English

Common Superalloy Materials Used in High-Precision Laser Cladding

Table of Contents
Nickel-Based Superalloys
Cobalt-Based Superalloys
Iron-Nickel-Based Superalloys
Specialized and Advanced Materials
Material Selection Considerations
Common Superalloys for Laser Cladding

Nickel-Based Superalloys

Nickel-based superalloys dominate high-precision laser cladding applications due to their exceptional high-temperature strength and corrosion resistance. Inconel 718 is the most widely used nickel-chromium alloy, offering excellent tensile and creep strength up to 700°C with good weldability. Inconel 625 provides superior oxidation and corrosion resistance, making it ideal for marine and chemical processing applications. For the most demanding high-temperature environments, Rene 80 and Rene 142 offer exceptional creep rupture strength through advanced γ' precipitation strengthening, though they require precise thermal management during cladding to prevent cracking.

Cobalt-Based Superalloys

Cobalt-based superalloys excel in wear resistance and high-temperature performance under constant load. The Stellite series, particularly Stellite 6 and Stellite 21, are extensively used for laser cladding on valve seats, turbine blade tips, and other components requiring galling and erosion resistance. These alloys maintain hardness at elevated temperatures (typically 30-45 HRC at 800°C) through carbide reinforcement (Cr7C3, WC) in a cobalt-chromium matrix. Haynes 188 offers outstanding oxidation resistance up to 1150°C, making it suitable for aerospace combustion components.

Iron-Nickel-Based Superalloys

Iron-nickel superalloys provide a cost-effective alternative for moderate temperature applications. A-286 and Incoloy 800H/HT are commonly clad for components operating between 500-700°C where oxidation resistance and thermal fatigue are primary concerns. These materials offer good strength and fabricability with lower nickel content than full nickel-based alloys. For specialized applications requiring thermal expansion matching, controlled expansion superalloys like Incoloy 903 and 909 are precision-clad onto components subjected to thermal cycling.

Specialized and Advanced Materials

Several specialized superalloys address unique application requirements. Hastelloy X offers exceptional oxidation resistance to 1200°C with good fabrication characteristics. Mar-M247 and CM247LC provide the highest temperature capability among conventional cast superalloys but require extremely precise cladding parameters to avoid defect formation. For single-crystal component repair, fourth and fifth-generation single-crystal alloys containing rhenium and ruthenium are increasingly being deployed with specialized laser cladding techniques.

Material Selection Considerations

Selecting the appropriate superalloy for high-precision laser cladding involves balancing multiple factors. Compatibility with the substrate material is critical to minimize thermal stress and prevent interfacial failure. Processability considerations include solidification cracking susceptibility, powder flow characteristics, and sensitivity to oxygen pickup. Final application requirements dictate the optimal choice—with nickel-based alloys preferred for high-strength applications, cobalt-based for wear resistance, and iron-nickel for cost-sensitive components. All materials require stringent quality validation to ensure they meet the precise specifications demanded by aerospace, power generation, and other high-performance industries.

Common Superalloys for Laser Cladding

Material Category

Specific Alloys

Key Properties

Typical Applications

Nickel-Based

Inconel 718, 625, 738 Rene 80, 142 Mar-M247

High temperature strength Oxidation resistance Creep resistance

Turbine blades, combustors High-temperature fasteners Rocket engine components

Cobalt-Based

Stellite 6, 21 Haynes 188 Tribaloy T-800

Wear resistance Hot hardness Galling resistance

Valve seats, bearing surfaces Turbine blade tips High-wear tooling

Iron-Nickel

A-286 Incoloy 800H/HT Incoloy 903/909

Moderate temperature strength Thermal fatigue resistance Controlled expansion

Turbocharger housings Exhaust components Seals and casings

Specialized

Hastelloy X CM247LC Nimonic 263

Extreme oxidation resistance Single crystal repair Thermal stability

Combustion chambers Single crystal blade repair High-temperature ducts