HIP is specifically designed to mitigate critical internal defects that arise during solidification or additive layer formation. In superalloy castings produced by vacuum investment casting, metal turbulence, feeding limitations, and cooling rate variations can introduce voids that reduce fatigue performance and fracture resistance. HIP applies high isostatic pressure and elevated temperature simultaneously, collapsing these flaws and restoring near-wrought density without altering overall geometry.
This process is essential for complex thin-wall and critical rotating components—especially those used in aerospace and aviation turbines—where defect elimination directly influences service life and reliability.
HIP effectively eliminates the following defect categories:
Microshrinkage porosity – formed during solidification when feeding channels are insufficient; common in alloys like Inconel 713.
Entrapped gas porosity – caused by turbulent metal flow or reactions during melting, especially in intricate mold geometries.
Interdendritic voids – found between dendrite arms in cast microstructures; HIP compresses these voids and enhances grain boundary cohesion.
Additive-layer porosity – generated during superalloy 3d printing due to incomplete fusion or powder packing irregularities.
Bond-line defects in powder metallurgy parts – common in turbine disks manufactured through powder metallurgy turbine disc technology.
By eliminating internal defects, HIP increases fatigue strength, improves creep resistance, and suppresses crack initiation under thermomechanical loads. Single-crystal and directional castings produced through superalloy directional casting show significant improvements when HIP is combined with controlled heat treatment—for example, enhanced γ′ distribution and reduced stress concentration along grain boundaries.
For rotating components, leak-tight housings, or combustor hardware, HIP can be considered an essential step before final heat treatment, superalloy CNC machining, and final quality verification using material testing and analysis.