Thermoplastics to Photopolymers: Unlock Your Designs with Plastic 3D Printing

Table of Contents
Introduction to Material-Driven Plastic 3D Printing
Plastic 3D Printing Technology Overview
Overview of Thermoplastics vs. Photopolymers
Selection Strategy by Material Type
Material Capabilities for Advanced Applications
Thermoplastics and Resins: Performance at a Glance
Material Selection Strategy
Case Study: SLA and SLS Printed Components for Medical Device Prototyping
Project Background
Manufacturing Work Flow
Post Process
Results and Verification
FAQs

Introduction to Material-Driven Plastic 3D Printing

Plastic 3D printing supports a full spectrum of materials—from flexible thermoplastics to rigid photopolymers—offering unmatched design freedom and functionality. Engineers can now tailor material properties to specific mechanical, thermal, or visual needs in a single manufacturing workflow.

At Neway Aerotech, our plastic 3D printing services include SLA, SLS, MJF, and FDM technologies with broad material compatibility for prototypes, tooling, and end-use parts.

Plastic 3D Printing Technology Overview

Overview of Thermoplastics vs. Photopolymers

Technology

Material Type

Resolution (μm)

Tolerance (mm)

Key Characteristics

Common Use Cases

FDM

Thermoplastic

100–300

±0.2–0.4

Tough, low cost, structural-grade

Functional jigs, brackets, housings

SLS

Thermoplastic

80–120

±0.1–0.25

Durable, no supports, flexible options

Mechanical prototypes, load-bearing parts

MJF

Thermoplastic

70–100

±0.1–0.2

Batch-scalable, consistent strength

End-use parts, enclosures, connectors

SLA

Photopolymer

25–100

±0.05–0.15

Smooth surface, high resolution

Fit-checks, visual models, dental, medical

Note: Photopolymers cure with light; thermoplastics fuse under heat. Selection depends on performance and visual priorities.

Selection Strategy by Material Type

  • Thermoplastics: Use for durability, heat resistance, and mechanical performance in functional or structural components.

  • Photopolymers: Select when ultra-smooth surface, detail resolution, or transparency are critical in early-stage prototyping.

Material Capabilities for Advanced Applications

Thermoplastics and Resins: Performance at a Glance

Material

Type

Strength (MPa)

HDT (°C)

Key Benefit

Applications

PLA

Thermoplastic

~60

~55

Fast, easy prototyping

Design mockups, visual prototypes

ABS

Thermoplastic

~45

~96

Impact and chemical resistant

Housings, automotive components

Nylon PA12

Thermoplastic

~50

~180

Abrasion resistant, semi-flexible

Snap fits, wearable components

TPU

Thermoplastic

~30

~60

Flexible, tear-resistant

Gaskets, sleeves, soft contact elements

SLA Tough Resin

Photopolymer

~55

~50

High accuracy, stiff and resilient

Fixtures, consumer-grade housing prototypes

SLA Clear Resin

Photopolymer

~50

~45

Transparent, polishable

Light pipes, fluid models, optics testing

Material Selection Strategy

  • PLA: Ideal for quick, cost-effective iteration and early stage physical model validation.

  • ABS: Used for structural applications needing higher temperature and chemical durability.

  • Nylon PA12: Preferred for mechanically stressed components and industrial prototype systems.

  • TPU: Applied where shock absorption or movement compatibility is required.

  • Tough Resin: For applications needing precision with better impact resistance than general-purpose resins.

  • Clear Resin: Chosen for transparency and polishability, especially in optical or fluidic studies.

Case Study: SLA and SLS Printed Components for Medical Device Prototyping

Project Background

A medical technology startup required functional and cosmetic parts to demonstrate an inhaler device prototype for investor review and early usability testing.

Manufacturing Work Flow

  1. Material Selection: SLA Tough Resin for transparent caps and detail housing; SLS Nylon PA12 for internal brackets.

  2. Design Optimization: Snap-fit geometry designed with ±0.1 mm tolerances and uniform wall thickness for strength.

  3. Printing Process: SLA used 50 μm layer thickness; SLS built in nested batches for reduced cost.

  4. Post Processing: SLA parts UV-cured, polished to <4 μm Ra; SLS parts bead-blasted and assembled dry.

  5. Validation: Functional airflow tested through assembled device; all components passed fit and assembly trials.

Post Process

  • Surface Finish: SLA parts polished manually for optical clarity; SLS parts sealed for handling comfort.

  • Dimensional Control: Verified via 3D scan inspection; variation < ±0.08 mm across 15 units.

  • Assembly: Snap-fit retained its shape after 100+ insertion cycles with no loss in force retention.

Results and Verification

Final assembled devices showcased full functional and cosmetic intent, receiving positive client feedback with zero iteration needed.

Dimensional tolerances and mechanical engagement were within ±0.1 mm, meeting preclinical testing and packaging requirements.

Part production and post-processing were completed in 5 business days, reducing the timeline by over 60% compared to traditional CNC.

SLA clarity eliminated the need for transparent molded covers, saving tooling costs and speeding visual feedback.

FAQs

  1. What’s the difference between SLA resin and thermoplastic 3D printing materials?

  2. Can I use clear or medical-grade materials for plastic 3D printed parts?

  3. How do SLA and SLS compare in accuracy and durability?

  4. Are functional snap-fit components possible using plastic 3D printing?

  5. How fast can I receive prototype parts made from specialty resins or nylons?