English

Superalloy Investment Castings Precision Electro-Discharge Machining

Table of Contents
Introduction to EDM for Superalloy Investment Castings
EDM Machining Technology Overview
Classification of EDM Machining
EDM Machining Selection Strategy
Material Considerations
Typical Superalloys for EDM After Investment Casting
Materials Selection Strategy
Case Study: EDM Finishing for Investment Cast Turbine Nozzle Ring
Project Background
Manufacturing Work Flow
Post Process
Surface Finishing
Inspection
Results and Verification
FAQs

Introduction to EDM for Superalloy Investment Castings

Electro-Discharge Machining (EDM) is critical for post-processing precision features in superalloy investment castings. It enables tight-tolerance machining without inducing mechanical stress in high-hardness materials or complex geometries that are difficult to conventionally machine.

At Neway Aerotech, our superalloy EDM services complement vacuum investment casting to produce high-performance components for aerospace, energy, and nuclear applications.

EDM Machining Technology Overview

Classification of EDM Machining

EDM Process

Surface Roughness (Ra, μm)

Dimensional Tolerance (mm)

Aspect Ratio

Heat Affected Zone (HAZ, μm)

Min. Feature Size (mm)

Wire EDM

0.3–1.2

±0.002–±0.01

Up to 20:1

2–5 μm

~0.1

Sinker EDM

0.4–2.5

±0.005–±0.02

Up to 10:1

5–10 μm

~0.2

Hole Drilling EDM

0.5–3.0

±0.02–±0.05

Up to 30:1

10–15 μm

~0.1

Micro-EDM

0.1–0.4

±0.001–±0.005

Up to 15:1

<2 μm

<0.05

HAZ varies depending on energy level, pulse duration, and material conductivity.

EDM Machining Selection Strategy

  • Wire EDM: Ideal for trimming parting lines, tight contours, and gate removal on investment castings.

  • Sinker EDM: Best for refining internal cavities, cooling channels, and casting-based electrode seat features.

  • Hole Drilling EDM: Used for cooling or lubrication passages in turbine blades and nozzle rings.

  • Micro-EDM: Enables ultra-fine finishing in cast micro-feature zones or pilot-hole creation for complex assemblies.

Material Considerations

Typical Superalloys for EDM After Investment Casting

Material

Hardness (HRC)

Thermal Fatigue

Casting Suitability

EDM Efficiency

Applications

Inconel 713C

36–42

Excellent

Good

High

Turbine wheels, vanes

Rene 77

38–44

High

Excellent

Moderate

Combustor segments, aerospace brackets

CMSX-4

42–46

Superior

Single-crystal only

Low

Turbine blades, high-temperature airfoils

Hastelloy X

30–35

Good

Very good

High

Exhaust manifolds, chemical processing

Nimonic 115

40–45

Excellent

Moderate

Moderate

Rocket nozzles, valve seats

Materials Selection Strategy

  • Inconel 713C: Best for vanes with tight-profile machining; responds well to wire EDM with minimal recast.

  • Rene 77: Ideal for parts needing high creep strength; EDM recommended for sealing features and bolt holes.

  • CMSX-4: Requires low-energy EDM; used only where grinding is infeasible due to thermal damage risks.

  • Hastelloy X: Easily machined by sinker or wire EDM; good choice for welded cast assemblies.

  • Nimonic 115: Useful for high-cycle tooling; EDM ensures repeatability in fitting and flow-critical areas.

Case Study: EDM Finishing for Investment Cast Turbine Nozzle Ring

Project Background

A client in the power generation sector needed final machining of a Rene 77 turbine nozzle ring cast using vacuum investment technology. Tolerances of ±0.005 mm were required across 22 radial ports and sealing shoulders.

Manufacturing Work Flow

  1. Casting: Investment cast Rene 77, hot isostatically pressed post-casting at 1195°C, 100 MPa, 4 hours.

  2. Rough Machining: CNC-turned interfaces and ring surface, 0.5 mm stock left for EDM finishing.

  3. Wire EDM: Profiled each radial cooling port (Ø1.2 mm) at ±0.003 mm using 0.25 mm brass wire.

  4. Sinker EDM: Machined three internal cavities, spark gap 0.08 mm, depth 10 mm with ±0.005 mm tolerance.

Post Process

Surface Finishing

  • Electro-polished to Ra ≤ 0.6 μm

  • Passivated for corrosion resistance

  • Deburred under microscope to remove <50 μm edge burrs

Inspection

Results and Verification

EDM finishing held consistent profile tolerances of ±0.003 mm across all port entrances and sealing zones on the ring.

HIP post-processing resulted in 100% pore sealing, confirmed by ASTM E192 testing and X-ray level 2 acceptance.

Surface integrity after electro-polishing exceeded Ra ≤ 0.6 μm, eliminating risk of flow-induced erosion or fatigue cracking.

SEM analysis showed uniform spark-textured zones without recast layers or microcracking at grain boundaries.

Final inspection confirmed complete geometric compliance and zero internal defects, exceeding aerospace turbine component acceptance standards.

FAQs

  1. What surface finish can be achieved using EDM on cast superalloy components?

  2. How does EDM affect the metallurgical integrity of investment cast parts?

  3. Can internal cooling channels in turbine castings be processed with EDM?

  4. Is EDM suitable for single crystal or directionally solidified components?

  5. What post-treatment is required after EDM of aerospace castings?