environments.

The alloy’s chromium content promotes the formation of a protective oxide layer, enhancing corrosion resistance. While the low carbon content improves toughness, it also reduces hardness, balancing wear resistance, and fracture toughness for applications where both properties are essential.


Stellite 20 Mechanical Properties

Stellite 20 offers moderate tensile, yield strength, and excellent fracture toughness. It performs well under high temperatures and provides good fatigue resistance.

Property

Value

Tensile Strength (MPa)

800-900

Yield Strength (MPa)

400-500

Creep Strength

Long-term stability at 700°C

Hardness (HRC)

45-50

Elongation (%)

~10%

Modulus of Elasticity (GPa)

205


Key Features of Stellite 20 Superalloy

  1. High-Temperature Performance Stellite 20 maintains mechanical stability and strength at elevated temperatures, making it ideal for components operating in extreme thermal environments such as turbines and heat exchangers.

  2. Excellent Fracture Toughness The alloy offers high fracture toughness, ensuring reliable performance under mechanical stress. This makes it suitable for applications where components are exposed to impact or sudden loads.

  3. Moderate Thermal Fatigue Resistance Stellite 20 performs well under thermal cycling, withstanding repeated heating and cooling cycles. This makes it a preferred material for valves and seals in high-temperature environments.

  4. Corrosion and Wear Resistance With chromium and molybdenum content, Stellite 20 provides excellent resistance to wear and corrosion, ensuring long-term durability in chemical and marine environments.

  5. Long Service Life in Critical Applications The alloy's ability to perform reliably over extended periods under harsh conditions reduces maintenance needs and extends the lifespan of critical components.

Stellite 20 Superalloy’s Machinability and Processing

  • Vacuum Investment Casting: Stellite 20 can be effectively used in vacuum investment casting, producing excellent surface-quality components. The process ensures minimal oxidation and retains the alloy’s corrosion-resistant properties, ideal for aerospace and energy applications.

  • Single Crystal Casting: Stellite 20 is unsuitable for single crystal casting due to its carbides, which prevent uniform grain growth. This limits its use in applications requiring high directional strength, such as advanced turbine blades.

  • Equiaxed Crystal Casting: The alloy works well with equiaxed crystal casting, providing uniform mechanical properties and wear resistance. This makes it an excellent choice for components like valve seats and mechanical seals.

  • Superalloy Directional Casting: Stellite 20 is not recommended for directional casting due to its inability to align grains, which limits its high-temperature fatigue performance in rotating parts.

  • Powder Metallurgy Turbine Disc: Stellite 20 is not ideal for powder metallurgy turbine discs due to limited ductility, which may hinder its performance under high mechanical loads.

  • Superalloy Precision Forging: Due to its hardness, Stellite 20 is not ideal for precision forging, but it performs well in overlays and hard-facing applications to enhance wear resistance.

  • Superalloy 3D Printing: 3D printing of Stellite 20 is challenging due to carbide formation, which may cause cracking. Post-processing techniques can enhance the mechanical properties of printed parts.

  • CNC Machining: CNC machining is feasible with Stellite 20, though specialized tools and techniques are needed due to its hardness. Grinding is commonly employed to achieve precise tolerances.

  • Superalloy Welding: Stellite 20 exhibits excellent weldability, making it suitable for hard-facing applications. Welded components offer high wear resistance, extending service life in harsh environments.

  • Hot Isostatic Pressing (HIP): HIP processing enhances the mechanical integrity of Stellite 20 by eliminating internal porosity, ensuring consistent performance under thermal cycling and mechanical stress.


Stellite 20 Superalloy Applications

  • Aerospace and Aviation: Stellite 20 is used for valve seats, nozzles, and engine components, providing wear resistance and mechanical stability under extreme temperatures and pressures.

  • Power Generation: The alloy is ideal for steam turbines and heat exchangers, where its corrosion resistance and thermal stability ensure efficient long-term operation.

  • Oil and Gas: Stellite 20 is widely employed in valves, drill bits, and pipeline components, where it resists corrosion and abrasion in high-pressure, abrasive environments.

  • Energy: The alloy performs reliably in gas turbines and energy systems, ensuring consistent operation under thermal cycling and mechanical stress.

  • Marine: Stellite 20 is used for pumps and propeller shafts in marine environments, providing wear resistance and protection against saltwater corrosion.

  • Mining: The alloy’s durability makes it suitable for mining tools, crushers, and slurry pumps, delivering extended wear life in abrasive conditions.

  • Automotive: Stellite 20 is applied to exhaust valves and high-performance components, where its thermal fatigue resistance ensures reliability under extreme conditions.

  • Chemical Processing: The alloy is used for pumps, seals, and valves in chemical reactors, ensuring corrosion resistance and long service life in aggressive environments.

  • Pharmaceutical and Food: Stellite 20 ensures non-contaminating surfaces in pharmaceutical and food equipment, providing wear resistance and chemical protection.

  • Military and Defense: The alloy is used for missile components and protective coatings, where wear resistance and high fracture toughness are crucial.

  • Nuclear: Stellite 20 is employed in valves and seals within nuclear reactors, offering stability under high radiation and thermal cycling.


When to Choose Stellite 20 Superalloy

Choosing custom superalloy parts like Stellite 20 is ideal for applications that require a balance of wear resistance, corrosion protection, and thermal stability. It performs exceptionally well in high-stress environments with frequent thermal cycling, such as aerospace engines and chemical reactors.

Stellite 20 is preferred when long service life and minimal maintenance are essential. Although it presents challenges for machining, it is well-suited for CNC applications and welding. The alloy’s fracture toughness and corrosion resistance make it an excellent choice for valves, heat exchangers, and turbine components. Whether used in mining or nuclear applications, Stellite 20 ensures operational reliability in harsh conditions.