Different alloy families present unique challenges in WAAM due to their thermal behavior, reactivity and microstructural characteristics. Titanium alloys such as Ti-6Al-4V offer excellent strength-to-weight ratio but are highly reactive with oxygen and moisture. Without strict atmospheric control, contamination can lead to embrittlement and poor layer bonding. Therefore, oxygen levels must be maintained below critical thresholds, and shielding gas flow must be uniform during deposition.
Nickel-based alloys such as Inconel 718 and Hastelloy C-276 are prone to high residual stress due to their low thermal conductivity and strong work-hardening behavior. This increases the risk of warping and microcracking. Controlled deposition temperature, intermittent cooling and post-process stress relief methods such as HIP or heat treatment are essential to stabilize the microstructure.
Nimonic alloys, used in turbine blades and high-temperature applications, require precise control of the γ′ precipitation phase. Their response to rapid thermal cycles during WAAM can result in uneven grain growth or segregation. Using a fully monitored atmosphere and integrating material testing and analysis ensures alloy consistency, particularly when targeting creep and fatigue resistance.
Furthermore, the stiffness of Nimonic alloys increases cutting forces during finishing. Therefore, hybrid strategies combining WAAM with superalloy CNC machining must be used to achieve final dimensional accuracy.