English

Why are Inconel, Hastelloy, and Titanium alloys used in WAAM?

Table of Contents
Material Selection for WAAM
Titanium Alloys for Lightweight Structures
Application and Performance

Material Selection for WAAM

In Wire Arc Additive Manufacturing (WAAM), material choice is driven by mechanical performance, weldability, and high-temperature stability. Alloys such as Inconel 718, Hastelloy X, and titanium grades like Ti-6Al-4V combine good arc stability with resistance to distortion and oxidation. This makes them suitable for layer-by-layer deposition without compromising structural integrity.

Nickel-based alloys such as Inconel and Hastelloy maintain high tensile strength at temperatures exceeding 800 °C. Their weldability and controlled solidification behavior allow WAAM to achieve fully dense builds with minimal cracking. These alloys are widely applied in turbine cases, combustor liners and high-pressure ducts, often followed by post-process treatments to enhance fatigue resistance.

Titanium Alloys for Lightweight Structures

Titanium alloys provide the best strength-to-weight ratio for WAAM applications where weight reduction is critical—especially in aerospace and aviation applications. Alloys such as Ti-6Al-4V exhibit excellent layer adhesion and low residual stress, enabling the production of large, near-net-shape structures without excessive distortion. They can be efficiently finished through CNC machining to achieve tolerance requirements.

For demanding environments that involve creep and oxidation control, both nickel-based and titanium alloys can be further optimized using thermal barrier coatings to extend service life.

Application and Performance

The combination of WAAM with these materials enables cost-effective production of large components that would be challenging or uneconomical to forge or cast. Industries such as power generation and oil and gas benefit from corrosion-resistant Hastelloy structures, while aerospace sectors rely on titanium and Inconel for lightweight yet high-temperature assemblies. These alloys offer a stable process window for WAAM, supporting strong metallurgical bonding and minimal porosity.