Inconel Alloy Equiaxed Crystal Casting Turbine Components Heat Treatment Company

Table of Contents
Optimizing Inconel Turbine Components Through Controlled Heat Treatment
Core Heat Treatment Capabilities for Equiaxed Inconel Castings
Common Inconel Grades and Applications
Case Study: Heat Treatment of Inconel 738 Nozzle Segments
Project Background
Treated Components and Industry Applications
Heat Treatment Challenges for Equiaxed Inconel Turbine Components
Proven Thermal Treatment Solutions
Results and Quality Assurance
Process Execution
Metallurgical Results
Final Inspection
FAQs

Optimizing Inconel Turbine Components Through Controlled Heat Treatment

Inconel alloy turbine components produced via equiaxed crystal casting provide reliable high-temperature performance with isotropic grain structures ideal for complex geometries. However, achieving maximum strength, creep resistance, and microstructural stability requires precisely engineered heat treatment processes tailored to each Inconel grade and part geometry.

Neway AeroTech is a specialized heat treatment company for Inconel alloy turbine components. We offer NADCAP-compliant post-casting thermal processing for blades, vanes, nozzle segments, and combustor hardware to meet aerospace and energy industry specifications.

inconel-alloy-equiaxed-crystal-casting-turbine-components-heat-treatment-company

Core Heat Treatment Capabilities for Equiaxed Inconel Castings

Neway AeroTech uses precise temperature control, gas atmosphere monitoring, and multi-stage thermal cycles to enhance microstructure and mechanical properties.

  • Solution annealing to dissolve segregated phases and homogenize grain boundaries

  • Aging treatment for controlled gamma prime precipitation and hardness development

  • Stress relief to minimize distortion before CNC machining

  • Custom ramp rates to prevent incipient melting and grain coarsening

Processes are tailored to each alloy and validated through metallographic and mechanical testing.

Common Inconel Grades and Applications

Alloy

Max Temp (°C)

Yield Strength (MPa)

Heat Treatment Purpose

Inconel 738

1050

880

Aging to increase creep resistance

Inconel 713C

950

760

Solution treatment to reduce segregation

Inconel 617

1000

640

Stress relief prior to welding or CNC

Inconel 625

980

827

Low-temp aging for structural strengthening

Alloys are selected for their castability, oxidation resistance, and heat treatment responsiveness.

Case Study: Heat Treatment of Inconel 738 Nozzle Segments

Project Background

A power generation OEM supplied Inconel 738 nozzle castings with moderate porosity and surface dendritic structures. A controlled two-stage heat treatment was applied—solution annealing at 1160°C followed by aging at 845°C for 16 hours. Final microstructure exhibited >60% gamma prime phase with no interdendritic segregation.

Treated Components and Industry Applications

Component

Alloy

Treatment Method

Industry

Nozzle Segment

Inconel 738

Solution + Aging

Power Generation

Turbine Blade

Inconel 713C

Stress Relief + Aging

Aerospace

Combustor Shield

Inconel 625

Stress Relief

Energy

Transition Vane

Inconel 617

Annealing + Machining

Industrial Gas Turbines

Each part undergoes process verification through hardness testing, grain structure inspection, and dimensional validation.

Heat Treatment Challenges for Equiaxed Inconel Turbine Components

  1. Gamma prime precipitation control for target hardness and fatigue life

  2. Minimizing distortion during solution annealing in thin-wall geometries

  3. Avoiding incipient melting near the liquidus during high-temp holding

  4. Controlling carbide morphology to prevent grain boundary weakening

  5. Ensuring uniform grain size across shroud, platform, and blade regions

Proven Thermal Treatment Solutions

  • Solution heat treatment at 1120–1180°C with ±2°C precision control

  • Aging at 845°C for 8–24 hours depending on component cross-section

  • Vacuum or argon inert atmosphere to eliminate surface oxidation

  • HIP prior to heat treatment to remove porosity and improve phase response

  • Water or air quenching depending on alloy sensitivity

Results and Quality Assurance

Process Execution

Each component received custom thermal profiles based on alloy, geometry, and mechanical specification. Atmosphere control ensured oxidation-free surfaces, and programmable furnaces delivered consistent cycle accuracy.

Metallurgical Results

Post-treatment hardness for Inconel 738 ranged 350–390 HV. SEM confirmed uniform gamma prime precipitation; grain size remained within ASTM 5–7. No carbide agglomeration or residual microsegregation observed.

Final Inspection

CMM inspection verified dimensional stability post-treatment. X-ray ensured no deformation or cracking. SEM analysis validated grain structure and precipitate morphology.

FAQs

  1. What is the standard aging cycle for Inconel 738 cast parts?

  2. Can equiaxed Inconel 713C be treated without warping thin vane sections?

  3. How is heat treatment controlled to prevent incipient melting?

  4. Do you offer HIP + heat treatment packages for turbine parts?

  5. How is phase distribution verified after thermal processing?