Single crystal turbine blades made from CMSX and other SC superalloys are designed to operate under extreme thermal and mechanical stress in high-pressure turbine stages. These blades require highly controlled heat treatment processes to activate gamma-prime strengthening, stabilize the microstructure, and ensure resistance to creep, fatigue, and oxidation at temperatures exceeding 1100°C.
Neway AeroTech is a certified heat treatment manufacturer for single crystal castings. We specialize in post-casting thermal processing of CMSX-4, CMSX-10, CMSX-2, and other advanced superalloys used in turbine blades for aerospace and power generation sectors.
Single crystal blades depend on gamma-prime precipitation and directional stability to perform reliably under severe high-temperature stress cycles. Heat treatment:
Activates full mechanical potential through solution and aging cycles
Aligns phase distribution with crystallographic direction to reduce creep and distortion
Relieves residual casting stress before CNC machining and HIP processing
Stabilizes geometry for subsequent TBC coating
We ensure no stray grain formation or recrystallization throughout the cycle.
Alloy | Max Service Temp (°C) | Heat Treatment Cycle | Applications |
|---|---|---|---|
CMSX-4 | 1140 | 1290°C/3h + 870°C/20h | HPT blades, vanes |
CMSX-10 | 1170 | 1280°C/4h + 880°C/24h | Rotor blades |
CMSX-2 | 1120 | 1265°C/3h + 870°C/18h | Guide vanes |
We control temperature within ±3°C to avoid grain instability or phase imbalance.
A customer submitted 84 CMSX-4 single crystal airfoils, each 240 mm long with complex internal cooling. Heat treatment was conducted at 1290°C for 3 hours, followed by two-step aging. Post-process SEM and hardness data showed full gamma-prime activation and HAZ-free edges.
Blade Model | Description | Alloy | Industry |
|---|---|---|---|
SCB-820 | Single crystal blade with serpentine passages | CMSX-4 | Aerospace |
RBD-610 | Rotor blade with fir-tree root | CMSX-10 | Energy |
VNS-450 | Vane segment with platform fillets | CMSX-2 | Power Generation |
Each part undergoes controlled thermal cycles, SEM, and CMM verification.
Solution temperature: 1260–1290°C, depending on alloy; removes residual stress and dissolves interdendritic segregation.
Aging cycles: 870–880°C, for 18–24 hours to promote gamma-prime strengthening and phase uniformity.
Ramp rate: ≤5°C/min, limits thermal gradient and prevents recrystallization in thin trailing edges.
Atmosphere: high-purity argon or vacuum, ensures oxidation-free surfaces before TBC.
Validation: CMM, SEM, hardness, and EBSD for grain structure continuity.
Airfoils were solutioned at 1290°C for 3 hours, followed by aging at 870°C for 20 hours. Thermal uniformity held within ±3°C.
Blades were CNC machined to finish profiles. Optional weld repair and HIP processing followed.
X-ray NDT and SEM confirmed phase distribution and grain continuity. CMM validated dimensional compliance within ±0.008 mm.
What is the standard heat treatment for CMSX single crystal blades?
Can heat treatment affect grain orientation in SC airfoils?
How is recrystallization prevented during thermal cycles?
What inspections follow heat treatment of single crystal parts?
Do you offer heat treatment, HIP, and CNC as an integrated service?