English

Superalloy Powder Metallurgy Turbine Disc

Table of Contents
Introduction
Core Technology of Superalloy Powder Metallurgy
Material Characteristics of Powder Metallurgy Superalloys
Case Study: Superalloy Powder Metallurgy Turbine Disc
Project Background
Common Turbine Disc Models and Applications
Selection and Structural Features of Typical Turbine Disc
Turbine Disc Component Manufacturing Solution
Core Manufacturing Challenges
Results and Verification
FAQs

Introduction

Powder metallurgy turbine discs manufactured from superalloys are critical components designed for extreme conditions, delivering exceptional mechanical strength (up to 1500 MPa tensile strength) and resistance to fatigue and creep at operating temperatures up to 750°C. At Neway AeroTech, we specialize in the production of high-precision superalloy turbine discs through advanced powder metallurgy techniques for the aerospace and power generation industries.

Our advanced manufacturing solutions ensure optimized microstructures, superior mechanical properties, and unparalleled reliability in highly demanding applications.

superalloy-powder-metallurgy-turbine-disc

Core Technology of Superalloy Powder Metallurgy

  1. Powder Production: High-quality alloy powders produced via gas atomization, ensuring particle size uniformity (10–100 µm) and controlled chemical purity.

  2. Powder Compaction (HIP): Hot Isostatic Pressing (HIP) consolidates powders under high pressure (100–200 MPa) and temperature (1100–1200°C), eliminating porosity.

  3. Near-Net Shape Forming: Forming discs to near-final geometry reduces machining allowances to 2–5 mm, saving time and material costs significantly.

  4. Controlled Forging: Precision forging at temperatures of 1050–1150°C refines grain structures, enhancing fatigue resistance and mechanical properties of turbine discs.

  5. Heat Treatment: Customized heat treatment cycles (solution treatment at ~1150°C, aging at 760–800°C) optimize mechanical properties and stabilize microstructure.

  6. Precision Machining: Advanced CNC machining achieves final dimensional accuracy within ±0.01 mm, ensuring exceptional component integrity.

Material Characteristics of Powder Metallurgy Superalloys

Property

Specification

Common Alloys

Rene 95, Rene 88, Udimet 720, FGH97, Astroloy

Tensile Strength

1200–1500 MPa

Yield Strength

≥900 MPa

Fatigue Strength

Excellent high-cycle fatigue properties

Creep Resistance

High creep resistance at 700–750°C

Oxidation Resistance

Excellent, suitable for harsh conditions

Operating Temperature

Up to 750°C

Dimensional Accuracy

±0.01 mm

Case Study: Superalloy Powder Metallurgy Turbine Disc

Project Background

A leading aerospace engine manufacturer required high-performance turbine discs capable of operating reliably under temperatures exceeding 700°C with improved fatigue and creep resistance. Powder metallurgy superalloys were selected to achieve these stringent requirements.

Common Turbine Disc Models and Applications

  • High-Pressure Compressor Discs: Essential for aerospace engines, operating reliably at rotational speeds exceeding 15,000 RPM and temperatures around 700°C.

  • Low-Pressure Turbine Discs: Critical for long-life commercial jet engines, maintaining structural integrity for over 30,000 operational cycles at temperatures above 650°C.

  • Gas Turbine Generator Discs: Designed for power plants, these discs sustain high torque and thermal cycling up to 750°C over extended service periods.

  • Marine Propulsion Turbine Discs: Optimized for naval applications, delivering reliable performance in harsh marine environments, operating continuously at elevated temperatures.

Selection and Structural Features of Typical Turbine Disc

Superalloys such as Rene 95 and Udimet 720 were selected for superior creep strength, fatigue resistance, and oxidation resistance. Turbine discs feature optimized bore geometries, uniform grain structures, and minimized stress concentration factors for enhanced durability.

Turbine Disc Component Manufacturing Solution

  1. Powder Atomization: Alloy powders atomized into spherical particles (10–100 µm), ensuring consistent chemical composition and controlled microstructures.

  2. Hot Isostatic Pressing: Consolidation under 150 MPa pressure and 1150°C ensures full density and porosity elimination (<0.1% porosity).

  3. Forging and Shaping: Near-net shape forging at temperatures around 1100°C refines microstructures and achieves precision dimensional accuracy within ±0.5 mm.

  4. Heat Treatment Process: Solution annealing at 1150°C followed by aging at 760°C to achieve high tensile strength (~1450 MPa) and optimal fatigue resistance.

  5. Precision CNC Machining: Final machining ensures dimensional accuracy within ±0.01 mm and superior surface finishes, reducing stress risers significantly.

  6. Thermal Barrier Coating (TBC): Application of Thermal Barrier Coating enhances operational temperature capability and corrosion protection.

  7. Non-Destructive Testing (NDT): Comprehensive ultrasonic and radiographic (X-ray) inspections ensure zero internal defects.

  8. Final Validation Testing: Rigorous mechanical, thermal fatigue, and creep tests confirm turbine disc performance and durability under simulated operating conditions.

Core Manufacturing Challenges

  • Achieving uniform microstructures with minimal grain growth

  • Controlling dimensional tolerances within ±0.01 mm during machining

  • Ensuring complete removal of internal porosity (<0.1%)

  • Maintaining exceptional fatigue and creep resistance at high temperatures

Results and Verification

  1. Dimensional Verification: Coordinate Measuring Machine (CMM) confirmed all critical dimensions within ±0.01 mm tolerance.

  2. Mechanical Property Validation: Achieved tensile strengths up to 1500 MPa and yield strengths above 900 MPa, exceeding project targets.

  3. Fatigue and Creep Testing: Components demonstrated fatigue life extension by 30% and maintained creep integrity over 10,000 hours at 750°C.

  4. NDT Inspections: Passed rigorous ultrasonic and radiographic testing, ensuring defect-free internal structures.

  5. Operational Testing: Successful performance in engine tests verified reliability and extended component lifespan in operational conditions.

  6. Surface Integrity Check: Surface roughness consistently below Ra 1.6 µm significantly improved aerodynamic efficiency and reduced wear potential.

FAQs

  1. What advantages do powder metallurgy superalloy turbine discs offer compared to conventional casting?

  2. What alloys does Neway AeroTech commonly use for turbine discs?

  3. How does Neway AeroTech achieve tight dimensional tolerances in turbine discs?

  4. What non-destructive testing methods are employed for turbine disc quality assurance?

  5. Can Neway AeroTech customize turbine discs for specific operational requirements?