English

Ti-13V-11Cr-3Al (TC11) Titanium LENS Laser Melting Deposition (LMD) 3D Printing

Table of Contents
Introduction to TC11 Titanium LMD Additive Manufacturing
Laser Melting Deposition for TC11 Titanium Alloy
LMD Process Capabilities
TC11 Material Performance and Characteristics
Why TC11 is Ideal for LMD Applications
Case Study: LMD Repair of TC11 Aerospace Engine Pylon Component
Project Background
Manufacturing Workflow
Post-processing & Inspection
Results and Verification
FAQs

Introduction to TC11 Titanium LMD Additive Manufacturing

Ti-13V-11Cr-3Al (TC11) is a near-β titanium alloy known for its high strength-to-weight ratio, excellent hardenability, and superior thermal stability. LENS (Laser Engineered Net Shaping), a Laser Melting Deposition (LMD) process, enables the production and repair of large-scale TC11 components with near-net shape efficiency.

At Neway Aerotech, our titanium 3D printing services support advanced LMD manufacturing for TC11 aerospace, energy, and tooling applications requiring structural durability and high-temperature resistance.

Laser Melting Deposition for TC11 Titanium Alloy

LMD Process Capabilities

Parameter

Value

Description

Layer Thickness

300–800 µm

Suitable for high deposition rate, large geometry

Deposition Rate

10–30 cm³/h

Efficient for structural builds and part repair

Laser Power Range

500–2000 W

Adjustable based on wall thickness and feature size

Atmosphere

Inert Argon or Nitrogen

Prevents oxidation during melt pool formation

Powder Particle Size

45–105 µm

Ideal flowability for coaxial powder feed systems

TC11 Material Performance and Characteristics

Property

Value

Application Benefit

Ultimate Tensile Strength

1150–1250 MPa

Load-bearing aerospace and engine brackets

Yield Strength

~1050 MPa

High structural rigidity under static loads

Elongation

10–15%

Maintains ductility for critical aerospace fittings

Operating Temperature

Up to 500°C

Used in airframes and turbine-associated parts

Hardenability

Excellent via β-phase structure

Reliable in thick-section builds

Why TC11 is Ideal for LMD Applications

  • TC11 exhibits outstanding weldability and thermal processing response, making it compatible with LENS/LMD systems for both part manufacturing and component repair.

  • Compared to α+β alloys like Ti-6Al-4V, TC11 offers superior strength and creep resistance at elevated temperatures.

  • The alloy’s stability in LMD avoids common thermal cracking seen in less ductile materials.

Case Study: LMD Repair of TC11 Aerospace Engine Pylon Component

Project Background

An aerospace maintenance customer required structural repair of a forged TC11 engine pylon bracket suffering from fretting fatigue and surface erosion near mounting bosses. The geometry had high curvature and fatigue-sensitive zones that demanded low-distortion processing.

Manufacturing Workflow

  1. Powder Feedstock: TC11 titanium powder, gas-atomized, D50 = 70 μm, flow rate 10 g/min.

  2. System: 1.2 kW LENS system with coaxial powder feed and 4-axis table.

  3. Repair Strategy: Damaged zone scanned, model reconstructed; toolpath generated to rebuild 8 mm thickness.

  4. Deposition: 4 layers at 500 μm each, interpass temperature maintained at 200–250°C.

  5. Heat Treatment: Solution treated at 900°C + aged at 560°C for 6 hours for strength recovery.

Post-processing & Inspection

  • Machining: Surface milled to ±0.02 mm flatness and ±0.05 mm bore alignment.

  • X-ray NDT: No fusion or porosity defects in deposited material.

  • Ultrasonic Testing: Verified integrity of interface and base metal.

  • CMM: All rebuilt dimensions confirmed within ±0.03 mm accuracy.

Results and Verification

The repaired TC11 bracket passed vibration fatigue testing under full engine load simulation for 1 million cycles. Mechanical testing showed ultimate strength of 1220 MPa and hardness uniformity across the deposition zone. The LMD solution restored serviceability and extended part life by over 300%.

FAQs

  1. How does TC11 compare to Ti-6Al-4V in LMD applications?

  2. What are the powder requirements for LMD printing of titanium alloys?

  3. Can TC11 LMD be used for near-net shape manufacturing of full components?

  4. What post-processing is necessary after TC11 laser deposition?

  5. How is distortion controlled during LMD repair on titanium assemblies?