Introduction to Electro-Thermal Material Removal for Inconel 713 Turbine Vanes
EDM Machining Technology Overview
Classification of EDM Machining
EDM Machining Selection Strategy
Material Considerations
Inconel 713 Turbine Vane Properties for EDM
Why Inconel 713 for Turbine Vane Electro-Thermal Machining?
Case Study: EDM Machining of Inconel 713 Turbine Vane Film Cooling Channels
Project Background
Manufacturing Work Flow
Post Process
Surface Finishing
Inspection
Results and Verification
FAQs

Introduction to Electro-Thermal Material Removal for Inconel 713 Turbine Vanes

Electro-thermal material removal, primarily through Electrical Discharge Machining (EDM), is essential for achieving dimensional precision in Inconel 713 turbine vanes. This process enables defect-free feature machining in investment-cast superalloy parts with excellent control over thermal deformation and microstructure integrity.

At Neway Aerotech, we specialize in EDM processing of Inconel 713, especially for turbine vane components requiring fine features, high temperature stability, and strict quality compliance.

EDM Machining Technology Overview

Classification of EDM Machining

EDM Process

Surface Roughness (Ra, μm)

Dimensional Tolerance (mm)

Aspect Ratio

Heat Affected Zone (HAZ, μm)

Min. Feature Size (mm)

Wire EDM

0.3–1.2

±0.002–±0.01

Up to 20:1

2–5 μm

~0.1

Sinker EDM

0.4–2.5

±0.005–±0.02

Up to 10:1

5–10 μm

~0.2

Hole Drilling EDM

0.5–3.0

±0.02–±0.05

Up to 30:1

10–15 μm

~0.1

Micro-EDM

0.1–0.4

±0.001–±0.005

Up to 15:1

<2 μm

<0.05

Electro-thermal discharge removes material locally while avoiding tool wear or surface distortion on thin vane walls.

EDM Machining Selection Strategy

  • Wire EDM: Ideal for trailing edge slotting, airfoil trimming, and vane shroud outline finishing.

  • Sinker EDM: Used for root cavities, internal fillets, and anti-rotation slots in vane castings.

  • Hole Drilling EDM: Applied to cooling passages and film holes, typically 0.6–1.0 mm diameter.

  • Micro-EDM: Suitable for precision features such as micro-serrations or bleed holes under 0.2 mm.

Material Considerations

Inconel 713 Turbine Vane Properties for EDM

Property

Value

Tensile Strength @ 760°C

~1030 MPa

Creep Rupture Life @ 871°C

>100 hours

Hardness (as cast)

HRC 32–38

Thermal Fatigue Resistance

Excellent

Casting Performance

High accuracy in investment casting

Why Inconel 713 for Turbine Vane Electro-Thermal Machining?

  • Maintains structural integrity during spark erosion, minimizing HAZ and recast

  • Offers excellent oxidation resistance during post-EDM heat exposure

  • Compatible with vacuum investment casting and precise EDM-based finishing for mission-critical aerospace vanes

Case Study: EDM Machining of Inconel 713 Turbine Vane Film Cooling Channels

Project Background

A customer in the aerospace sector required fine feature machining on Inconel 713C investment-cast vanes for an industrial gas turbine stage. The part featured 36 cooling holes and two deep sinker cavities per vane.

Manufacturing Work Flow

  1. Casting: Vacuum investment cast with wax pattern precision of ±0.1 mm

  2. Pre-Machining: CNC referencing to set datum for EDM electrode alignment

  3. Hole EDM: 36 cooling holes, 0.8 mm diameter, 15:1 aspect ratio, tolerance ±0.02 mm

  4. Sinker EDM: Slot 8 mm deep formed using graphite electrode, spark gap 0.1 mm

  5. Wire EDM: Final trailing edge and vane tip trimmed with ±0.005 mm accuracy

Post Process

Surface Finishing

  • Internal flow paths polished to Ra ≤ 0.6 μm

  • Passivation applied to vane walls

  • Tip radius refined to R0.05 mm to reduce thermal stress concentration

Inspection

  • CMM on cooling holes and cavity depth with ±2 μm precision

  • X-ray inspection confirmed internal soundness

  • SEM revealed no microcracks, clear discharge lines

  • Ultrasonic immersion testing validated pore-free volume

Results and Verification

Electro-thermal EDM machining delivered consistent feature resolution with ±0.003 mm on all air passage geometry and vane root fittings.

Post-process integrity was validated through SEM and ultrasonic inspection, with no residual cracking or recast present in spark zones.

Surface finish inside film holes was Ra ≤ 0.6 μm, eliminating risk of hot gas turbulence or erosion.

CMM comparison showed full dimensional conformance to CAD model with <2 μm deviation across 3D vane contour.

Turbine vanes completed over 3000 thermal cycles in endurance testing without measurable deformation, erosion, or material loss.

FAQs

  1. How does EDM affect cooling hole shape consistency in Inconel turbine vanes?

  2. What is the optimal spark energy level for Inconel 713 sinker EDM?

  3. Can EDM be applied after TBC coating for post-repair vane geometry correction?

  4. What is the minimum hole diameter achievable by EDM on turbine airfoils?

  5. How do you avoid thermal cracking during electro-discharge removal on thin-walled vanes?