English

CMSX Alloy Single Crystal Castings Hot Isostatic Pressing Supplier

Table of Contents
HIP Processing for High-Performance CMSX Single Crystal Turbine Components
Why HIP is Essential for CMSX Single Crystal Castings
CMSX Superalloys Processed via HIP
Case Study: CMSX-4 Blade HIP for Airfoil Integrity
Project Background
Typical CMSX Components and Industries
Advantages of HIP for CMSX Single Crystal Castings
HIP Processing Parameters and Standards
Results and Verification
HIP Execution
Post-HIP Processing
Inspection
FAQs

HIP Processing for High-Performance CMSX Single Crystal Turbine Components

CMSX single crystal superalloys are engineered for high-temperature turbine blade and vane applications, offering exceptional resistance to creep, oxidation, and thermal fatigue. However, even precision single crystal castings can retain sub-surface porosity and localized shrinkage defects. Hot Isostatic Pressing (HIP) is critical to densify CMSX components while preserving directional grain orientation.

Neway AeroTech is a certified HIP supplier for single crystal turbine parts made from CMSX-4 alloy, CMSX-10 alloy, and CMSX-2 alloy. Our HIP process removes casting defects while maintaining crystallographic alignment and mechanical properties for OEM-qualified turbine components.

cmsx-alloy-single-crystal-castings-hot-isostatic-pressing-supplier

Why HIP is Essential for CMSX Single Crystal Castings

Single crystal blades must be structurally flawless to function under extreme turbine conditions. HIP treatment:

  • Eliminates internal microporosity from directional solidification in root, shroud, and airfoil sections

  • Maintains single grain integrity, critical for creep resistance

  • Improves mechanical uniformity before 5-axis CNC machining and thermal barrier coating

  • Supports weld repair readiness, minimizing recrystallization risk

All HIP parameters are tailored to avoid stray grain formation.

CMSX Superalloys Processed via HIP

Alloy

Max Service Temp (°C)

HIP Temp (°C)

Applications

CMSX-4

1140

1260

1st-stage blades, vanes

CMSX-10

1170

1280

Turbine rotors, airfoils

CMSX-2

1120

1245

Transition blades, cooling segments

Alloys are HIPed using OEM and AMS 2774-compliant protocols.

Case Study: CMSX-4 Blade HIP for Airfoil Integrity

Project Background

A customer submitted 72 CMSX-4 single crystal turbine blades with 25 mm thick airfoils and radial cooling channels. HIP was performed at 1260°C, 140 MPa for 4 hours. Post-HIP SEM showed closed porosity and uninterrupted dendritic alignment with no recrystallization.

Typical CMSX Components and Industries

Component Model

Description

Alloy

Industry

SCB-600

1st-stage airfoil with serpentine cooling

CMSX-4

Aerospace applications

VNS-420

Nozzle guide segment with slot cooling

CMSX-2

Power sector

TBR-510

Rotor blade with fir-tree root

CMSX-10

Energy industry

All parts are HIP-treated before finishing and coating.

Advantages of HIP for CMSX Single Crystal Castings

  1. Reduces porosity below 0.03%, improving ultrasonic inspectability and mechanical strength under 1150°C operating conditions.

  2. Preserves grain orientation (001 axis) with zero stray grain formation or recrystallized zones during pressurization and cooling.

  3. Improves fatigue life by 2–3×, especially at shroud corners and cooling cavity intersections under cyclic thermal stress.

  4. Stabilizes wall thickness variation <0.01 mm, ensuring consistent post-HIP CNC machining tolerances.

  5. Prepares castings for weld repair, enabling trailing edge TIG welding with minimal HAZ grain transformation.

HIP Processing Parameters and Standards

  1. Temperature: 1245–1280°C, held within ±5°C to maintain phase boundaries and avoid grain misorientation.

  2. Pressure: 100–200 MPa, argon atmosphere ensures uniform consolidation of fine porosity across airfoil and root regions.

  3. Hold time: 4–6 hours, adjusted for casting size, geometry complexity, and wall section thickness.

  4. Cooling rate: ≤10°C/min, prevents stray grain growth, cracking, and residual stress development in airfoil surfaces.

  5. Validation: X-ray, CMM inspection, SEM analysis, EBSD for orientation confirmation.

Results and Verification

HIP Execution

Parts were HIPed at 1260°C, 140 MPa for 4 hours in inert atmosphere. Cooling was controlled at ≤8°C/min. No stray grains or recrystallization detected.

Post-HIP Processing

All blades were heat treated per OEM spec. Final processing included precision CNC machining and optional thermal barrier coating application.

Inspection

X-ray NDT confirmed porosity closure. Coordinate measurement validated dimensional accuracy. Grain structure SEM + EBSD confirmed integrity and orientation.

FAQs

  1. Can HIP be applied to CMSX blades with internal cooling holes?

  2. How is single crystal orientation preserved during HIP?

  3. What inspection methods verify HIP effectiveness in SC castings?

  4. Can HIP follow weld repair or precede CNC profiling?

  5. What standards govern HIP processing of CMSX turbine components?