HIP is highly effective for alloy systems that contain casting-related porosity or require improved fatigue performance and density. It is most widely applied to nickel-based and cobalt-based superalloys, especially those used in turbine blades, combustor liners, and high-temperature structural components. Alloys such as Inconel 939, Stellite 31, and single-crystal materials like PWA 1480 are particularly compatible because they benefit from porosity elimination without phase degradation under HIP conditions.
However, HIP is not universally applicable to all alloys. Materials with high vapor pressure elements, hydrogen-sensitive structures, or specific phase-transformation risks may require temperature adjustments—or may not be suitable for HIP at all.
The following alloy categories commonly benefit from HIP:
Nickel-based superalloys – e.g., Rene 88, Inconel 718.
Cobalt-based alloys – such as wear-resistant grades produced via equiaxed crystal casting.
Titanium alloys – frequently used in aerospace components and 3D-printed near-net shapes.
Powder metallurgy-based parts – including turbine disks manufactured via FGH96 technology.
High-performance stainless steels – particularly martensitic grades and precipitation-hardening steels used in critical machinery.
Alloy compositions containing volatile elements, such as zinc or magnesium, may not withstand HIP temperatures. Some steel grades may require modified HIP conditions to prevent grain growth or embrittlement. Metallurgical compatibility must be evaluated before applying full-scale HIP, making pre-process material testing and analysis essential.
In additive manufacturing and complex castings, combining HIP with optimized heat treatment sequences ensures controlled precipitation and prevents phase degradation after densification.