CMSX Alloy Single Crystal Castings Heat Treatment Workshop

Table of Contents
Precision Thermal Processing for CMSX Series Turbine Blades and Vanes
Core Heat Treatment Services for CMSX Superalloys
Common CMSX Grades and Blade Applications
Case Study: Heat Treatment of CMSX-10 Airfoil Set
Project Background
Treated CMSX Components and Industries
CMSX Heat Treatment Challenges
Technical Solutions from the CMSX Heat Treatment Workshop
Results and Validation
Heat Treatment Execution
Metallurgical Outcomes
Final Inspection
FAQs

Precision Thermal Processing for CMSX Series Turbine Blades and Vanes

Single crystal superalloys from the CMSX series—such as CMSX-4 and CMSX-10—are the foundation of modern high-performance gas turbine components. These alloys offer superior creep resistance, thermal fatigue strength, and oxidation protection. However, their mechanical properties depend heavily on precise heat treatment after single crystal vacuum investment casting to control γ′ precipitation, remove residual stress, and prevent recrystallization.

Neway AeroTech operates a dedicated heat treatment workshop for CMSX alloy turbine components, providing OEM-grade stabilization, aging, and post-HIP thermal processing. Our workshop supports aerospace, power generation, and industrial turbine customers with NADCAP-compliant thermal cycles customized for blade, vane, and segment geometries.

cmsx-alloy-single-crystal-castings-heat-treatment-workshop

Core Heat Treatment Services for CMSX Superalloys

Single crystal heat treatment requires low ramp rates, inert atmospheres, and microstructure-driven aging profiles.

  • Stabilization at 1140–1175°C for stress relief and solidification stabilization

  • Two-stage aging at 870°C and 760°C to optimize γ′ morphology and mechanical strength

  • Vacuum or high-purity argon furnaces to prevent oxidation and preserve surface finish

  • Slow ramp rates (≤2°C/min) to avoid stray grain nucleation or recrystallization

Each CMSX treatment is traceable with full temperature and time profile documentation.

Common CMSX Grades and Blade Applications

Alloy

Max Service Temp (°C)

Yield Strength (MPa)

Application

CMSX-4

1140

980

First-stage turbine blades

CMSX-10

1160

1040

High-pressure turbine vanes

CMSX-6

1100

900

Turbine shrouds and cooling segments

CMSX-2

1120

910

Nozzle guide vanes, rotor airfoils

CMSX alloys are engineered for long-term exposure to thermal and mechanical stress in high-pressure turbine sections.

Case Study: Heat Treatment of CMSX-10 Airfoil Set

Project Background

An aerospace OEM required stabilization and aging for CMSX-10 turbine blades with 3D cooling channels. The blades underwent stabilization at 1165°C for 4.5 hours followed by aging at 870°C and 760°C. SEM evaluation confirmed complete γ′ precipitation, no recrystallization, and carbide distribution consistent with OEM microstructure specs.

Treated CMSX Components and Industries

Component

Alloy

Process

Industry

HPT Blade

CMSX-4

Stabilization + Dual Aging

Aerospace

Shroud Segment

CMSX-6

Anneal + Aging

Power Generation

Rotor Airfoil

CMSX-2

HIP + Aging

Energy

Vane Cluster

CMSX-10

Stress Relief + Aging

Industrial Gas Turbines

All components undergo metallographic validation, hardness testing, and profile inspection post-processing.

CMSX Heat Treatment Challenges

  1. Recrystallization risk if ramp rates or quench rates are not controlled

  2. Incomplete γ′ formation reduces creep resistance and strength

  3. Surface oxidation in uncontrolled furnace environments degrades component life

  4. Distortion of platform and trailing edge due to temperature gradients

  5. Stray grain formation compromises single crystal integrity and orientation

Technical Solutions from the CMSX Heat Treatment Workshop

  • Multi-zone furnace control ±2°C for thermal uniformity across blade batch

  • Vacuum annealing with <10⁻⁵ torr for oxidation-free results

  • Timed dual aging for optimized γ′ size (300–500 nm target)

  • Orientation-protected fixtures to avoid platform movement during heat cycles

  • CMM and SEM for final inspection

Results and Validation

Heat Treatment Execution

Furnaces maintained uniformity within ±2°C. All blades were tracked individually with batch ID, thermal curves, and real-time logging. Total thermal cycle time: 23 hours.

Metallurgical Outcomes

Final microstructure showed homogeneous γ′ distribution across platform and airfoil. No recrystallization detected. Hardness achieved 400–430 HV with minimal variance across batches.

Final Inspection

CMM inspection confirmed no deformation beyond ±0.02 mm. X-ray inspection showed structural integrity. SEM analysis validated phase morphology and grain boundaries.

FAQs

  1. What is the aging cycle used for CMSX-4 turbine blades?

  2. Can CMSX-10 blades be processed without recrystallization risk?

  3. How is γ′ precipitate size controlled during aging?

  4. What inspection methods confirm SX integrity post heat treatment?

  5. Do you offer HIP and heat treatment integration for CMSX castings?