Stellite 20, a cobalt-based superalloy, is renowned for excellent thermal stability up to 950°C and superior resistance to oxidation and erosion in aggressive operating environments. At our specialized workshop, precision Equiaxed Crystal Casting techniques achieve controlled grain structures (0.5–3 mm grain size) and dimensional accuracy within ±0.1 mm, ensuring exceptional performance of turbine blades in power generation applications.
Utilizing advanced casting technologies and rigorous quality protocols, we produce robust Stellite 20 turbine blades designed for extended service life in demanding power plant operations.
Our equiaxed crystal casting technology precisely controls mold preheat temperatures (950–1050°C) and alloy pouring at approximately 1435°C. Controlled solidification rates of 30–100°C/min ensure uniform grain size distribution (0.5–3 mm), optimal isotropic mechanical properties, and minimal internal porosity (<1%), critical for reliable turbine blade operation at elevated temperatures and stress conditions.
Stellite 20 alloy provides exceptional resistance to oxidation, thermal fatigue, and erosion, ideal for power plant turbine blades. Key material properties include:
Property | Value |
|---|---|
Melting Range | 1310–1390°C |
Density | 8.33 g/cm³ |
Tensile Strength (Room Temp.) | 860 MPa |
Yield Strength (Room Temp.) | 680 MPa |
Hardness (HRC) | 52–58 HRC |
Oxidation Resistance | Excellent (up to 950°C) |
Wear Resistance | High (erosion, abrasion resistance) |
These outstanding properties make Stellite 20 ideal for critical turbine components requiring durability and long-term reliability.
A leading power plant operator required robust turbine blades capable of prolonged operation under continuous thermal cycles (~900°C) and highly erosive steam conditions. Utilizing equiaxed crystal casting, our workshop manufactured Stellite 20 turbine blades in full compliance with ASTM F75 and ISO 9001 standards, ensuring exceptional reliability and extended operational life.
Steam Turbine Rotor Blades: Cast Stellite 20 blades providing exceptional oxidation and erosion resistance, optimal for continuous operation in high-pressure steam turbines.
Gas Turbine Compressor Blades: Components engineered to withstand cyclic thermal stress, significantly reducing wear and extending blade life.
Low-Pressure Turbine (LPT) Blades: Highly durable blades offering reliable resistance to corrosive environments and thermal fatigue at intermediate temperatures (500–750°C).
High-Pressure Turbine (HPT) Nozzle Vanes: Precisely cast blades with exceptional erosion resistance, optimized for harsh operating conditions at temperatures around 900°C.
These turbine blade models substantially enhance the efficiency, reliability, and longevity of power generation equipment.
Casting Process Turbine blades are produced using advanced equiaxed crystal casting, controlling solidification rates (approximately 30–100°C/min) and mold preheat (around 1000°C) to achieve uniform grain structures (0.5–3 mm grain size) and dimensional tolerances within ±0.1 mm.
Post-processing Components undergo Hot Isostatic Pressing (HIP) at approximately 1200°C and 100 MPa to eliminate residual porosity (<1%) and enhance fatigue resistance, ensuring consistent mechanical properties throughout the turbine blades.
Surface Treatment Blades receive thermal barrier coatings (TBC), typically composed of yttria-stabilized zirconia applied by plasma spraying, significantly reducing blade surface temperatures (~150–200°C reduction), improving resistance to thermal fatigue and oxidation during extended operations.
Testing and Inspection Comprehensive inspection and testing processes include digital X-ray radiographic inspection, precise dimensional verification via Coordinate Measuring Machine (CMM), and mechanical performance evaluation through tensile testing at elevated temperatures, adhering to stringent industry standards.
Manufacturing Stellite 20 turbine blades involved addressing key challenges:
Ensuring dimensional precision (±0.1 mm) for complex aerodynamic geometries.
Minimizing porosity below 1% through stringent control of casting parameters and solidification conditions.
Achieving uniform grain size distribution (0.5–3 mm) and microstructural consistency for optimal mechanical performance.
Our Stellite 20 turbine blades consistently demonstrated exceptional performance metrics:
Verified dimensional accuracy (±0.1 mm), confirmed through advanced CMM inspection.
Porosity levels consistently maintained below 1%, verified via comprehensive X-ray and ultrasonic examinations.
Mechanical property tests confirming tensile strength ≥860 MPa, yield strength ≥680 MPa, and hardness between 52–58 HRC, meeting and exceeding power industry standards.
Why choose equiaxed crystal casting for manufacturing Stellite 20 turbine blades?
What are the key advantages of Stellite 20 alloy for power plant applications?
Which inspection methods guarantee turbine blade quality and reliability?