Composition and Microstructural Differences

TA15 (Ti-6.5Al-1Mo-1V-2Zr) and Ti-6Al-4V represent different approaches to titanium alloy design. TA15 features higher aluminum content (6.5% vs 6%) and additional zirconium, creating a near-alpha titanium alloy with superior stability at elevated temperatures. Ti-6Al-4V is an alpha-beta alloy with vanadium as the primary beta stabilizer. In additive manufacturing processes like LENS or WAAM, TA15 typically develops a fine basketweave α+β microstructure with excellent thermal stability, while Ti-6Al-4V exhibits acicular alpha prime martensite in as-built conditions that requires precise heat treatment to transform to the optimal α+β structure.

Mechanical Properties and Performance Characteristics

TA15 demonstrates superior performance in elevated temperature applications, maintaining strength and creep resistance up to 500°C compared to Ti-6Al-4V's effective limit of approximately 350°C. This makes TA15 particularly valuable for components in aerospace engines and high-temperature structures. At room temperature, Ti-6Al-4V typically offers higher strength (ultimate tensile strength ~950-1100 MPa vs TA15's ~930-1000 MPa) and better fracture toughness, while TA15 provides better weldability and reduced susceptibility to stress corrosion cracking.

Additive Manufacturing Processability

Both alloys are suitable for additive manufacturing, but exhibit different processing characteristics. Ti-6Al-4V has been more extensively characterized for AM processes with well-established parameters, while TA15 requires more precise control of thermal conditions during deposition. TA15's composition provides better resistance to oxidation during processing and reduced sensitivity to interstitial elements. However, Ti-6Al-4V generally demonstrates slightly better deposition efficiency and fewer process-induced defects in laser-based AM processes due to its broader processing window.

Post-Processing Requirements

Both alloys require similar post-processing including Hot Isostatic Pressing to achieve maximum density, but differ in their heat treatment approaches. Ti-6Al-4V typically requires solution treatment and aging to transform martensitic structures, while TA15 benefits from duplex annealing to optimize its high-temperature performance. TA15 generally exhibits less distortion during stress relief due to its lower residual stress accumulation during deposition, making it advantageous for large, complex structures where dimensional stability is critical.

Application-Specific Selection Criteria

The choice between TA15 and Ti-6Al-4V depends heavily on application requirements. Ti-6Al-4V is preferred for structural components requiring maximum strength-to-weight ratio at lower temperatures, such as airframe components in commercial aircraft. TA15 excels in applications demanding sustained performance at 400-500°C, including engine compressor components and missile structures. For military aerospace applications where both high-temperature capability and structural efficiency are required, TA15 often provides the optimal balance.

Comparison Table: TA15 vs Ti-6Al-4V

Property

TA15

Ti-6Al-4V

Maximum Service Temperature

500°C

350°C

Room Temperature UTS

930-1000 MPa

950-1100 MPa

Creep Resistance

Excellent

Good

Fracture Toughness

Good

Excellent

Weldability

Superior

Good

AM Process Window

Narrower

Broader

Oxidation Resistance

Better

Good