English

IN713LC Superalloy Equiaxed Crystal Casting Gas Turbine Parts

Table of Contents
Introduction
Core Technology of IN713LC Equiaxed Crystal Casting
IN713LC Material Properties for Gas Turbine Parts
Case Study: IN713LC Turbine Components for Power Generation
Project Background
Typical Gas Turbine Parts
Manufacturing Process for Equiaxed IN713LC Turbine Parts
Core Challenges in Equiaxed-Cast Turbine Parts
Results and Verification
FAQs

Introduction

Gas turbine components must withstand continuous exposure to high-temperature combustion gases, mechanical stress, and oxidation. To meet these challenges, IN713LC—an age-hardened nickel-based superalloy—is widely used for gas turbine parts such as blades, vanes, shrouds, and nozzle segments. Manufactured using equiaxed crystal casting, IN713LC parts offer uniform mechanical properties, stable microstructure, and reliable long-term performance.

Neway AeroTech offers vacuum investment casting of IN713LC gas turbine parts using equiaxed solidification under AS9100-certified processes. Our castings support aerospace, power generation, marine, and defense turbine applications.

in713lc-superalloy-equiaxed-crystal-casting-gas-turbine-parts

Core Technology of IN713LC Equiaxed Crystal Casting

  1. Wax Pattern Production High-precision wax patterns replicate complex geometries within ±0.05 mm tolerance, suitable for turbine blades, vanes, and segments.

  2. Ceramic Shell Construction Multi-layer ceramic shells are formed (6–8 mm thick) using refractory slurry and stucco, with excellent thermal shock resistance.

  3. Dewaxing and Shell Firing Shells are dewaxed via autoclave at 150°C and sintered at ~1050°C to provide strength during molten metal pouring.

  4. Vacuum Induction Melting IN713LC alloy is melted in vacuum at ~1450°C (≤10⁻³ Pa), minimizing oxides and ensuring uniform chemical composition.

  5. Equiaxed Solidification Molten alloy fills preheated molds and cools under controlled conditions, producing equiaxed grains with sizes between 0.5–2 mm.

  6. Shell Knockout and Surface Cleaning Shell removal is performed using vibration and high-pressure blasting without damaging precision-cast features.

  7. Heat Treatment Solution treatment and aging are applied to refine γ′ phase distribution and enhance creep resistance.

  8. Final Machining and Inspection CNC machining and EDM achieve dimensional precision; CMM and X-ray ensure conformance.

IN713LC Material Properties for Gas Turbine Parts

  • Operating Temperature: Up to 982°C (1800°F)

  • Tensile Strength: ≥1034 MPa

  • Yield Strength: ≥862 MPa

  • Creep Rupture Strength: ≥200 MPa at 760°C for 1000 hours

  • Oxidation Resistance: Excellent under cyclic hot gas environments

  • Grain Size (ASTM): 5–7, uniform across thick and thin sections

Case Study: IN713LC Turbine Components for Power Generation

Project Background

A global power turbine OEM commissioned Neway AeroTech to manufacture IN713LC equiaxed-cast blades, vanes, and shrouds for a 70 MW gas turbine operating continuously at 950°C. The customer required minimal distortion, high creep resistance, and dimensional stability across all hot-section parts.

Typical Gas Turbine Parts

  • Turbine Blades are subjected to high centrifugal and thermal stresses, requiring a fine equiaxed microstructure and oxidation resistance.

  • Nozzle Guide Vanes Direct combustion gases through turbine stages; demand tight geometric control and thermal fatigue resistance.

  • First-Stage Shrouds Seal rotating blade tips and endure extreme thermal cycles and gas erosion.

  • Combustion Ring Segments: Static arc components exposed to radiant heat and fluctuating temperatures.

Manufacturing Process for Equiaxed IN713LC Turbine Parts

  1. Gating and Mold Design Casting systems are optimized through CFD analysis to promote directional flow and eliminate hot spots.

  2. Vacuum Investment Casting Execution IN713LC alloy is poured into molds under vacuum, solidified under equiaxed conditions, and cooled to minimize residual stress.

  3. Heat Treatment Heat treatment cycles stabilize microstructure and increase creep life through uniform γ′ phase precipitation.

  4. Post-Casting Finishing Machining of attachment faces, holes, and cooling features is completed via CNC and EDM to meet tight tolerances.

  5. Inspection and NDT All parts are verified using X-ray inspection, ultrasonic testing, and CMM measurement for dimensional accuracy and structural soundness.

Core Challenges in Equiaxed-Cast Turbine Parts

  • Avoiding micro-segregation in thick-wall parts

  • Achieving consistent grain size in variable section geometries

  • Maintaining dimensional stability after heat treatment

  • Preventing oxidation and cracking during thermal cycling

Results and Verification

  • Grain size ASTM 6–7 achieved across all blade and vane sections

  • Tensile properties exceeded 1034 MPa with consistent batch-to-batch quality

  • 100% defect-free status confirmed by X-ray and ultrasonic inspection

  • Dimensional deviation within ±0.03 mm achieved post-machining

FAQs

  1. What advantages does equiaxed casting offer for gas turbine components?

  2. How does IN713LC compare to other turbine-grade superalloys?

  3. What inspection methods are used to verify casting integrity?

  4. Can IN713LC equiaxed parts be used in marine turbines?

  5. What tolerances are achievable with CNC and EDM finishing?